Spent hydrodesulfurization (Co-Mo/γ-Al2O3) catalyst generally contains valuable metals like molybdenum (Mo), cobalt (Co), aluminium (Al) on a supporting material, such as γ-Al2O3. In the present study, a two stages alkali/acid leaching process was conducted to study leaching of cobalt, molybdenum and aluminium from Co-Mo/γ-Al2O3 catalyst. The acid leaching of spent catalyst, previously treated by alkali solution to remove molybdenum, yielded a solution rich in cobalt and aluminium.
Thirty three specimens of the blue-cheeked bee-eater were collected at central and southern Iraq from April 1997 to October 2000. Two nematodes Hadjelia truncata and Syphaciella capensis, were recovered from the alimentary tract. Reporting these two nematodes represents the first record for Iraq as well as a new host record.
The objective of this study is to determination the content of some heavy metals (lead, cadmium, chromium) in colored tattoo stickers. twelve kinds of colored tattoo stikcers were collected from Baghdad markets, it was estimated heavy metals using atomic absorption spectrophotometer (Shimadzu A5000). The results indicated the concentrations of lead in all samples (1.61_1.00 mg / kg) and chromium in the three samples (0.85_0.97 mg / kg) while other samples are free of chromium , and cadmium. These elements are the components of printing inks and dyes in tattoo stickers, and this does not conform to the health and safety conditions for the packaging of food according to the organizations of the health and safety of
... Show MoreIn this research, the performance of a two kind of membrane was examined to recovering the nutrients (protein and lactose) from the whey produced by the soft cheese industry in the General Company for Food Products inAbo-ghraab.Wheyare treated in two stages, the first including press whey into micron filter made of poly vinylidene difluoride (PVDF) standard plate type 800 kilo dalton, The membrane separates the whey to permeate which represent is the main nutrients and to remove the fat and microorganisms.The second stage is to isolate the protein by using ultra filter made of polyethylsulphone(PES)type plate with a measurement of 10,60 kilo dalton and the recovery of lactose in the form of permeate.
The results showed that the percen
Background: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD c
... Show MoreAbstract :In this study, amygdaline in Iraqi plant seeds was extracted and isolated from their seeds matrix using reflux procedure and subsequently identified and determined by high performance liquid chromatography (HPLC) on reversed phase column of LC-18 (150mm x 4.6mm, 5?m )with actonitrile :water ( 50 : 50 ) as mobile phase at flow rate of ( 0.5 mL/min ) and detection at wavelength of 215 nm.The experimental results indicated that the linearity of calibration is in the range of 1.0-30.0 mg L-1amygdaline with the correlation coefficient of 0.9949. The limit of detection (LOD) and limit of quantitation (LOQ) for amygdaline were of 0.88 and 2.93 mg L-1 in standard pure sample. The mean recovery percent is 97.34±0.58 at 95% confidence inte
... Show MoreAlPO4 catalysts supported with WO3 were prepared by impregnating the catalysts with ammonium metatungstate. The catalysts were checked by X-ray Diffraction (XRD), AFM, and SEM; also, the catalysts analysis was done by X-Ray (EDX). Finally, the N2 adsorption-desorption was used to measure the pore volume and surface area of the catalyst. The prepared catalyst has a surface area of 185.83 m2/g, pore volume of 0.645 cm3/g at a calcination temperature of 500°C for 3 hrs, and particle size of AlPO4 with an average of 35.36 nm. Transesterification of edible oil using WO3/AlPO4 was performed, it was observed that WO3/AlPO4 catalysts give high conversion of edible oil, and this is attributed to the high surface area, smaller particle size, and the
... Show MoreThis work deals with the production of light fuel cuts of (gasoline, kerosene and gas oil) by catalytic cracking treatment of secondary product mater (heavy vacuum gas oil) which was produced from the vacuum distillation unit in any petroleum refinery. The objective of this research was to study the effect of the catalyst -to- oil ratio parameter on catalytic cracking process of heavy vacuum gas oil feed at constant temperature (450 °C). The first step of this treatment was, catalytic cracking of this material by constructed batch reactor occupied with auxiliary control devices, at selective range of the catalyst –to- oil ratio parameter ( 2, 2.5, 3 and 3.5) respectively. The conversion of heavy vacuum gas
... Show MoreThe present study was invistigated to show the bioaccumulation of some heavy metals (Cd, Co, Cr, Cu, Fe, Mn, Ni, Pb, Zn) by use Aquatic plant Myriophyllum verticilatum growing in Euphrates river between Spring 2004 to Winter 2005, and these heavy maters was studied in Dissolved and particulat phase of water and exchangable and residual phase of sediment. Heavy metals accumulated according the system water-sediment-aquatic plant, and recorded bioaccumulation factor 1.010, 0.005, 0.009, 0.011, 0.012, 0.010, 0.010, 0.010, 0.011, respectively.
The aim of this work is to study the factors that affect the welding joint of dissimilar metals. Austenitic stainless steel-type AISI (316L) with a thickness of (2mm) was welded to carbon steel (1mm) using an MIG spot welding. The filler metal is a welding wire of the type E80S-G (according to AWS) is used with (1.2mm) diameter and CO2 is used as shielding gas with flow rate (7L/min) for all times was used in this work.
The results indicate that the increase of the welding current tends to increase the size of spot weld, and also increases the sheer force. Whereas the sheer force increased inversely with the time of welding. Furthermore, the results indicate that i
... Show More