Verrucae vulgares are commonly encountered. The present work is designed in an attempt to build a systematic procedure for treating warts by carbon dioxide laser regarding dose parameters, application parameters and laser safety.
Patients and Methods: The study done in the department of dermatology in Al-Najaf Teaching Hospital in Najaf, Iraq. Forty-two patients completed the study and follow up period for 3 months. Recalcitrant and extensive warts were selected to enter the study. Carbon dioxide laser in a continuous mode, in non-contact application, with 1 mm spot size was used. The patients were divided into two groups. The first group of patients consisted of 60 lesions divided to 6 equal groups, in whom we use different outputs and two modes of application (helical and radial) to assess the optimal power density and the best mode of application. The second group consisted of 75 lesions treated with output of 10 W continuous mode using helical mode of application.
Results: The optimal power was found to be 10 W. In the second group of patients, after 1 - 6 passes of laser (median 2.8 pass), complete clearance of the lesion was noticed in 56 lesions with a cure rate of 74.6%. This was found in 32 (68%) recalcitrant lesions and 24 (85.7%) lesions that had no previous treatment. The main complications were scarring in 17(22.5%) lesions and hyperpigmentation in 7 (12.5%) lesions. Post-operative infection was noticed in 4 (6%) lesions that were larger than 2 cm in diameter.
Conclusion: Carbon dioxide laser therapy of recalcitrant and extensive viral warts should be considered as a viable alternative to other more traditional techniques. This treatment offers good results in eliminating the verrucae and minimizing the squeals of recurrence, scarring and the post-operative pain.
Stimulative effect of 10 mW He-Ne laser on the phagocytic activity of human polymorphonuclear leukocytes( PMNs) has been studied in vitro. Normal polymorphonuclear leucocytes were isolated from the human peripheral blood. A mixture of 0.25 ml of Hanks solution, 0.25 ml of serum, 0.25 ml of Candida albicans suspension and 0.25 ml of PMNs suspension was prepared. The samples of mixture of PMNs and Candida were subdivided in 1 ml ependrof tubes and irradiated to He-Ne laser for 1, 3, 5, 10 and 20 min. The diameter of the irradiated area was 0.8 cm. For calculation of Phagocytic index before and after irradiation, the samples were incubated (37°C) at 5, 15, 30, 60 min. The slides of samples were prepared and stained using Giemsa stain. The
... Show MoreBackground: Low-level laser therapy (LLLT) has been extensively applied to improve wound healing due to some biostimulatory properties presented by laser arrays apparently able to accelerate the repair of soft tissue injuries. However, the role of proinflammatory interlukines not been studied yet. IL_1 ? represent one of the most important poroinflammatory interlukines that involved in wound healing. The goal of this study was to investigate the effect of 790-805nm diode laser on the expression of IL_1 ? during wound healing in mice. Materials and Methods: Standard-sized wounds (1.5cm) were carried out in the face of 96 white albino mice. Half of them underwent LLLT treatment (360 J/cm 2) at 790-805 nm delivered immediately after wound pro
... Show MoreThe influence of sintering and annealing temperatures on the structural, surface morphology, and optical properties of Ag2Cu2O4 thin films which deposited on glass substrates by pulsed laser deposition method have been studied. Ag2Cu2O4 powders have polycrystalline structure, and the Ag2Cu2O4 phase was appear as low intensity peak at 35.57o which correspond the reflection from (110) plane. Scan electron microscopy images of Ag2Cu2O4 powder has been showed agglomerate of oxide particles with platelets shape. The structure of thin films has been improved with annealing temperature. Atomic Force micrographs of Ag2Cu2O4 films showed uniform, homogenous films and the shape of grains was almost spherical and larger grain size of 97.85 nm has o
... Show MoreAims: This study was done to investigate the effect of low energy laser therapy on bone healing at the extraction site. Materials and methods:(24) male albino rats were exposed to the extraction procedure of the maxillary first molar on the first day of a seven day experiment and these animals were divided into two main groups; the control group and the laser group. The laser experiment involved using (Ga-As infrared diode laser) from optodent by directing the probe over the extraction site. The control group consisted of 4 rats, and the laser group was subdivided into 5 subgroups of 4 rats each. The laser dose was as follows: B1: a single dose of 5 minutes immediately after extraction.,
