The oxidation desulphurization assisted by ultrasound waves was applied to the desulphurization of heavy naphtha. Hydrogen peroxide and acetic acid were used as oxidants, ultrasound waves as phase dispersion, and activated carbon as solid adsorbent. When the oxidation desulphurization (ODS) process was followed by a solid adsorption step, the performance of overall Sulphur removal was 89% for heavy naphtha at the normal condition of pressure and temperature. The process of (ODS) converts the compounds of Sulphur to sulfoxides/ sulfones, and these oxidizing compounds can be removed by activated carbon to produce fuel with low Sulphur content. The absence of any components (hydrogen peroxide, acetic acid, ultrasound waves and activated carbon) from the ODS process leading to reduce the performance of removal, hydrogen peroxide was the most crucial factor. The ultrasound waves increase the dispersion of carbon, water and oil phase, promotes the interfacial mass transfer, and this leads to accelerates the reaction. The ultrasound waves did not affect the chemical or physical properties of the fuel. The chemical analysis of treated fuel oil showed that <1% of the hydrocarbon fuel compounds were oxidized in the ODS process. In this work, desulphurization by oxidation is the main mechanism was tested with several parameters that effects desulphurization efficiency such as sonication time (5-40) min, activated carbon (0.01-0.5) gm, hydrogen peroxide (1-30) ml, and acetic acid (1-15) ml. It was found that the hydrogen peroxide amounts lead to increase oxidation rates of Sulphur compounds so, the desulphurization efficiency increases. The optimum amounts of oxidants are 10 ml hydrogen peroxide per 100 ml of heavy naphtha. Increasing the amount of acid catalyst lead to increase Sulphur removal, it was found that7.5 ml acid per 10 ml oxidant was the optimum amount. Activated carbon as a solid adsorbent and reaction enhancer with 0.1gm weight was found as the optimum amount for 100 ml heavy naphtha. Increasing sonication time lead to increase desulphurization rate, it was found that (10 min) is the optimum period. By applying the optimum parameters 89% of sulfur can be removed from heavy naphtha with 598.4 ppm Sulphur content.
Gypseous soils represented one of the most complex salty soils that faced the geotechnical engineers. Structures that built on gypsum soil will undergo unexpected distortions that will eventually contribute to catastrophic failure. The purpose of this article is to understand the durability of gypsum soil against wetting drying cycles after improvement with polyurethane polymer especially investigate the effect of the wetting-drying cycle on collapsibility. The soil was brought from Sawa lake in AL-Muthanna Governorate in Iraq, with gypsum content 65.5%, A set of Odometer tests were performed to determine the collapsibility potential (CP) for treated and untreated gypsum soil. The result shows that adding a different per
... Show MoreAG Al-Ghazzi, 2009
Petroleum is one of the most important substances consumed by man at present times, a major energy source in this century, petroleum oils can cause environmental pollution during various stages of production, transportation, refining and use, petroleum hydrocarbons pollutions ranging from soil, ground water to marine environment, become an inevitable problem in the modern life, current study focused on bioremediation process of hydrocarbons contaminants that remaining in the bottom of gas cylinders and discharged to the soil. Twenty-four bacterial isolates were isolated from contaminated soils all of them gram negative bacteria, bacterial isolates screening to investigate the ability of biodegradation of hydrocarbons, these isolates
... Show MoreSimple, sensitive and economical spectrophotometric methods have been developed for the determination of cefixime in pure form. This method is based on the reaction of cefixime as n-electron donor with chloranil to give highly colored complex in ethanol which is absorb maximally at 550 nm. Beer's law is obeyed in the concentration ranges 5-250 µg ml-1 with high apparent molar absorptivities of 1.52×103 L.mole-1. cm-1.
Activated carbon was Produced from coconut shell and was used for removing sulfate from industrial waste water in batch Processes. The influence of various parameter were studied such as pH (4.5 – 9.) , agitation time (0 – 120)min and adsorbent dose (2 – 10) gm.
The Langmuir and frandlich adsorption capacity models were been investigated where showed there are fitting with langmmuir model with squre regression value ( 0.76). The percent of removal of sulfate (22% - 38%) at (PH=7) in the isotherm experiment increased with adsorbent mass increasing. The maximum removal value of sulfate at different pH experiments is (43%) at pH=7.
Leishmaniasis is endemic ofIraq in both cutaneous and visceral form. The available tools for diagnosis and detection of Leishmaniaare nonspecific and may interfere with other species. In this study, Polymerase Chain Reaction (PCR) has been used to identify Iraqi isolate of visceral leishmaniasis (MHOM/ IQ/2005/MRU15) which a previously diagnosed by classical serological tests. PCR amplificationwas carried out using species-specific primers of Leishmania donovani. Four primer pairs of mini-circle DNA and ITS-1 were used.13A/13B, which is used to identify Leishmaniaas a genus, NM12, LITSR/L5.8S and BHUL18S, were used to detect the sub species of L. donovani.The result ofPCR
... Show More