PPSU hollow fiber nanofiltration membranes are prepared by applying two concentrations and various extrusion pressures according to the phase inversion method. Cross-sectional area and outer structures were characterized by using scanning electron microscope (SEM) and atomic force microscopy (AFM). In additional to the pore size distribution, either the mean roughness or the mean pore size of the PPSU hollow fiber surfaces was evaluated by AFM. It was found that the morphology of the PPSU fibers had both sponge-like and finger-like structures through different extrusion pressures and PPSU concentrations. The mean pore size and mean roughness for inner and outer surfaces were seen to be decreased with the increase of extrusion pressure at two different PPSU concentrations. Moreover, the lead ion rejection was significantly improved from 19 to 78 % with increasing the extrusion pressure from 2.5 to 3 bar at 25 wt.% PPSU concentration.
The silicon carbide/carbon fiber (SiC/CF) hybrid fillers were introduced to improve the electrical and thermal conductivities of the epoxy resin composites. Results of Fourier transform infrared spectroscopy revealed that the peaks at 3532 and 2850 cm−1 relate to carboxylic acid O–H stretching and aldehyde C–H stretching appearing deeper with an increased volume fraction of SiC. Scanning electron microscopic image shows a better interface bonding between the fiber and the matrix when the volume fraction of SiC particles are increased. As frequency increases from 102 Hz to 106 Hz, dielectric constants decrease slightly. Dissipation factor (tan δ) values keep low a
... Show MoreThe analysis of rigid pavements is a complex mission for many reasons. First, the loading conditions include the repetition of parts of the applied loads (cyclic loads), which produce fatigue in the pavement materials. Additionally, the climatic conditions reveal an important role in the performance of the pavement since the expansion or contraction induced by temperature differences may significantly change the supporting conditions of the pavement. There is an extra difficulty because the pavement structure is made of completely different materials, such as concrete, steel, and soil, with problems related to their interfaces like contact or friction. Because of the problem's difficulty, the finite element simulation is
... Show MoreCarbon fiber reinforced polymers (CFRP) were widely used in strengthening reinforced concrete members
in the last few years, these fibers consist mainly of high strength fibers which increase the member capacity in addition to changing the mode of failure of the reinforced concrete beams. Experimental and theoretical investigations were carried to find the behavior of reinforced concrete beams strengthened by CFRP in shear and bending. The experimental work included testing of 12 beams divided into 4 groups; each group contains 3 beams. The following parameters were taken into consideration: - Concrete crushing strength. - CFRP strengthening location (shear strengthening and both shear and flexure strengthening). Reinforced beams were
To enhance interfacial bonding between carbon fibers and epoxy matrix, the carbon fibers have been modified with multiwall carbon nanotubes (MWCNTs) using the dip- coating technique. FT-IR spectrum of the MWCNTs shows a peak at 1640 cm−1 corresponding to the stretching mode of the C=C double bond which forms the framework of the carbon nanotube sidewall. The broad peak at 3430 cm−1 is due to O–H stretching vibration of hydroxyl groups and the peak at 1712 cm−1 corresponds to the carboxylic (C=O) group attached to the carbon fiber. The peaks at 2927 cm−1 and 2862 cm−1 ar
The aim of this research is to benefit from recycl the aircraft waste oils which is discarded in sewage network, to be used in preparation of greases for industrial purposes and to reduce the environmental pollution. In this research synthetic greases were prepared with special specifications by mixing the waste oils after treating with (silica gel as adsorbent agent, and filtration to precipitate impurities then heated to 110 C? to get rid of water) bentonite produced in Iraq which is available and cheap with existence of high density polyethylene at specific conditions of ( heating and mixing) . The best weight proportion were reached, then paraffin wax and additives were added to improve the properties of grease and give the
... Show MoreAbstract: In this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
In this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
Polyvinyl alcohol, (PVA) was prepared using polyvinyl acetate emulsion (manufactured by Al-Jihad factory,
That-Al-Sawary Company) as a local raw material. In this investigation, polyvinyl acetate emulsion was converted to
solid form by coagulation the polymer from its emulsion using sodium sulphate salt as coagulant aid, then alcoholyzed
the solid polyvinyl acetate in methanol using sodium hydroxide as catalyst, polyvinyl alcohol produced by this method is
a dry, white to yellow powder.
Three affecting variables on the degree of hydrolysis of PVA were studied, these variable are Catalyst to
polymer weight ratio in the range of 0.01 – 0.06, reaction time in the range of 20 – 90 min, and reaction temperature in
the
Objective: The purpose of this work was to develop and optimize the emulgel formulation of piroxicam with two types of gelling agent chitosan and xanthan gum. The release profiles of prepared formulas were investigated. In addition, the rheology and stability of the best formula were investigated.Methods: Emulsified piroxicam was prepared to use oleic acid, tween 80 and PG with a ratio (3:10:10). In xanthan based emulgel, the xanthan gum (1% and 1.5%) was spread as powder on emulsified piroxicam with stirring until emulgel was formed. In chitosan-based emgels, Chitosan gel was added to emulsified piroxicam and stirring until the Emulgel was constructed. Chitosan gels were prepared by incorporating different concentration, 2%, 3%, 6%
... Show More