In this study, titanium dioxide (TiO2) nanoparticles incorporated with cement were synthesis by a simple casting method as a function concentration of TiO2 (0.2, 0.4, 0.8, 1, and 2 wt%). The prepared samples were characterized using the technique of Field Emission Scanning Electron Microscope (FESEM) and UV-Visible spectrophotometer, which was used to measure the adsorption spectra. The observed photocatalytic efficiency of TiO2 nanoparticles (NP) incorporated with cement was investigated by decomposing the dye methyl blue (MB) solution under sunlight irradiation. According to the slope, the value of the k constant at the best sample is 0.8wt%, k=0.8265 min-1. FESEM image of the TiO2/cement with 0.8 wt% content show the TiO2 NPs were well-attached to cement particles, and they covered the cement surface. The increase in photocatalytic (PC) activity was due to an increase of TiO2 concentration in the cement, which best occur of 0.8 wt% of TiO2 in cement. The degradation at the MB (5ppm) was 98.864 % after 120 min under sunlight irradiation. The method involves easily and simply preparing TiO2/cement that is used in self-cleaning and studying the effect of different festive factors, including the concentration of the dye. The preparation of TiO2/cement was successful as a photocatalyst for a self-cleaning surface.
Coffee is the most essential drink today, aside from water, the high consumption of coffee and the byproducts of its soluble industries such as spent coffee grounds can have a negative effect on the environment as a source of toxic organic compounds. Therefore, caffeine removal from the spent coffee ground can be applied as a method to limit the effect of its production on the environment. The aim of this study is to determine the kinetics and thermodynamics parameters and develop models for both processes based on the process parameters by using traditional solid-liquid extraction and Ultrasound-assisted extraction methods. The processes were performed at a temperature range of 25 to 55 °C for traditional and ultrasound baths, and
... Show MoreIn this research constructed N2 laser system by use developed method of electric discharge. In this method used four step of electric discharge by using four capacitors, three spark gaps, high tension power supply varying in range from 12kV to 24 kV and three resistors, this method called three stage blumlein circuit. The breakdown time delay of these parallel spark gaps cement strong ultraviolet preionization in the laser channel, thus the result of these amendments the laser output is many doubled and is more increasing than that obtained using the one and two stage blumlein circuits. This system has been designed and operated to give pulse laser with wavelength at 337.1 nm. This laser system can operate without mirrors and optical res
... Show MoreIn this paper, a comparison between horizontal and vertical OFET of Poly (3-Hexylthiophene) (P3HT) as an active semiconductor layer (p-type) was studied by using two different gate insulators (ZrO2 and PVA). The electrical performance output (Id-Vd) and transfer (Id-Vg) characteristics were investigated using the gradual-channel approximation model. The device shows a typical output curve of a field-effect transistor (FET). The analysis of electrical characterization was performed in order to investigate the source-drain voltage (Vd) dependent current and the effects of gate dielectric on the electrical performance of the OFET. This work also considered the effects of the capacitance semiconductor on the performance OFETs. The value
... Show MoreWe study in this paper the composition operator that is induced by ?(z) = sz + t. We give a characterization of the adjoint of composiotion operators generated by self-maps of the unit ball of form ?(z) = sz + t for which |s|?1, |t|<1 and |s|+|t|?1. In fact we prove that the adjoint is a product of toeplitz operators and composition operator. Also, we have studied the compactness of C? and give some other partial results.
We report on using a CO2 (10.6 µm) laser to debond the lithium disilicate veneers. Sixty-four sound human premolar teeth and 64 veneer specimens were used in the study. The zigzag movement via CO2 laser handpiece along with an air-cooled jet to prevent temperature elevation above the necrosis temperature limit (5.5 C°) was applied. The optimal deboning irradiation time was super-fast, at about 5 seconds at 3 Watt CO2 laser power. It is 20 times less than any previously published work for veneers debonding. The enamel beneath the debonded veneers has been assessed by atomic force microscopy (AFM) and shear stress technique as criteria for the easiness of debonding. The
... Show More