Due to the advantages over other metallic materials, such as superior corrosion resistance, excellent biocompatibility, and favorable mechanical properties, titanium, its alloys and related composites, are frequently utilized in biomedical applications, particularly in orthopedics and dentistry. This work focuses on developing novel titanium-titanium diboride (TiB2; ceramic material) composites for dental implants where TiB2 additions were estimated to be 9 wt.%. In a steel mold, Ti-TiB2 composites were fabricated using a powder metallurgy technique and sintered for five hours at 1200 °C. Microstructural and chemical properties were analyzed by energy dispersive X-ray spectroscopy (EDX), scanning electron microscopy (SEM), and X-ray diffraction (XRD) to evaluate the impact of the TiB2 ceramic addition. Compressive strength, Brinell hardness, porosity, and density, among other mechanical and physical properties, were also measured and characterized. It has been found that adding TiB2 to Ti increases its porosity (35.53%), compressive strength (203.04 MPa), and surface hardness (296.3 kg/mm2) but decreases its density (3.79 gm/cm3). The lightweight and strong composite could be suitable for dental implant applications.
Background: Undergraduate dental students are more susceptible to situations of stress that affected quality of sleep, such profiles of stress may result in sleep bruxism and/or awake bruxism, parafunctions that can affect oral and general health. The aim of the study was to evaluate the association of sleep bruxism, awake bruxism and sleep quality among dental students. Materials and methods: A cross-sectional study was performed including 260 Iraqi dental students from university of Baghdad aged from 20to25years old. Students enrolled in the third and fifth class participated in the study. The Pittsburgh Sleep Questionnaire Index (PSQI) was used for data collection. The PSQI was distributed during lecture classes. Sleep bruxism and awake
... Show MoreThirty five samples were collected from patients (1-30) years old, suffered from, infected skin , rushes, boils , oral thrush, anal & vaginal itches. Candida albicans 57.3% (20 isolates) and Candida tropicalis 22.5% (8 isolates) Aspergillus fumegatus 11.5% (4 isolates) Aspergillus nigar 8.7%(3 isolates) , were isolated & identified from these samples. Alcoholic & water hot extracts of the punica granatum (Pomegranate) peels as well as the dried powder were prepared. The anti-fungal activity of the extracts was evaluated by means of the agar-well diffusion assay. The extract exhibited potent activity against yeast. The Minimum inhibitory concentra
... Show MoreIndustrial buildings usually are designed to sustain several types of load systems, such as dead, live, and dynamic loads (especially the harmonic load produced by rotary motors). In general, these buildings require high-strength structural elements to carry the applied loads. Moreover, Reactive Powder Concrete (RPC) has been used for this purpose because of its excellent mechanical strength and endurance. Therefore, this study provides an experimental analysis of the structural behaviors of reinforced RPC beams under harmonic loads. The experimental program consisted of testing six simply supported RPC beams with lengths of 1500 mm, widths of 150 mm, and thicknesses of 200 mm under harmonic loading with varied frequencies between 1
... Show MoreSoil stabilization with stone powder is a good solution for the construction of subgrade for road way and railway lines, especially under the platforms and mostly in transition zones between embankments and rigid structures, where the mechanical properties of supporting soils are very influential. Stone powder often has a unique composition which justifies the need for research to study the feasibility of using this stone powder type for ground improvement applications. This paper presents results from a comprehensive laboratory study carried out to investigate the feasibility of using stone powder for improvement of engineering properties of clays.
The stone powder contains bassanite (CaSO4. ½ H
... Show MoreLinear and mass attenuation coefficient of reactive powder concrete (RPC) sample ( of compressive strength equal to 70 Mpa) using beta particles and gamma ray with different energies have been calculated as a function of the absorber thickness and energy. The attenuation coefficient were obtained using NaI(Tl) energy selective scintillation counter with 90Sr/90Y beta source having an energy rang from (0.546-2.274) MeV and gamma ray energies (0.569, 0.662, 1.063, 1.17 and 1.33) MeV . The attenuation coefficient usually depends upon the energy of radiations and nature of the material. The result represented in graphical forms. Exponential decay was observed. It is found that the capability of reactive powder concrete to absorber beta particle
... Show MoreIn this work, Soda Lime Glass (S.L.G.) powder was used ,as
fluxe in traditional porcelain instead of feldspar. Two ceramics
porcelain were compared; commercial or traditional porcelain that
content of 50wt % kaolin, 25wt % quartz, and 25wt % feldspar.
Feldspar mass was substituted by scraps soda lime glass yielding a
new porcelain composition, to determine the softening points and
then the effect of glass addition on porcelain firing process.
Eight samples, for each patch, were prepared and 8wt % water
was added. The resulting composite blends were then die pressed at
2N, to produce disk specimens with diameter of 1.5 cm, and then
they were sintered at (1000, 1100, 1200, 1250,1300,1350,1400 and
1450) ˚C,
Industrial buildings usually are designed to sustain several types of load systems, such as dead, live, and dynamic loads (especially the harmonic load produced by rotary motors). In general, these buildings require high-strength structural elements to carry the applied loads. Moreover, Reactive Powder Concrete (RPC) has been used for this purpose because of its excellent mechanical strength and endurance. Therefore, this study provides an experimental analysis of the structural behaviors of reinforced RPC beams under harmonic loads. The experimental program consisted of testing six simply supported RPC beams with lengths of 1500 mm, widths of 150 mm, and thicknesses of 200 mm under harmonic loading with varied frequencies between 1