Porous silicon (PS) layers were formed on n-type silicon (Si) wafers using Photo- electrochemical Etching technique (PEC) was used to produce porous silicon for n-type with orientation of (111). The effects of current density were investigated at: (10, 20, 30, 40, and50) mA/cm2 with etching time: 10min. X-ray diffraction studies showed distinct variations between the fresh silicon surface and the synthesized porous silicon. The maximum crystal size of Porous Silicon is (33.9nm) and minimum is (2.6nm) The Atomic force microscopy (AFM) analysis and Field Emission Scanning Electron Microscope (FESEM) were used to study the morphology of porous silicon layer. AFM results showed that root mean square (RMS) of roughness and the grain size of porous silicon decreased as etching current density increased and FESEM showed that a homogeneous pattern and confirms the formation of uniform porous silicon. The chemical bonding and structure were investigated by using Fourier transformation infrared spectroscopy (FTIR). The band gap of the samples obtained from photoluminescence (PL). These results showed that the band gap of porous silicon increase with increasing porosity.
Forest cover in Mosul Province experienced significant changes following the 2014 occupation. These changes can be effectively analyzed using multitemporal remote sensing imagery. This study aims to evaluate the ability of multi-temporal Landsat 8 images and the Forest Canopy Density (FCD) model to detect changes in forest canopy density in a protected forest in Mosul Governorate during the period from 2014 to 2025. The remote sensing data used in this research are Landsat 8 images captured on March 21, 2014, and April 4, 2025. The method employed is FCD modeling, which produces pixel-level canopy density estimates. The results of the FCD model are then used to analyze changes in canopy density following the occupation. The findings of this
... Show MoreIn this paper, a miniaturized 2 × 2 electro-optic plasmonic Mach– Zehnder switch (MZS) based on metal–polymer–silicon hybrid waveguide is presented. Adiabatic tapers are designed to couple the light between the plasmonic phase shifter, implemented in each of the MZS arms, and the 3-dB input/output directional couplers. For 6 µm-long hybrid plasmonic waveguide supported by JRD1 polymer (r33= 390 pm/V), a π-phase shift voltage of 2 V is obtained. The switch is designed for 1550 nm operation wavelength using COMSOL software and characterizes by 2.3 dB insertion loss, 9.9 fJ/bit power consumption, and 640 GHz operation bandwidth
Thin films of (Cu2S)100-x( SnS2 )x at X=[ 30,40, &50)]% with thickness (0.9±0.03)µm , had been prepared by chemical spray pyrolysis method on glass substrates at 573 K. These films were then annealed under low pressure of(10-2) mbar ,373)423&473)K for one hour . This research includes , studying the the optical properties of (Cu2S)100-x-(SnS2)x at X=[ 30,40, &50)]% .Moreover studying the effect of annealing on their optical properties , in order to fabricate films with high stability and transmittance that can be used in solar cells. The transmittance and absorbance spectra had been recorded in the wavelength range (310 - 1100) nm in order to study the optical properties . It was found that these films had direct optical band
... Show MoreThe effect of UV-light on the tensile properties of pure PC has been studied. It was shown that irradiation of PC undergo a drop in the tensile properties of 30 hour of exposure. The results of irradiated samples shows that the addition of ZnO and TiO2 with different percentages (0.5, 1, 1.5 %) will reduce the Young modulus and ultimate stress of PC/ZnO ,PC/ TiO2 composites
Thin films of CdTe were prepared with thickness (500, 1000) nm on the glass substrate by vacuum evaporation technique at room temperature then treated different annealing temperatures (373,473,and 573)K for one hour. Results of the Hall Effect and the electrical conductivity of (I-V) characteristics were measured in darkness and light.at different annealing temperature results show that the thin films have ability to manufacture solar cells, and found that the efficient equal to (2.18%) for structure solar cell (Algrid / CdS / CdTe /glass/ Al) and the efficient equal to (1.12%) for structure solar cell (Algrid / CdS / CdTe /Si/ Al) with thick ness of (1000) nm with CdTe thin films at RT.
The ground state proton, neutron, and matter density distributions and corresponding root-mean-square radii (rms) of the unstable neutron-rich
22C exotic nucleus are investigated by two-frequency shell model (TFSM) approach. The single-particle wave functions of harmonic-oscillator (HO)
potential are used with two oscillator parameters bcore and bhalo. According to this model, the core nucleons of 20C are assumed to move in the model
space of spsdpf. Shell model calculations are performed with (0+2)hw truncations using Warburton-Brown psd-shell (WBP) interaction. The outer (halo) two neutrons in 22C are assumed to move in HASP (H. Hasper) model space (2s1/2, 1d3/2, 2p3/2, and 1f7/2 orbits) using the HASP interaction. The halo st
In this paper, investigates the biosynthesis of gold nanoparticles (AuNPs) by biochemical method using Myrtus communis leaves extract as reducing agent and Chloroauric acid (HAuCl4) as precursors. X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM) and FTIR were used in addition to UV-visible spectroscopy (UV) in order to characterize the AuNPs. The biosynthesized AuNPs exhibited inhibitory effects on alpha amylase and alkaline phosphatase in sera of patient with type 2 Diabetes Miletus and the sera of healthy control subjects; the inhibition percentage with alpha amylase was 72 % and 45 % for patient and control group respectively. Oral consent obtained from the most of patients and healthy subjects before them being under
... Show MoreThe work concerned with studying the effect of (SiO2) addition as a
filler on the adhesive properties of (PVA). Samples were prepared as
sheets by using casting method. The mechanical properties showed
that increase in tensile strength from (34MPa) to (68MPa) when
(SiO2) added to (PVA). The adhesive strength showed that joint
properties depend upon specific adhesive characteristic of material
(PVA) and (SiO2\PVA)composites at different concentrations (1.5%,
2.5%, 3.5%, 4.5wt%), the cohesive strength of the adhesive material,
the joint design, and adherent type (Sponge Rubber(SR), Natural
leather (NL), Vulcanized Rubber(VR), and Cartoon). The results
proved the tensile strength increased with (SiO2) ratio, so