Titanium dioxide nanorods have been prepared by sol-gel template
method. The structural and surface morphology of the TiO2 nanorods was
investigated by X-ray diffraction (XRD) and atomic force microscopy
(AFM), it was found that the nanorods produced were anatase TiO2 phase.
The photocatalytic activity of the TiO2 nanorods was evaluated by the
photo degradation of methyl orange (MO). The relatively higher
degradation efficiency for MO (D%=78.2) was obtained after 6h of exposed
to UV irradiation.
Reaction of L1 [((E)-N1-(nitrobenzylidene)benzene-1,2-diamine] and L2( m-aminophenol), and one equivalent of di- or tri-valent metals(Cr(ӀӀӀ), Mn(ӀӀ), Fe(ӀӀӀ), Co(ӀӀ), Ni(ӀӀ), Cu(ӀӀ) and Zn(ӀӀ) afforded the complexes [M(L1)(L2)2]Cl, M=Cr(ӀӀӀ) and Fe(ӀӀӀ) and the complexes [M(L1)(L2)2] M= Mn(ӀӀ), Co(ӀӀ), Ni(ӀӀ), Cu(ӀӀ) and Zn(ӀӀ). The structure of the Schiff base ligand and their complexes are characterized by (C:H:N), FT.IR, UV.Vis, 1HNMR, 13CNMR and mass spectral. The presence of metal in the complexes are characterized by flame atomic absorption. The spectral data of the complexes have revealed the octahedral geometry. The (L1), (L2) and mixed ligand metal complexes were screened for their ability as cataly
... Show Moreتعد مراجعة النظير واحدة من الأســاليب الحديثة فــي مجال الرقابة والتدقيق ونشــأة كأداة لقياس مــدى فاعليــة الرقابــة علــى الجــودة هو لبنة أساسية في إدارة الجودة الشاملة ووسيلة لتحســين أدوات الرقابــة المعمول بها، وللتحقق من مدى الانسجام بين المعايير الدولية للأجهزة العليا للرقابة المالية والمحاسبة والاجراءات المعمول بها من قبل الاجهزة العليا للرقابة وعليه فأن مراجعة النظير أداة تستخدم ف
... Show MoreIn this study, experimental and numerical applied of heat distribution due to pulsed Nd: YAG laser surface melting. Experimental side was consists of laser parameters are, pulse duration1.3
Electrochemical method was used to prepare carbon quantum dots (CQDs). Size of matter was nature when evaluate via X-ray diffraction (XRD). A distinct peak at 2θ equal to 31.6° and three other small peaks at 38.28°, 56.41° and 66.12° were observed. The measures of Fourier Transform Infrared Spectroscopy (FTIR) showed the bonds in the transmittance spectrum are manufactured with carbon nanostructures in view. The first peaks are the O–H stretching vibration bands at (3417 and 2922) cm−1, (C–O–H at 1400, and 1317) cm−1, (C–H), (C=C), (C–O–H), (C=O), and (C–O) bonds at 2850, 1668, 1101, and 1026 cm−1 sequentially. The transmission electron microscopy (TEM) results presented that the spherical CQDs are in shape and on a
... Show MoreForward osmosis (FO) process was applied to concentrate the orange juice. FO relies on the driving force generating from osmotic pressure difference that result from concentration difference between the draw solution (DS) and orange juice as feed solution (FS). This driving force makes the water to transport from orange juice across a semi-permeable membrane to the DS without any energy applied. Thermal and pressure-driven dewatering methods are widely used, but they are prohibitively energy intensive and hence, expensive. Effects of various operating conditions on flux have been investigated. Four types of salts were used in the DS, (NaCl, CaCl2, KCl, and MgSO4) as osmotic agent and the experiments were performed at the concentration of
... Show Morethe study including isolation and identification of candida spp causing UTIs from patintes coming to al-yarmouk hospital
Adsorption techniques are widely used to remove certain classes of pollutants from waters, especially those that are not easily biodegradable. Dyes represent one of the problematic groups. The removal of methyl green from waste water using bamboo was studied in batch and continuous system. In batch system equilibrium time and adsorption isotherm was studied at different concentrations (5, 10, 15, 20, 25 and 30 ppm) and 50 mg weight of adsorbent.
Langmuir and Freundlich equations were applied for adsorption isotherm data. Langmiur equation was fitted better than Freundlich equation (R2=0.984 for Langmuir equation).The maximum percentage dye removal obtained 79.4% and adsorption capacity was 15.5 mg/g. For continuous system the breakthr