PVA, Starch/PVA, and Starch/PVA/sugar samples of different
concentrations (10, 20, 30 and 40 % wt/wt) were prepared by casting
method. DSC analysis was carried; the results showed only one glass
transition temperature (Tg) for the samples involved, which suggest
that starch/PVA and starch/PVA/sugar blends are miscible. The
miscibility is attributed to the hydrogen bonds between PVA and
starch. This is in a good agreement with (FTIR) results. Tg and Tm
decrease with starch and sugar content compared with that for
(PVA). Systematic decrease in ultimate strength, due to starch and
sugar ratio increase, is attributed to (PVA), which has more hydroxyl
groups that made its ultimate strength higher than that for
starch/PVA, and starch/PVA/sugar blends. It is observed from water
uptake tests that the solubility time decreases with starch ratio; it is
attributed to decrease in hydroxyl groups caused by PVA ratio
decrease. The inter- and inter-molecular bonds of the hydroxyl
groups enhanced the solubility process of the starch/PVA blends in
water. The water immersion causes hydrogen bonds (inter and
intermolecular bonds) to decompose, that increases the film
solubility. Water absorption and capacity of degradability are most
important in biodegradable materials. The results suggest the samples
that have undergone investigation, can be used for shopping, and
food packaging.
The study of soil burial for the sample at (3cm) depth, and at (13cm)
depth has exhibited weight loss increase with soil burial time. The
biodegradability rapidly increases at the first (6-7) weeks; it is found
that the weight loss at (3cm) depth is greater than that at (13cm) that
was attributed to the differences in the availability of oxygen ratio. It
is found that PVA undergoes lowest weight loss, the weight loss
changes with starch, and sugar content. In dry soil, the weight loss is
lower. The results proved that the biodegradation decreases with soil
burial time after seven weeks of burial. It is concluded that the
samples involved are biodegradable material that can be used for
packaging applications and biologically friendly synthetic polymer
blends to solve the solid waste accumulation problem.
Synthetic polymers such as polyurethane are used widely in the field of biomedical applications such as implants or part of implant systems.
This paper focuses on the preparation of base polymer matrix composite materials by (Hand Lay-Up) method, and studying the effect of selected grain size (32, 53, 63, 75, and 90) µm of (Reenia) particles on some properties of the prepared composite.
Mechanical tests were used to evaluate the prepared system (Tensile, Compression, Impact, and Hardness) tests, and a physical test of (Water absorption %), and all tests were accomplished at room temperature.
Where results showed tensile test (maximum tensile strength and modulus of elasticity) high at small grain size while
... Show MoreAbstract:
This research seeks to test the influence of intellectual capital as an explanatory variable and its components (human capital, structural capital, relational capital) and sustainable competitive performance as a responsive variable and its components (reducing service delivery cycle time, rapid response to market demand, increasing customer satisfaction, providing better Quality of service, increasing market share)” through a field study, and here the research problem was diagnosed in an attempt to answer the following question: Is there awareness among the senior management within the private colle
... Show MorePseudoephedrine (PSE) or (Sudafed) is one of the sympathomimetic group of drugs (ephedrine, PSE and amphetamines) which effects cardiovascular system, respiratory system, and gastrointestinal tract. However, only little researches had supported its effect on solid abdominal organs. This study aims to investigate the effects of different doses of Sudafed in the liver and kidney of albino mice. The current study included 18 albino mice grouped into 2 groups: control (3 mice), and acute group (15 mice). The acute group was further subdivided into 5 subgroups, each subgroup of 3mice wasgiven a lonely intaperitonial injection of 0.3ml of the following conc. (500mg/kg, 250mg/kg, 125mg/kg, 62.52mg/kg, and 31.24mg/kg) for 24hrs. After the m
... Show MoreThis study was conducted in the Tissue Culture laboratory of the Horticultural Department of the Faculty of Agriculture at Karbala University to investigate the effects of a light source (Florescent, LED) and adenine sulfate (Ads) a 0, 40, 80, and 120 mg l-1 on the multiplication and rooting of
The marine collagens are biocompatible and biodegradable materials that are considered as a biomimetic approach for tissue regeneration. This study evaluated the effect of daily consumption of marine collagen supplement drink on enamel white spot lesions (WSLs), comparing the results against Regenerate system and Sylc air abrasion methods. Fifty human enamel slabs were allocated into five groups (n = 10 per group): non-treated (sound); non-treated (WSLs, 8% methylcellulose gel with 0.1 M lactic acid (pH 4.6) at 37 °C for 21 days); and three treated surfaces with marine collagen; Regenerate system; and Sylc air abrasion. The treatment lasted for 28 days followed by four weeks’ storage in artificial saliva (pH = 7.0, 37 °C). Evalu
... Show MoreThe induced photodegradation of methyl cellulose (MC) films in air was investigated in the absence and presence of aromatic carbonyl compounds(photosenssitizers): 1,4-naphthaquinone (NQ) and benzophenone (BPH) by accelerated weathering tester. The addition of (0.01 wt %) of low molecular weight aromatic carbonyl compounds to cellulose derivatives films(25µm in thickness) enhanced the photodegradation of the polymer films.The photodegradation rate was measured by the increase in carbonyl absorbance. Decreases in solution viscosity and reduction of molecular weight were also observed in the irradiated samples. Changes in the number-average chain scission, the degree of deterioration and in the quantum yield of chain scission values are als
... Show More