Preferred Language
Articles
/
ijcpe-433
The Effect of Ageing on Physical and Chemical Properties of Asphalt Cement
...Show More Authors

Two grades of paving asphalt with penetration of 46 and 65 are studied for determining changes in their physical and chemical properties caused by ageing.
The ageing process has been conducted on two petroleum paving asphalt cement using thin film oven test at 150, 163 and 175 C, and ageing time 5, 10,15, 20, 25 and 30 hours. The effect of ageing time and temperature on penetration, kinematic viscosity, softening point, solubility in trichloroethylene, heat loss and changes in chemical composition are investigated. The results of thin film oven test process indicte that the asphaltenes concentration of all aged asphalt increases with increasing ageing time, while the opposite was observed for polar-aromatic and naphthene-aromatic. The saturate of low penetration grade asphalt is higher than that for high penetration grade asphalt and remained unchanged with ageing time. Th kinematic viscosity and softening point seem to increase with increasing ageing time, while the penetration decreases with increasing ageing time. The DI of aged asphalt inreases with increasing ageing time.

View Publication Preview PDF
Quick Preview PDF
Publication Date
Mon Nov 17 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Selected salivary constituents, physical properties and nutritional status in relation to dental caries among 4-5 year’s old children (Comparative study)
...Show More Authors

Background: Tooth decay is still one of most common diseases of childhood, child’s primary teeth are important even though they aretemporary. This study was conducted to assess the physiochemical characteristic of saliva among caries experience preschool children and compared them with caries free matching in age and gender. Then an evaluation was done about these salivary characteristics to dental caries and evaluated the relation of body mass index to dental caries and to salivary variables. Materials and method: After examination 360 children aged 4-5 years of both gender. Caries-experiences was recorded according to dmfs index by (World Health Organization criteria 1987) during pilot study children with caries experience was di

... Show More
View Publication Preview PDF
Publication Date
Thu Jul 07 2011
Journal Name
Arabian Journal Of Geosciences
Mineralogy, geochemistry, and reserve estimation of the Euphrates limestone for Portland cement industry at Al-Najaf area, South Iraq
...Show More Authors

View Publication
Scopus (23)
Crossref (6)
Scopus Clarivate Crossref
Publication Date
Sat Mar 01 2008
Journal Name
Al-khwarizmi Engineering Journal
Evaluation of Hydrated Lime Filler in Asphalt Mixtures
...Show More Authors

Mineral filler is one of important  materials and affecting on properties and quality of asphalt mixtures .There are different types of mineral filler depended on cost and quality , the matter encourages us to achieve this study to evaluate hydrated lime filler effects on properties of asphalt mixes related with strength and durability. Conventional asphaltic concrete mixtures with Portland cement and soft sandstone fillers and mixtures modified with hydrated lime were evaluated for their fundamental engineering properties as defined by Marshall properties , index of retained strength , indirect tensile strength , permanent deformation characteristics , and fatigue resistance .A typical dense graded mixture employed in construction

... Show More
View Publication Preview PDF
Publication Date
Sun Jan 01 2012
Journal Name
7th Rilem International Conference On Cracking In Pavements
Mechanistic Evaluation of Lime-Modified Asphalt Concrete Mixtures
...Show More Authors

Frequently, Load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some sections poorly drained are the main failure types found in some of the newly constructed road within Baghdad as well as other cities in Iraq. The use of hydrated lime in pavement construction could be one of the possible steps taken in the direction of improving pavement performance and meeting the required standards. In this study, the mechanistic properties of asphalt concrete mixes modified with hydrated lime as a partial replacement of limestone dust mineral filler were evaluated. Seven replacement rates were used; 0, 0.5, 1, 1.5, 2, 2.5 and 3 percent by weight of aggregate. Asphalt concrete mixes were prepared at their

... Show More
View Publication
Crossref (9)
Crossref
Publication Date
Tue May 01 2018
Journal Name
Journal Of Engineering
Performance Evaluation of Plant Produced Warm Mix Asphalt
...Show More Authors

