In this study, a double frequency Q-switching Nd:YAG laser beam (1064 nm and λ= 532 nm, repetition rate 6 Hz and the pulse duration 10ns) have been used, to deposit TiO2 pure and nanocomposites thin films with noble metal (Ag) at various concentration ratios of (0, 10, 20, 30, 40 and 50 wt.%) on glass and p-Si wafer (111) substrates using Pulse Laser Deposition (PLD) technique. Many growth parameters have been considered to specify the optimum condition, namely substrate temperature (300˚C), oxygen pressure (2.8×10-4 mbar), laser energy (700) mJ and the number of laser shots was 400 pulses with thickness of about 170 nm. The surface morphology of the thin films has been studied by using atomic force microscopes (AFM). The Root Mean Square (RMS) value of thin films surface roughness increased with increasing of Ag contents, while the crystallite size was found to decrease with increase in different silver content. The sensitivity toward NO2 and NH3 gas has been measured under different ppm concentrations. TiO2 with noble metal has a sensitivity higher than pure TiO2 where as TiO2 with Ag metal deposited on glass substrate has maximum sensitivity to NO2 gas with a value of ~(50 %) at the nanocomposite 90%TiO2/10%Ag films with best operation temperature at 200 °C. In addition, noble metal like Ag to the titanium dioxide materials makes them sensitive to NO2 gas.
Background: Sperm motility disorder is an important cause of infertility in male, and one of the causes of reduced motility of the sperm is the disorders of the mitochondria because it provides the required energy for sperm motility, Laser biostimulation or low-level laser therapy has a positive effect on the mitochondria and led to increasing the synthesis of ATP. Method: Twenty fresh human semen samples were used in this research study, each sample was separated into two portions, one was used as control which is not exposed to the laser beam and the other was irradiated with the wavelength of 410 nm diode laser with an output power of 100 mW and an exposure time of 60 seconds, then the measurement of
... Show MoreDesign and Construction system for recording Finger print by laser, and separted the signal to noise by holographic element, was done. For safety, total reflection lighting ensures hat aser earns an not enter An operators eyes. Holographic diffraction grating was used instead of computer program to contrast images.
Background: Cartilage forms most of the temporary skeleton of the embryo and provides a model in which most bones developObjective: Using laser therapy to enhance autologous cartilage grafts expansibility and to analyze whether this "enhancement" results in reduced rates of cartilage resorption and greater preservation of normal architectural features compared with "unenhanced" grafts. Type of the study: Cross sectional study.Methods: 24 New Zealand rabbits were divided into two groups (control and treated with 904nm, 10mW diode laser). Auricular cartilage segments measuring 1 cm2 were harvested from both ears of each rabbit, and were implanted in to the subcutaneous region of the left flank. 3 rabbits from each group were anaesthetized
... Show MoreSilver selenide telluride Semiconducting (Ag2Se0.8Te0.2) thin films were by thermal evaporation at RT with thickness350 nm at annealing temperatures (300, 348, 398, and 448) °K for 1 hour on glass substrates .using X-ray diffraction, the structural characteristics were calculated as a function of annealing temperatures with no preferential orientation along any plane. Atomic force microscopy (AFM) and X-ray techniques are used to analyze the Ag2SeTe thin films' physical makeup and properties. AFM techniques were used to analyze the surface morphology of the Ag2SeTe films, and the results showed that the values for average diameter, surface roughness, and grain size mutation increased with annealing temperature (116.36-171.02) nm The transm
... Show MoreSilver selenide telluride Semiconducting (Ag2Se0.8Te0.2) thin films were by thermal evaporation at RT with thickness350 nm at annealing temperatures (300, 348, 398, and 448) °K for 1 hour on glass substrates .using X-ray diffraction, the structural characteristics were calculated as a function of annealing temperatures with no preferential orientation along any plane. Atomic force microscopy (AFM) and X-ray techniques are used to analyze the Ag2SeTe thin films' physical makeup and properties. AFM techniques were used to analyze the surface morphology of the Ag2SeTe films, and the results showed that the values for average diameter, surface roughness, and grain size mutation increased with annealing temperature (116.36-171.02) nm The transm
... Show MoreCrystalline silicon (c-Si) has low optical absorption due to its high surface reflection of incident light. Nanotexturing of c-Si which produces black silicon (b-Si) offers a promising solution. In this work, effect of H2O2 concentrations towards surface morphological and optical properties of b-Si fabricated by two-step silver-assisted wet chemical etching (Ag-based two-step MACE) for potential photovoltaic (PV) applications is presented. The method involves a 30 s deposition of silver nanoparticles (Ag NPs) in an aqueous solution of AgNO3:HF (5:6) and an optimized etching in HF:H2O2:DI H2O solution under 0.62 M, 1.85 M, 2.47 M, and 3.7 M concentrations of H2O<
... Show MoreShort fiction, documentary and animation films constitute an outlet for many young filmmakers, who find in them a fulfillment of their ambitions. Therefore, this expansion in the cinematic movement witnessed by the cultural scene, despite the differences in levels, has produced films and names of promising young directors. In spreading cultural and artistic awareness and developing aesthetic taste. The research problem was represented in the following question (What are the characteristics of the short film and how its directive treatments are).
The theoretical framework included three sections: the first topic is the short film, its nature and features, the second topic is the elements of construction, and the third topic is Iraqi
CdO films were deposited on substrates from glass, Silicon and Porous silicon by thermal chemical spray pyrolysis technique with different thicknesses (130 and 438.46) nm. Measurements of X-ray diffraction of CdO thin film proved that the structure of the Polycrystalline is cubic lattice, and its crystallite size is located within nano scale range where the perfect orientation is (200). The results show that the surface’s roughness and the root mean square increased with increasing the thickness of prepared films. The UV-Visible measurements show that the CdO films with different thicknesses possess an allowed direct transition with band gap (4) eV. AFM measurement revealed that the silicon porosity located in nano range. Cadmium oxide f
... Show MorePbxCd1-xSe compound with different Pb percentage (i.e. X=0,
0.025, 0.050, 0.075, and 0.1) were prepared successfully. Thin films
were deposited by thermal evaporation on glass substrates at film
thickness (126) nm. The optical measurements indicated that
PbxCd1-xSe films have direct optical energy gap. The value of the
energy gap decreases with the increase of Pb content from 1.78 eV to
1.49 eV.