NiO0.99Cu0.01 films have been deposited using thermal evaporation
technique on glass substrates under vacuum 10-5mbar. The thickness
of the films was 220nm. The as -deposited films were annealed to
different annealing temperatures (373, 423, and 473) K under
vacuum 10-3mbar for 1 h. The structural properties of the films were
examined using X-ray diffraction (XRD). The results show that no
clear diffraction peaks in the range 2θ= (20-50)o for the as deposited
films. On the other hand, by annealing the films to 423K in vacuum
for 1 h, a weak reflection peak attributable to cubic NiO was
detected. On heating the films at 473K for 1 h, this peak was
observed to be stronger. The most intense peak is at 2θ = 37.12o with
the preferential orientation of the films being (111) plane. The optical
properties of the films have been studied. The effect of annealing
temperature on the optical parameters of NiO0.99Cu0.01 such as
transmittance, reflectance, absorption coefficient, refractive index,
extinction coefficient, and real and imaginary parts of dielectric
constant has been reported.
Samples of Oxytricha falax were collected from Tigris River by 55µ. mesh net. Culturing of O. falax were cultivated in specific conditions (DO 3-5mg/l.; W.Temp. 24±1ºC; pH: 6.8-7.5).The effect of various furfural concentration 0, 20, 40, 80,100 and 124 ppm and toluene concentration 0, 15, 30, 34.2, 34.5 and 35 ppm after two periods of treatment (24 and 48 hr.) on the physiological parameters of O. falax ciliate were observed. This study showed that the lethal concentration of furfural was 124ppm and 80ppm after 24hr. and 48hr. from treatment which killed all the individual community respectively. Furthermore the treatment of O. falax individuals with different concentrations of toluene indicated that 34.5 ppm of it caused disappearance o
... Show MoreBackground: White spot lesion considered as irreversible tooth demineralization presenting challenge to orthodontists during treatment schedules, fluoride was the most successfully used measure to overcome this challenge. Materials and method: A total of forty sound human permanent premolars were used in the present study and categorized into four groups, in one group the teeth were bonded with stainless steel brackets using Resin-modified glass ionomer cement (RMGIC) and the other three groups the teeth were bonded with light cured composite Resilience® (Ortho technology Co., USA). Group A; Acidulated phosphate fluoride (APF) topical gel (Mfg by DEEPAK PRODUCTS, INC, USA), fluoride ion 1.23% applied on examine area for four minute. Gro
... Show MoreEffect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.
The effect of gamma radiation at the doses (0 , 5 , 10 or 15 ) Gray on the callus of four Triticum aestivum immature embryos genotypes (AL-Hashmiya , AL-Noor AL-Zahraa and AL-Mellad ) were studied . The fresh and dry weight for callus and shoot tips beside numbers and lengths of the shoots were used as indicators after 8 weeks . Results revealed that (AL-Noor and AL-Zahraa ) was superior by giving highest fresh and dry weight reached 274.2 and 269.2 mg and 26 and 24.3 mg respectively as compared with AL-Hashmiya and AL-Mellad. Moreover, the control treatment and the dose 10 Gray gave highest fresh weight reached 277.4 and 259.1 mg while the dry weight was highest in the control treatment and the dose 5 Gray. addition 10 Gra
... Show MoreA dynamic analysis method has been developed to investigate and characterize embedded delamination on the dynamic response of composite laminated structures. A nonlinear finite element model for geometrically large amplitude free vibration intact plate and delamination plate analysis is presented using higher order shear deformation theory where the nonlinearity was introduced in the Green-Lagrange sense. The governing equation of the vibrated plate were derived using the Variational approach. The effect of different orthotropicity ratio, boundary condition and delamination size on the non-dimenational fundamental frequency and frequency ratios of plate for different stacking sequences are studied. Finally th
... Show More