The most important environmental constraints at the present time
is the accumulation of glass waste (transparent glass bottles). A lot of
experiments and research have been made on waste and recycling
glass to get use it as much as possible. This research using recycling
of locally waste colorless glass to turn them into raw materials as
alternative of certain percentages of cement to save the environment
from glass waste and reduce some of the disadvantages of cement
with conserving the mechanical and physical properties of concrete
made. A set of required samples were prepared for mechanical test
with different weight percentage of waste glass (2%, 4%, 5%, 6%,
8%, 10%, 15%, 20% and 25%). American standard for calibration
(ASTM C109 / C109M-02) to measure the compressive strength
where the results showed that the Maximum compressive strength
was obtained at the low weight percentage replacement 2%, 4% and
5% 6% which is 67.12, 69.24, 62.56 and 59.96 Mpa respectively. for
originally mix recorded bending resistance (54.16) Mpa.
This research is devoted to study the effect of different in weight percentage of Sio2 particles and glass fibers (5, 10, 15, 20) wt. % on the wear rate epoxy resin. The results show that the value of hardness increase with the increase for the weight percentage of reinforcing particles and fibers, while the wear rate decrease with the increase the load level of the reinforcing particles and fibers . The largest value of the hardness, and the lowest value of the wear rate for epoxy reinforced with 20% of SiO2, the wear rate increase in general with increasing the applied load.
Sewage sludge samples were collected from Al-rasafa and Al-karkh refinement stations which represent the main stations of Baghdad city. Samples were collected from all treatment stages: before, after, and during refinement processes. The High Purity Germanium Coaxial Detector system with energy resolution 1.8 keV for energy line 1333 keV of Co – 60 radioactive sources was used to measure radioactivity from both natural and artificial sources. GENIE – 2000 analysis the results statistically and qualitatively. The results showed that all sewage sludge samples exhibited natural radioactive level and sometimes less than the international regular standards, but Al–Karkh station showed increment in radioactive levels than Al– Rasa
... Show More|
Measurement of radon concentration level was carried out in 40 houses in Al – Najaf city during summer season of 2012. Long term measurement of indoor of old building radon concentrations have been taken, using a previously calibrated passive diffusion dosimeters containing CR – 39 solid state nuclear track detectors which are very sensitive for alpha particles. The measurement of the indoor radon concentration obtained in summer in these regions ranged from 11.654±4.216 Bq.m-3 to 53.610±8.777 Bq.m-3. The results were within universally permitted levels. |
This research presents experimental and theoretical investigation of 15 reinforced concrete spliced and nonspliced girder models. Splices of hooked dowels and cast in place joints, with or without strengthening steel plates were used. Post-tensioning had been used to enhance the splice strength for some spliced girders. The ANSYS computer program was used for analyzing the spliced and non-spliced girders. A nonlinear three dimensional element was used to represent all test girders. The experimental results have shown that for a single span girder using steel plate connectors in the splice zone has given a sufficient continuity to resist flexural stresses in this region. The experimental results have shown that the deflection of hooked do
... Show MoreThis research aims to test the ability of glass waste powder to adsorb cadmium from aqueous solutions. The glass wastes were collected from the Glass Manufacturing Factory in Ramadi. The effect of concentration and reaction time on sorption was tested through a series of laboratory experiments. Four Cd concentrations (20, 40, 60, and 80) as each concentration was tested ten times for 5, 10, 15, 20, 25, 30, 35, 40, 45, and 50 min. Solid (glass wastes) to liquid was 2g to 30ml was fixed in each experiment where the total volume of the solution was 30ml. The pH, total dissolved salts and electrical conductivity were measured at 30ºC. The equilibrium concentration was determined at 25 minutes, thereafter it was noted that the sorption
... Show MoreThis study is a numerical investigation of the performance of reinforced concrete (RC) columns after fire exposure. This study aims to investigate the effect of introducing lateral ties and using the RC jacket on improving post-fire behavior of these columns, the effect of the duration of the fire on ultimate load of columns. The analysis was performed through ABAQUS, a 3D – non-linear finite element program. 4 m tall lengthening square RC column with a cross- section of 0.4 m × 0.4 m was used as a test specimen. The RC column was reinforced by 4Ø28 mm longitudinal bars bonded by steel tie bars of Ø10 mm spaced at 400 mm. The firing temperature was increased to 60
This study presents an investigation about the effect of fire flame on the punching shear strength of hybrid fiber reinforced concrete flat plates. The main considered parameters are the fiber type (steel or glass) and the burning steady-state temperatures (500 and 600°C). A total of 9 half-scale flat plate specimens of dimensions 1500mm×1500mm×100mm and 1.5% fiber volume fraction were cast and divided into 3 groups. Each group consisted of 3 specimens that were identical to those in the other groups. The specimens of the second and the third groups were subjected to fire flame influence for 1 hour and steady-state temperature of 500 and 600°C respectively. Regarding the cooling process, water sprinkling was applied directly aft
... Show MoreIn this work, Soda Lime Glass (S.L.G.) powder was used ,as
fluxe in traditional porcelain instead of feldspar. Two ceramics
porcelain were compared; commercial or traditional porcelain that
content of 50wt % kaolin, 25wt % quartz, and 25wt % feldspar.
Feldspar mass was substituted by scraps soda lime glass yielding a
new porcelain composition, to determine the softening points and
then the effect of glass addition on porcelain firing process.
Eight samples, for each patch, were prepared and 8wt % water
was added. The resulting composite blends were then die pressed at
2N, to produce disk specimens with diameter of 1.5 cm, and then
they were sintered at (1000, 1100, 1200, 1250,1300,1350,1400 and
1450) ˚C,