Porous silicon (PS) layers were formed on n-type silicon (Si) wafers using Photo- electrochemical Etching technique (PEC) was used to produce porous silicon for n-type with orientation of (111). The effects of current density were investigated at: (10, 20, 30, 40, and50) mA/cm2 with etching time: 10min. X-ray diffraction studies showed distinct variations between the fresh silicon surface and the synthesized porous silicon. The maximum crystal size of Porous Silicon is (33.9nm) and minimum is (2.6nm) The Atomic force microscopy (AFM) analysis and Field Emission Scanning Electron Microscope (FESEM) were used to study the morphology of porous silicon layer. AFM results showed that root mean square (RMS) of roughness and the grain size of porous silicon decreased as etching current density increased and FESEM showed that a homogeneous pattern and confirms the formation of uniform porous silicon. The chemical bonding and structure were investigated by using Fourier transformation infrared spectroscopy (FTIR). The band gap of the samples obtained from photoluminescence (PL). These results showed that the band gap of porous silicon increase with increasing porosity.
This qualitative study was conducted on eight types of commercial baking yeast which available in local markets to estimate their fermentation activity as affecting the Bread industry and the impact of the salt added to DoughLeavening, The results showed a great variation in the fermentation capacity of yeast samples (their role in swelling the dough), most notably the sample value Y3 and least sample Y7 and reached 80% and 20% respectively, and the value of Leavening by using the two types of yeast with addition of three levels of salt (0 , 1 and 2%) have 20.0 , 19.7 and 15.7 of the sample Y3, compared with 10.5 , 10.3 and 8.8 of the sample Y7 for each of the levels of salt respectively, reflect
... Show MoreThis study investigated the shear performance of concrete beams with GFRP stirrups vs. traditional steel stirrups. Longitudinal glass fiber‐reinforced polymer (GFRP) bars were used to doubly reinforce the tested beams at both the top and bottom of their cross sections. To accomplish this, several stirrup spacings were provided. Eight beam specimens, measuring 300 × 250 × 2400 mm, were used in an experimental program to test under a two‐point concentrated load with an equal span‐to‐depth ratio until failure. Four beams in Group I have standard mild steel stirrups of 8 mm diameter, while four beams in Group II have GFRP stirrups with the same adopted diameter. The difference betwe
This study investigated the shear performance of concrete beams with GFRP stirrups vs. traditional steel stirrups. Longitudinal glass fiber‐reinforced polymer (GFRP) bars were used to doubly reinforce the tested beams at both the top and bottom of their cross sections. To accomplish this, several stirrup spacings were provided. Eight beam specimens, measuring 300 × 250 × 2400 mm, were used in an experimental program to test under a two‐point concentrated load with an equal span‐to‐depth ratio until failure. Four beams in Group I have standard mild steel stirrups of 8 mm diameter, while four beams in Group II have GFRP stirrups with the same adopted diameter. The difference betwe
This study includes the direct influence of (single & multi) dose of Cold Atmospheric Plasma (CAP) on the no. of platelets for mice for different exposure time (15, 30, 60, and 120) sec. the influence of CAP on mice was measured after 1, 2, 3, 7, and 14 day from exposure.
The results obtained in this study indicate that the effect of low doses of CAP on platelets was stimulatory effect in the first few hours from exposure (1day) but the high dose was inhibitory, It was found that after two weeks of exposure that the number of platelets became normal comparable to the control one, and this indicates that plasma effect was removed after this period.
The importance of internal audit in the growing demand for services in the public and private economic units, and in the rapid growth of its systems professional, has also been recognition of the importance of internal audit quality and the quality of information provided in a long time, as well as the importance of achieving the greatest possible quality in his work to reduce accounting risks of financial reports misleading or fraudulent, which is one of the important features of the audit.
The internal audit quality are linked with the ability of auditors to detect errors in the financial statements, and their willingness to express an opinion technical neutral and non-aligned based on the results of th
... Show MoreA field experiment was conducted at the experimental field of botanical garden, faculty of science, university of Baghdad, in order to study the effect of plant density on growth and yield of two local cultivars of sunflower (Sin Althieb and Shumose). The densities used were 4.4 and 8.8 plant/m2. The results showed difference between cultivars in their agronomic traits and their yields. There was a significant increase in plant height and leaf area index by increasing the plant density, while head diameter, number of seeds and leaf area decreased. But the most significant effect was the increasing in yield and biological yield by increasing the plant density. There was an increase by 72% and 58% in the yield and 79% an
... Show MoreSome transition metal ions (Cr +3, Co+2 , Ni+2,Cu+2, Zn+2,Ag + ,Cd+2 ) complexes of [(N, N- - Bis(2- hydroxy ethyl) Glycine] (Bicine) have been synthesized and characterized by FTIR ,UV-Visble spectroscopy, atomic absorption, magnetic susceptibility, conductivity measurements and study of the nature of the complexes formed in ethanolic solution following the moleratio method. From the results obtained the following general formola have been given for the prepared complexes [M m+ (Bicine)n]. XH2O
NiO0.99Cu0.01 films have been deposited using thermal evaporation
technique on glass substrates under vacuum 10-5mbar. The thickness
of the films was 220nm. The as -deposited films were annealed to
different annealing temperatures (373, 423, and 473) K under
vacuum 10-3mbar for 1 h. The structural properties of the films were
examined using X-ray diffraction (XRD). The results show that no
clear diffraction peaks in the range 2θ= (20-50)o for the as deposited
films. On the other hand, by annealing the films to 423K in vacuum
for 1 h, a weak reflection peak attributable to cubic NiO was
detected. On heating the films at 473K for 1 h, this peak was
observed to be stronger. The most intense peak is at 2θ = 37