Nonlinear diffraction patterns can be obtained by focusing a laser beam through a thin slice of the material. Here, we investigated experimentally the formation of the far field nonlinear diffraction patterns of cw laser beam at 532 nm passing through a quartz cuvette containing multi-wall carbon nanotubes (MWCNT's) suspended in acetone and in DI water at concentrations of 0.030.wt.%, 0.045 wt.%, 0.060 wt.%, and 0.075 wt.%. Our results show that increasing the concentration of both types of suspensions (MWCNTs in acetone and MWCNTs DI water) led to increase in the number of pattern rings which indicates an increase in their nonlinear refractive indices. Moreover, MWCNTs DI water suspension at a concentration of 0.075 wt. % was more efficient for achieving a high optical nonlinearity.
A field experiment was conducted in the growth season 2019-2020 at the botanical garden of the Biology Department at the College of Education for Pure Sciences/Ibn Al-Haitham, University of Baghdad-Iraq. The experiments’ purpose is to determine the effects of different melatonin concentrations on some morphological and physiological characteristics of mung (Vigna radiata L.) plant under the influence of three periods of drought (5, 10, 15 days). The results were showed that the increasing of water stress periods had significant effects in the reducing rates of the studied characteristics, especially at the period 15 days. The external treatment of different concentrations of melatonin reduced the drought effects and that’s led to signif
... Show MoreAbstract
The aim of the current research is to extract the psychometric properties of Philip Carter's tests (for mental agility) according to the classical measurement theory. To achieve these goals, the researcher took a number of scientific steps to analyze Philip Carter's tests (for mental agility) according to the classical measurement theory. The researcher translated Philip Carter's (mental agility) tests from English into Arabic and then he translated them conversely. For the purpose of statistical analysis of paragraphs of the Philip Carter tests (mental agility) to extract the psychometric properties, the tests were applied to a sample of (1000) male and female students who were selected by cluster sampl
... Show More
Abstract
Personality is one of the most important elements that should be developed in university student. Thus, we have to develop the positive traits and neutralize the negative traits of students as well as we have to pay attention to the level of student achievement at the same time, the researcher designed a scale to measure the traits of study sample. The research come out with a number of recommendations and proposals, the most important of which Enhancing the positive characteristics of university students in order to reach them to the level of mature personality with mental health. Enhancing the positive role of the high level of achievement by motivating the stude
... Show MoreOptical fiber technology is without a doubt one of the most significant phases of the communications revolution and is crucial to our daily lives. Using the free version (2022) of RP Fiber Calculator, the modal properties for optical fibers with core radii (1.5−7.5) μm, core index (1.44−1.48) and cladding index (1.43−1.47) have been determined at a wavelength of 1000 nm. When the fiber core’s radius is larger than its operating wavelength, multimode fibers can be created. The result is a single-mode fiber in all other cases. All of the calculated properties, it has been shown, increase with increasing core radius. The modes’ intensity profiles were displayed.
A nanocrystalline CdS thin film with 100 nm thickness has been prepared by thermal evaporation technique on glass substrate with substrate temperature of about 423 K. The films annealed under vacuum at different annealing temperature 473, 523 and 573 K. The X-ray diffraction studies show that CdS thin films have a hexagonal polycrystalline structure with preferred orientation at (002) direction. Our investigation showed the grain size of thin films increased from 9.1 to 18.9 nm with increasing the annealing temperature. The optical measurements showed that CdS thin films have direct energy band gap, which decreases with increasing the annealing temperature within the range 3.2- 2.85 eV. The absorbance edge is blue shifted. The absorption
... Show MoreEffect of [Cu/In] ratio on the optical properties of CuInS2 thin films prepared by chemical spray pyrolysis on glass slides at 300oC was studied. The optical characteristics of the prepared thin films have been investigated using UV-VIS spectrophotometer in the wavelength range (300-1100 nm). The films have a direct allow electronic transition with optical energy gap (Eg) decreased from 1.51 eV to 1.30 eV with increasing of [Cu/In] ratio and as well as we notice that films have different behavior when annealed the films in the temperature 100oC (1h,2h), 200oC (1h,2h) for [Cu/In]=1.4 . Also the extinction coefficient (k), refractive index (n) and the real and imaginary dielectric constants (ε1, ε2) have been investigated
In the present work we prepared heterojunction not homogenous CdS/:In/Cu2S) by spray and displacement methods on glass substrate , CdS:In films prepared by different impurities constration. Cu2S prepared by chemical displacement method to improve the junction properties , structural and optical properties of the deposited films was achieved . The study shows that the film polycrystalline by XRD result for all film and the energy gap was direct to 2.38 eV with no effect on this value by impurities at this constration .
The growing demand for optical fibers is due to their superior the ability to transmit information with high efficiency and minimal loss across extensive distances. In this study, four optical fibers with core radii ranging from (2.05-5.05) μm, and with a numerical aperture of 0.1624 were analyzed. The modal properties of these fibers were calculated at a wavelength of 1030 nm using the RP Fiber Calculator software (free version 2025). Furthermore, the impact of increasing the core radius on these properties was examined. The results showed that multimode fibers are formed when the core radius is much larger than the wavelength used. In contrast, single-mode fiber is obtained when th