An acidic environment causes surface changes of resin composites. Filler particlesize and filler distribution also have a direct effect on these surface changes. This invitro study evaluated the influence of Pepsi Cola drink on the surface roughness ofComposan LCM and Composan Ceram over time. Sixteen disc shaped specimens(10mm diameter, 2mm thickness) of each resin composite were fabricated, therebyforming two groups (n= 8). Surface roughness (Ra) was analyzed after 24 hrs beforeexposure to beverage. The specimens were submitted to a five minutes immersion inPepsi Cola three times daily interrupted by immersion in deionized distilled water (37C˚). Surface roughness measurements were done at 10, 30, and 60 days intervals. Datawere submitted to paired t-test. There was a statistically highly significant (p <0.001)increase in surface roughness values of the tested composites after 30 days and 60days immersion in Cola drink. Composan LCM exhibited a significantly (p <0.05)higher surface roughness values than Composan Ceram.The surface roughness of the composite materials are significantly affected byexposure to acidic drink over time, highly filled micro hybrid composites with smallfiller particle size are significantly more resistant to acid erosion.
Background: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets
... Show MoreIn this work, results from an optical technique (laser speckle technique) for measuring surface roughness was done by using statistical properties of speckle pattern from the point of view of computer image texture analysis. Four calibration relationships were used to cover wide range of measurement with the same laser speckle technique. The first one is based on intensity contrast of the speckle, the second is based on analysis of speckle binary image, the third is on size of speckle pattern spot, and the latest one is based on characterization of the energy feature of the gray level co-occurrence matrices for the speckle pattern. By these calibration relationships surface roughness of an object surface can be evaluated within the
... Show MoreBackground: This study was conducted to evaluate the surface roughness and dimensional accuracy of commercially obtainable alginate impression material in terms of imbibition after immersion in two different media. Materials and method: Two disinfecting agents, ethanol 70% and povidone-iodine 4%, were used to access the dimensional accuracy and surface roughness of alginate impression material. Weights of specimen discs of alginate impressions were measured before and immediately after immersion to gain a measure of imbibition. For surface roughness, disinfected specimens rectangle was examined before and after disinfection. Results: Minimal changes in weight were observed after disinfection, but a statistically non-significant differenc
... Show MoreShatt al-Arab is the only navigational artery in Iraq, extending from the city of Qurna to its mouth in the Arabian Gulf at the city of Al-Fao within the governorate of Basrah for a length of approximately 204 km. Its width ranges from 400 m to 2000 m, and its depth ranges from 8 m to 20 m. The southern part of it, 93 km long from Umm al-Rassas Island to Ras al-Bisha, represents the international border between Iraq and Iran, where the Thalweg line represents the border between the two countries, which is the deepest point in the riverbed (according to the 1975 Algiers Agreement). The western bank (the Iraqi side) within the common border of Shatt al-Arab is subject to continuous erosion, which leads to the shifting of t
... Show MoreElectro-chemical Machining is significant process to remove metal with using anodic dissolution. Electro-chemical machining use to removed metal workpiece from (7025) aluminum alloy using Potassium chloride (KCl) solution .The tool used was made from copper. In this present the optimize processes input parameter use are( current, gap and electrolyte concentration) and surface roughness (Ra) as output .The experiments on electro-chemical machining with use current (30, 50, 70)A, gap (1.00, 1.25, 1.50) mm and electrolyte concentration (100, 200, 300) (g/L). The method (ANOVA) was used to limited the large influence factors affected on surface roughness and found the current was the large influence f
... Show MoreBackground: Prophylaxis methods are used to mechanically remove plaque and stain from tooth surfaces; such methods give rise to loss of superficial structure and roughen the surface of composites as a result of their abrasive action. This study was done to assess the effect of three polishing systems on surface texture of new anterior composites after storage in artificial saliva. Materials and methods: A total of 40 Giomer and Tetric®N-Ceram composite discs of 12 mm internal diameter and 3mm height were prepared using a specially designed cylindrical mold and were stored in artificial saliva for one month and then samples were divided into four groups according to surface treatment: Group A (control group):10 specimens received no surfa
... Show MoreUrea formaldehyde resin was prepared by using basic media by yield 95%. The Remaining of ureaplasts resin were prepared in acetic acid media by high yield. Alkyde resins were prepared by condensation polymerization by react Succinic, Maleic, Phthalic anhydrides with Ethylene glycol or Glycerol. Select samples of the prepared alkyde resins were mixed with Azo dyes in special ratio. The mixtures were used as coatings for wood, and compaised with pure dyes. The Coating that some alkyde resins showed better adhesion from using dyes alone. Preparation of wood coating by mixing ureaplast resins and alkyde resins with Azo dyes in special ratios. The coating showed better adhesion, brighter colors and better resistance to heat from Preceding coat