This study investigated the shear performance of concrete beams with GFRP stirrups vs. traditional steel stirrups. Longitudinal glass fiber‐reinforced polymer (GFRP) bars were used to doubly reinforce the tested beams at both the top and bottom of their cross sections. To accomplish this, several stirrup spacings were provided. Eight beam specimens, measuring 300 × 250 × 2400 mm, were used in an experimental program to test under a two‐point concentrated load with an equal span‐to‐depth ratio until failure. Four beams in Group I have standard mild steel stirrups of 8 mm diameter, while four beams in Group II have GFRP stirrups with the same adopted diameter. The difference between the beams in each group was mainly due to the spacing between the reinforcing stirrups in the constant shear and pure bending spans. The test matrix consists of two beams with shear reinforcement equally distributed at 100 mm and 200 mm in constant shear and pure bending spans, respectively. Stirrups were placed uniformly over the whole effective span of the other six beams. In two beams, stirrups were placed 100 mm apart; in the other two, 75 mm; and in the last two, 50 mm. Test outcomes showed that GFRP stirrups, as opposed to steel stirrups, decreased the ultimate load by around 8%–27% based on stirrup spacing, while reducing the stirrup spacing increased the shear capacity. Also, the presence of compression GFRP bars and GFRP stirrups in the pure bending span led to an increase in the flexural stiffness of the tested beams. Consequently, this increase contributed to a higher ductility index. Accordingly, it is essential to prioritize adequate shear strength above flexural strength when designing GFRP‐reinforced concrete beams, as evidenced by the continuous observation of flexure‐shear cracking as the primary mode of failure in almost all tested beams.
The main objective of this work was to adopt an environmentally friendly technology with enhanced results. The technology of magnetic water (MW) treatment system can be used in concrete mixture production instead of potable water (PW) to improve both workability and strength. Two types of concrete were adopted: normal concreter production with two grades 25 and 35 MPa and the self-compacted concrete (SCC) with 35 MPa grade. The concrete mixes containing MW instead of PW results showed that, for 25 MPa grade, an improvement in a compressive strength of 15.1, 14.8, and 10.2% was achieved for 7, 28, and 90 days, respectively. For 35 MPa grade, an improvement of 13.6, 11.5, and
The main objective of this work was to adopt an environmentally friendly technology with enhanced results. The technology of magnetic water (MW) treatment system can be used in concrete mixture production instead of potable water (PW) to improve both workability and strength. Two types of concrete were adopted: normal concreter production with two grades 25 and 35 MPa and the self-compacted concrete (SCC) with 35 MPa grade. The concrete mixes containing MW instead of PW results showed that, for 25 MPa grade, an improvement in a compressive strength of 15.1, 14.8, and 10.2% was achieved for 7, 28, and 90 days, respectively. For 35 MPa grade, an improvement of 13.6, 11.5, and
The aim of the current study is to identify the effectiveness of cognitive conflict strategy in comprehending reading among literary fifth students in literature and literature texts. The researcher uses experimental method with partial control. The sample consisted of (80) students distributed into control and experimental groups. The scientific material, the behavioral goals, the teaching plans, and the instrument of the research have been prepared (reading comprehension test) by the researcher.
The instrument's validity and reliability have been calculated and then applied to the sample. After treating the data statistically by using SPSS, the results have revealed that there is a statistically significant difference at the si
... Show MoreThis study aims to evaluate the influence of the air abrasion of dentin on the shear bond strength of lithium disilicate using three different types of luting cements. Sixty cylindrical specimens were milled from lithium disilicate CAD/CAM blocks (IPSe.max CAD). Sixty sound human maxillary premolar teeth were decoronated to the level of peripheral dentin, then randomly divided into three groups according to the type of luting cement used for the cementation of the lithium disilicate specimens (n = 20); Group A: Glass ionomer cement (Riva Self- Cure); Group B: Adhesive resin cement (Rely X Ultimate); Group C: Self-adhesive resin cement (Rely X U200). Each group was then further subdivided into two subgroups (n=10); Subgroups AI, BI, and CI,
... Show MoreFire is the most sever environmental condition affecting on concrete structures, thus investigating for fire safet, IJSR, Call for Papers, Online Journal
Fire is the most sever environmental condition affecting on concrete structures, thus investigating for fire safety in structural concrete is important for building construction. The slow heat transfer and strength loss enables concrete to be effective for fire resistance. Concrete structures withstand when exposed to fire according to: their thermal properties, rate of heating, characteristic properties of concrete mixes and their composition and on the duration of fire, and concerned as thermal property with other factors such as loss of mass which affected by aggregate type, moisture content, and composition of concrete mix. The present research goal is to study the effect of rising temperature on the compressive strength of the rea
... Show MoreThe performance and durability of the asphalt pavement structure mainly depend on the strength of the bonding between the layers. Such a bond is achieved through the use of an adhesive material (tack coat) to bond the asphalt layers. The main objective of this study is to evaluate the effect of moisture in conjunction with repeated traffic loads on the strength of the bonding between asphalt layers using two types of tack coats with different application rates. Using the nominal maximum size of aggregate (NMAS), the layers were graded (25/19) and (19/9.5) mm. The slabs of multilayer asphalt concrete were prepared using a roller compactor using two types of tack coats to bond between layers, namely rapid curing cut back a
... Show MoreThe present study aimed to assess the potential impact of serum concentration of undercarboxylated osteocalcin (the active form of osteocalcin) and fibroblast growth factor-23 on the incidence of cardiovascular diseases in type 2 diabetics with carotid artery calcification and the possible association with metabolic changes in relation to glucose and minerals homeostasis.
This study included 52 men with carotid artery calcification type 2 diabetes mellitus. These patients were categorized; as follows: group A includes 30 patients who had cardiovascular disease and group B includes 22 patients who had no cardiovascular disease. These groups were compared with 25 apparently healthy control (Group C).
It has been shown
... Show More