Palladium nanoparticles are produced by Polyol method. The characterization of the Pd nanoparticle has been conducted by various techniques such as SEM and AFM. The results of Pd powder showed that the particle size is directly proportional to the temperature and the reaction time. The optimum conditions for obtaining minimum nanoparticles size are 45 oC reaction temperature and 60 min reaction time and the smaller particle size achieved is equal to 25 nm. The optical limiting of smaller size nanoparticles has been studied. The palladium nanoparticles appear to be attractive candidates for optical limiting applications.
Herein, a cost-effective bio approach using extract derived from desert truffles (Tirmania nivea) is utilized to synthesize gold nanoparticles (AuNPs). AuNPs were thoroughly investigated using UV–vis, XRD, SEM, and TEM analyses. It was shown that nanoparticles had an fcc structure with a smooth spherical surface, an average diameter of 9.44 ± 0.26 nm, and an SPR band observed at 548 nm. Investigations were conducted on AuNPs' antibacterial and anti-cancer properties of prostate cancer cells. The findings suggest that AuNPs showed better antibacterial effects against S. aureus compared to E. coli, P. aeruginosa, and K. pneumoniae. AuNPs’ combination with antibiotics demonstrated a synergistic effect with significant antibacterial activi
... Show MoreIn wide range of chemical, petrochemical and energy processes, it is not possible to manage without slurry bubble column reactors. In this investigation, time average local gas holdup was recorded for three different height to diameter (H/D) ratios 3, 4 and 5 in 18" diameter slurry bubble column. Air-water-glass beads system was used with superficial velocity up to 0.24 m/s. the gas holdup was measured using 4-tips optical fiber probe technique. The results show that the axial gas holdup increases almost linearly with the superficial gas velocity in 0.08 m/s and levels off with a further increase of velocity. A comparison of the present data with those reported for other slurry bubble column having diameters larger than
... Show MoreThe coefficient of performance of a window type Air-Conditioner system can be improved if a reduction in the work of compressor can be achieved by a suitable technique. The present study investigates the effect of dispersing a low concentration of TiO2 nanoparticles in the mineral oil based lubricant, as well as on the overall performance of a window type Air-Conditioner system using R22 as the working fluid. An enhancement in the COP of the refrigeration system has been observed and the existence of an optimum volume fraction noticed, with low concentrations of nanoparticles suspended in the mineral oil. Results showed that the average compressor work reduced by 13.3%, which ultimately resulted in an increase of 11.99% in the COP due to
... Show MoreObjective: The goal of this research is to load Doxorubicin (DOX) on silver nanoparticles coupled with folic acid and test their anticancer properties against breast cancer. Methods: Chitosan-Capped silver nanoparticles (CS-AgNPs) were manufactured and loaded with folic acid as well as an anticancer drug, Doxorubicin, to form CS-AgNPs-DOX-FA conjugate. AFM, FTIR, and SEM techniques were used to characterize the samples. The produced multifunctional nano-formulation served as an intrinsic drug delivery system, allowing for effective loading and targeting of chemotherapeutics on the Breast cancer (AMJ 13) cell line. Flowcytometry was used to assess therapy efficacy by measuring apoptotic induction. Results: DOX and CS-Ag
... Show MoreAims: This study was conducted to assess the effect of the addition of yttrium oxide (Y2O3) nanoparticles on the tensile bond strength, tear strength, shore A hardness, and surface roughness of soft-denture lining material. Materials and Methods: Y2O3 NPs with 1.5 and 2 wt.% were added into acrylic-based heat-cured soft-denture liner. A total of 120 specimens were prepared and divided into four groups according to the test to be performed (tensile bond strength, tear strength, surface hardness, and surface roughness). Results: There was a highly significant increase in tensile bond strength between the soft liner and the acrylic denture base, tear strength, and hardness at both concentrations as compared to the control group, whereas ther
... Show More