ATTAPULGITE clay was modified in this study by the graphene oxide sheets and the clay was diagnosed before and after modification using several techniques (Fourier-transform infrared spectroscopy FT-IR, X-ray powder diffraction XRD, Scanning electron microscope SEM , energy dispersive spectroscopy EDX ) ,The surface of the attapulgite clay (before (Ata) after modification by graphene oxide (Ata-GO) ) was applied to adsorption of the Alizarin dye from its water solutions through the application of several kinetic models (pseudo first-order model , pseudo second -order model , intraparticle diffusion model ),It was found that the practical results follow pseudo second -order model. The process of modification on the surface of the mud has improved the adsorption properties where the quantity dye adsorbed is equal to (55,81) mg/g by the surfaces (Ata ,Ata-GO) respectively.
The aim of the current research is to study the effect of adding green tea to the edible film prepared from the whey protein isolate on the effectiveness of microorganisms and evaluating the of antimicrobial effectiveness of these films on Iraqi soft cheese packaging during the nine days of storage as an alternative to commercial packaging. At the beginning of the study, the minimum inhibitory concentration was measured by calculate the diameter of the zone of inhibition on growth of the bacteria and it's included the group of Gram negative bacteria (Escherichia coli, Salmonella spp, Pseudomonas Aeruginosa) and the group of Gram positive bacteria (Staphylococcus Aureus, Bacillus spp) and a yeast (Candida Albican). Where the diameter of t
... Show MoreABSTRACT. The reaction between benzil and hexamethylenediamine formed a new ligand [L], [(1Z,3Z)-2,3-diphenyl-5,6,7,8,9,10-hexahydro-1,4-diazecine], of the type [N2], was synthesized by the condensation reaction through Schiff base reaction between benzil and hexamethylenediamine. The new Schiff base ligand reacts with Mnп, Niп and Coп metal ions to give the complexes with the general formula: [M(L)Cl2]. The elemental investigations have been used to analyze the ligand and its complexes by CHN, FT-IR, UV-Vis, TLC, mass spectrum, melting point with the study of biological activity to the formed compounds. From the data obtained, the proposed molecular structure adopts square planar structure about the metal ions. The study reveals
... Show MoreAmoxicillin 1 was treated with thiosemicarbazide and Phosphoryl chloride to obtain a new derivatives that contains 1,3,4-thiadiazole moiety 2. Schiff bases compounds were synthesized by the reaction of compound 2 with different aldehydes such as benzaldehyde and some substituted Benzaldehyde; p-hydroy, p-Chloro, p-Nitro, p-Dimethylamino, p-Methyl, p-Methoxy, p-Ethoxy to give compounds 3a-h. The obtained compounds have tested towards gram -ve and gram +ve bacteria. The compound shows good to moderate result towards the bacteria.
In this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest degradation percent. In additio
... Show MoreIn this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest deg
... Show MoreIn this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest degradation percent. In additio
... Show MoreThe main objectives of this study were investigating the effects of the maximum size of coarse Attapulgite aggregate and micro steel fiber content on fresh and some mechanical properties of steel fibers reinforced lightweight self-compacting concrete (SFLWSCC). Two series of mixes were used depending on maximum aggregate size (12.5 and 19) mm, for each series three different steel fibers content were used (0.5 %, 1%, and 1.5%). To evaluate the fresh properties, tests of slump flow, T500 mm, V funnel time, and J ring were carried out. Tests of compressive strength, splitting tensile strength, flexural tensile strength, and calculated equilibrium density were done to evaluate mechanical properties. For reference mixes, the
... Show MoreIn this study, Zinc oxide nanostructures were synthesized via a hydrothermal method by using zinc nitrate hexahydrate and sodium hydroxide as a precursor. Three different annealing temperatures were used to study their effect on ZnO NSs properties. The synthesized nanostructure was characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Atomic force microscope (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Their optical properties were studied by using UV -visible spectroscopy. The XRD analysis confirms that all ZnO nanostructures have the hexagonal wurtzite structure with average crystallite size within the range of (30.59 - 34
... Show More