... Show MoreBackground: The irradiation of teeth with a laser results in an interaction between the light and the biological constituents of the dental hard substance, which is converted directly into heat.This thermal effect is the cause of the structural and chemical enamel changes.The combined treatment of topical fluoride agent with laser may increase fluoride uptake, and reduce progression of caries-like lesions. The aim of this study was to measure the uptake of the acidulated phosphate fluoride and sodium fluoride to the buccal and lingual caries-like lesion enamel surfaces before and after irradiated by Nd-YAG laser in comparison with matching control group. Materials and methods: The sample consisted of 30 human healthy upper premolar teeth wh
... Show MoreAim of the study: Using surface roughness and tensile bond strength tests, the objective of this investigation was to ascertain the impact of laser surface modification on the binding strength of injectable thermoplastic acrylic denture base material to acrylic-based soft-liner material. Materials and methods: Acrylic base soft liner material was bonded to injectable thermoplastic acrylic resin (Deflex). Forty specimens were created (20 disc, 20 dumbbells) 10 of each specimen type as control specimens, and 10 were treated with nano pulse Nd: YAG laser. The data were analyzed using the Kruskal-Wallis test and unpaired t-test (a=.05) and the roughness test was performed utilizing a double column universal test machine. Results: Compar
... Show MoreIn the present work, heterojunction diode detectors will be prepared using germanium wafers as a substrate material and 200 nm tin sulfide thickness will be evaporated by using thermal evaporation method as thin film on the substrate. Nd:YAG laser (λ=532 nm) with different energy densities (5.66 J/cm2 and 11.32 J/cm2) is used to diffuse the SnS inside the surface of the germanium samples with 10 laser shots in different environments (vacuum and distilled water). I-V characteristics in the dark illumination, C-V characteristics, transmission measurements, spectral responsivity and quantum efficiency were investigated at 300K. The C-V measurements have shown that the heterojunction were of abrupt type and the maximum value of build-in pot
... Show MoreIn this study, gold nanoparticle samples were prepared by the chemical reduction method (seed-growth) with 4 ratios (10, 12, 15 and 18) ml of seed, and the growth was stationary at 40 ml. The optical and structural properties of these samples were studied. The 18 ml seed sample showed the highest absorbance. The X- ray diffraction (XRD) patterns of these samples showed clear peaks at (38.25o, 44.5o, 64.4o, and 77.95o). The UV-visible showed that the absorbance of all the samples was in the same range as the standard AuNPs. The field emission-scanning electron microscope (FE-SEM) showed the shape of AuNPs as nanorods and the particle size between 30-50 nm. Rhodamine-610 (RhB) was prepared at 10<
... Show MoreThe electrical properties of pure NiO and NiO:Au Films which are
deposited on glass substrate with various dopant concentrations
(1wt.%, 2wt%, 3wt.% and 4wt.%) at room temperature 450 Co
annealing temperature will be presented. The results of the hall effect
showed that all the films were p-type. The Hall mobility decreases
while both carrier concentration and conductivity increases with the
increasing of annealing temperatures and doping percentage, Thus,
indicating the behavior of semiconductor, and also the D.C
conductivity from which the activation energy decrease with the
doping concentration increase and transport mechanism of the charge
carriers can be estimated.
Incident laser power and concentration effects on fluorescence emission from DCM dye in PMMA polymer have been investigated. Different concentrations of the dye were used. It was found that the fluorescence intensity increased with increasing of the concentration of the dye, with a red shift. In addition, it was found that the fluorescence intensity increased with the increase of the incident laser power I0.