Cadmium sulfide photodetector was fabricated. The CdS nano
powder has been prepared by a chemical method and deposited as a
thin film on both silicon and porous p- type silicon substrates by spin
coating technique. Structural, morphological, optical and electrical
properties of the prepared CdS nano powder are studied. The X-ray
analysis shows that the obtained powder is CdS with predominantly
hexagonal phase. The Hall measurements show that the nano powder
is n-type with carrier concentration of about (-5.4×1010) cm-3. The
response time of fabricated detector was measured by illuminating
the sample with visible radiation and its value was 5.25 msec. The
specific detectivity of the fabricated detector is found to be (9×1011
W-1 .Hz1/2.Cm- 1). The responsivity was (0.03A/W).
Abstract: Despite the distinct features of the continuous wave (CW) Terahertz (THz) emitter using photomixing technique, it suffers from the relatively low radiation output power. Therefore, one of effective ways to improve the photomixer emitter performance was using nanodimensions electrodes inside the optical active region of the device. Due to the nanodimension sizes and good electrical conductivity of silver nanowires (Ag-NWs), they have been exploited as THz emitter electrodes. The excited surface plasmon polariton waves (SPPs) on the surface of nanowire enhances the incident excitation signal. Therefore, the photomixer based Ag-NW compared to conventional one significantly exhibits higher THz output signal. In thi
... Show MoreFabrication of a photodetector consists of the conjugated polymer "MEH-PPV"- poly (2-methoxy-5-(2'-ethylhexyloxy)-1,4-phenlenevinylene) and MEH-PPV:MWCNT nanocomposite thin film. The volume ratio investigated was 0.75:0.25. MEH-PPV was dissolved in chloroform solvent and doped with MWCNTs. The spin coating method was used to achieve a facile and low cost photodetector. The absorption spectrum decreases by adding the CNTs. The PL spectrum detected recombination curve results by doping the polymer with CNTs, and AFM measurement showed an increase of roughness average from (0.168 to 2.43nm) of "MEH-PPV" and "MEH-PPV:CNTs", respectively. The doping ratio 0.25, which has a higher photoresponsivity, was evaluated at 1.70 A/W and 2.14 A/W of th
... Show MoreThis work aimed to produce PVA and PVA/Ag nanofibers ultra-high sensitivity photodetector by electrospinning. The electrospinning process was used to successfully prepare PVA nanofibers and a PVA-Ag nanofiber composite. FE-SEM, XRD, UV, I-V characterizations are used to study the morphological, structural, optical, and electrical properties of the material. In contrast, the PVA-Ag nanofiber composite film displayed a cubic structure with favored orientation (200) that indicated the presence of Ag NPs in the PVA-Ag nanofibers film. While the optical energy gap for PVA was 3.96 eV, it was only 2.14 eV for PVA-Ag nanofibers composite film, making this composite sensitive to visible light, particularly green light at 550 nm with a 65% photosens
... Show MoreA hybrid cadmium sulfide nanoparticles (CdSNPs) electroluminescence (EL) device was fabricated by Phase – Segregated Method and characterized. It was fabricated as layers of (ITO/poly-TPD:CdS ) and (ITO/poly-TPD:CdS /Alq3). Poly-TPD is an excellent Hole Transport Layer (HTL), CdSNPs is an emitting layer and Alq3 as electron transport layer (ETL). The EL of Organic-Inorganic Light Emitting Diode (OILED) was studied at room temperature at 26V. This was achieved according to band-to-band transition in CdSNPs. From the I-V curve behavior, the addition of Alq3 layer decreased the transfer of electrons by about 250 times. The I-V behavior for (poly-TPD/CdS) is exponential with a maximum current of 4500 µA. While, the current i
... Show MorePartial shading is one of the problems that affects the power production and the efficiency of photovoltaic module. A series of experimental work have been done of partial shading of monocrystalline PV module; 50W, Isc: 3.1A, Voc: 22V with 36 cells in series is achieved. Non-linear power output responses of the module are observed by applying various cases of partial shading (vertical and horizontal shading of solar cells in the module). Shading a single cell (corner cell) has the greatest impact on output energy. Horizontal shading or vertical shading reduced the power from 41W to 18W at constant solar radiation 1000W/m2 and steady state condition. Vertical blocking a column
... Show MoreAn experimental work has been conducted on wall attachment fluidics amplifiers, one of them to study the effect of output pressure or load on the amplifier performance. The output load has been simulated as a piston connected to the device output and the piston can be loaded accordingly. The results shows that the output volume flow rate increases as the supply pressure increases under different load and the output pressure remains constant as the supply pressure increases under constant load.
This study was carried out to evaluate parasitological and immunological of the effect of chitosan and chitosannanoparticles loaded with spiramycin on toxoplasmosis infected mice. After injection intra peritoneal with 103viable tachyzoites for acute infection, treatments given for seven days. Peritoneal fluid examination revealed a significant decrease in the number of Toxoplasmagondiitachyzoites in all treated infected mice compared with infected non-treated. The combined therapy gave better results than single. The best effect was observed in group of mice treated with spiramycin combined with chitosan nanoparticles. Also immunoglobulin Ig Manti body and gamma Interferon (INFγ), Tumor Necrosis Factor alpha (TNF-α) cytokines responses ag
... Show MoreThe paper include study the effect thickness of the polymeric sample which is manufactured by thermo press way. The sample was used as an active tunable R6G laser media. The remarks show that, when the thickness of the samples is increased, with the same concentration, the spectrum will shift towards the short wavelength, & the quantum fluorescence yield will increased. The best result we obtained for the quantum fluorescence yield is (0.68) at the sample, with thickness (0.304mm) in Ethanol solvent, while when we used the Pure Water as a solvent, we found that the best quantum fluorescence yield is (0.63) at (0.18mm) thickness of the sample.