Warm mix asphalt (WMA) is relatively a new technology which enables the production and compaction of asphalt concrete mixtures at temperatures 15-40 °C lower than that of traditional hot mix asphalt HMA. In the present work, six asphalt concrete mixtures were produced in the mix plant (1 ton each) in six different batches. Half of these mixes were WMA and the other half were HMA.  Three types of fillers (limestone dust, Portland cement and hydrated lime) were used for each type of mix. Samples were then taken from these patches and transferred to lab for performance testing which includes: Marshall characteristics, moisture susceptibility (indirect tension test), resilient modulus, permanent deformation (axial repeated load test)

... Show More
Preview PDF
Crossref (9)
Crossref
Publication Date
Tue May 01 2018
Journal Name
Journal Of Engineering
Performance Evaluation of Plant Produced Warm Mix Asphalt
...Show More Authors

Warm mix asphalt (WMA) is relatively a new technology which enables the production and compaction of asphalt concrete mixtures at temperatures 15-40 °C lower than that of traditional hot mix asphalt HMA. In the present work, six asphalt concrete mixtures were produced in the mix plant (1 ton each) in six different batches. Half of these mixes were WMA and the other half were HMA.  Three types of fillers (limestone dust, Portland cement and hydrated lime) were used for each type of mix. Samples were then taken from these patches and transferred to lab for performance testing which includes: Marshall characteristics, moisture susceptibility (indirect tension test), resilient modulus, permanent deformation (axial repe

... Show More
View Publication Preview PDF
Crossref (9)
Crossref
Publication Date
Wed Mar 01 2006
Journal Name
Journal Of Engineering
Production of Graphite Electrodes Binder from Iraqi Asphalt
...Show More Authors

Basrah crude oil Vacuum residue 773+ K with specific gravity 1.107 and 4.87wt. % sulfur, was treated with hexane commercial fraction provided from Al-Taji Gas Company for preparing deasphaltened oil(DAO)suitable for hydrotreating process. Deasphaltening was carried out with 1h mixing time, 10ml:1g solvent to oil ratio and at room temperature. Hexane deasphaltened oil was hydrotreated on presulfied commercial Co-Mo/γ-Al2O3 catalyst in a trickle bed reactor. The hydrotreating process was carried out at temperature 660 K,LHSV 1.3 h^ –1, H2/oil ratio 300 l/l and constant pressure of 4MPa. The hydrotreated product was distillated under vacuum distillation unit. It is found that the mixture of 75% of vacuum residue with 25% anthracene satisfie

... Show More
View Publication Preview PDF
Publication Date
Thu Dec 01 2011
Journal Name
Journal Of Engineering
MECHANISTIC EVALUATION OF LIME-MODIFIED ASPHALT CONCRETE MIXTURES
...Show More Authors

Frequently, Load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some sections poorly drained are the main failure types found in some of the newly constructed road within Baghdad as well as other cities in Iraq. The use of hydrated lime in pavement construction could be one of the possible steps taken in the direction of improving pavement performance and meeting the required standards. In this study, the mechanistic properties of asphalt concrete mixes modified with hydrated lime as a partial replacement of limestone dust mineral filler were evaluated. Seven replacement rates were used; 0,0.5, 1, 1.5, 2, 2.5 and 3 percent by weight of aggregate. Asphalt concrete mixes were prepared at their

... Show More
View Publication Preview PDF
Crossref
Publication Date
Thu Jun 08 2023
Journal Name
Open Engineering
A review of rutting in asphalt concrete pavement
...Show More Authors

Undoubtedly, rutting in asphalt concrete pavement is considered a major dilemma in terms of pavement performance and safety faced by road users as well as the road authorities. Rutting is a bowl-shaped depression in the wheel paths that develop gradually with the increasing number of load applications. Heavy axle loadings besides the high pavement summer temperature enhance the problem of rutting. According to the AASHTO design equation for flexible pavements, a 1.1 in rut depth will reduce the present serviceability index of relatively new pavement, having no other distress, from 4.2 to 2.5. With this amount of drop in serviceability, the entire life of the pavement in effect has been lost. Therefore, it is crucial to look at the mechani

... Show More
View Publication
Scopus (32)
Crossref (27)
Scopus Clarivate Crossref
Publication Date
Tue May 30 2017
Journal Name
Environmental Earth Sciences
Purification of aqueous solutions from Pb(II) by natural bentonite: an empirical study on chemical adsorption
...Show More Authors

View Publication
Scopus (15)
Crossref (8)
Scopus Clarivate Crossref