PMMA (Poly methyl methacrylate) is considered one of the most commonly used materials in denture base fabrication due to its ideal properties. Although, a major problem with this resin is the frequent fractures due to heavy chewing forces which lead to early crack and fracture in clinical use. The addition of nanoparticles as filler performed in this study to enhance its selected mechanical properties. The Nano-additive effect investigated in normal circumstances and under a different temperature during water exposure. First, tests applied on the prepared samples at room temperature and then after exposure to water bath at (20, 40, 60) C° respectively. SEM, PSD, EDX were utilized for samples evaluation in this study. Flexural strength, shear stress, hardness value were evaluated for all samples, the tests applied periodically at (15, 30, 45) min. Interestingly, it is found that at the normal condition (NC) the cooperation of TiO2 NPs significantly improves the selected properties. The maximum increase is located at 4 wt % of TiO2 NPs addition. The results also showed that temperature increase accelerate the water permeability within all samples thus decrease the mechanical properties. Obviously, a better hardness value determined for the prepared nanocomposite comparing to the control group at the same test condition.
A reinforced concrete frame is referred as "RIGID FRAMES". However, researches indicate that the Beam-Column joint (BCJ) is definitely not rigid. In addition, extensive research shows that failure may occur at the joint instead of in the beam or the column. Joint failure is known to be a catastrophic type which is difficult to repair.
This study was carried out to investigate the effect of hoops and column axial load on the shear strength of high-strength fiber reinforced Beam-Column Joints by using a numerical model based on finite element method using computer program ANSYS (Version 11.0). The variables are: diameter of hoops and magnitude of column axial load.
The theoretical results obtained from ANSYS program are in a good a
Background: Reduction in bond strength when bonding was done immediately after intracoronal bleaching procedure has been recognized. The purpose of this study is to assess the effect of antioxidants (10% sodium ascorbate (SA), 0.1M thiourea and7% sodium bicarbonate (SB)) on reversing bonding strength of composite resin to bleached dentin. Materials and method: Sixty upper 1st premolar teeth, were selected, the crowns of the teeth were embedded in acrylic resin blocks exposing a flat dentin from the buccal surface, then divided into 6 groups (10 samples each). Bleaching for the experimental groups was performed using 35% hydrogen peroxide bleaching gel (pola–office).Group A (Negative
... Show MoreBackground and objectives: This study aimed at testing the effect of plastic sleeve or barrier, used to cover the guide of the light cure unit to prevent cross-infection, on the shear bond strength and site of bond failure of stainless steel and ceramic orthodontic brackets. Materials and methods: Forty orthodontic brackets; twenty stainless steel and twenty ceramic brackets bonded to forty extracted human maxillary first premolars using light cure adhesive cured with and without the use of a protective plastic barrier on the guide. Comparing the effect of this barrier on the shear bond strength and adhesive remnant index was performed using an independent t-test and Chi-square test. Results: The protective barrier had decreased the shear b
... Show MoreBackground: Fracture of different types of acrylic denture base is a common problem associated with dental prosthesis. Studies suggested that the repair strength may be improved by several means including surface treatment with chemical agents. The aim of the study was to evaluate the effect of surface treatment with acrybond-bonding agent and monomer on fractured denture base in respect to transverse, tensile and shear bond strength and evaluation of the mode of failure by light microscope. Materials and methods: Two hundred seventy specimens were prepared and divided into 3 groups according to the material used (regular conventional, rapid simplified and high impact) heat cure acrylic. The specimen in each groups were prepared specificall
... Show MoreBackground: The combination of thermoplastic nylon resin materials and auto polymerizing resin is necessary in some situation for repair and adjustment. This study evaluated shear bond strength between thermoplastic nylon material (flexible) and auto polymerizing acrylic resin subjected to holes and silica coated layer. Materials and Method: Forty five (45) specimens were prepared from flexible acrylic bonded to auto-polymerizing acrylic resin and divided into three groups according to the surface treatments as follows: Group A: 15 specimens of flexible acrylic bonded with cold-cure acrylic by holes. Group B: 15 specimens of flexible acrylic bonded with cold-cure acrylic by silica coated layer. Group C: 15 specimens of flexible acrylic bon
... Show MoreAbstract
The current research aims to know the reality of the research's coefficients, to know correlation and effectiveness between the organizational Agility and high performance . The current research has been applied on the official banks , including a sample of senior administration members (120) ; besides , the research has used questionnaire that being considered as the main tool for gathering information and data . It includes 59 questions in addition to the personal interviews program as to support the questionnaire and to fulfill a great deal of reality. It has been anal
... Show MoreThe aim of this work is to evaluate some mechanical and physical
properties (i.e. the impact strength, hardness, flexural strength,
thermal conductivity and diffusion coefficient) of
(epoxy/polyurethane) blend reinforced with nano silica powder (2%
wt.). Hand lay-up technique was used to manufacture the composite
and a magnetic stirrer for blending the components. Results showed
that water had affected the bending flexural strength and hardness,
while impact strength increased and thermal conductivity decreased.
In addition to the above mentioned tests, the diffusion coefficient
was calculated using Fick’s 2nd law.
The aim of the study was to investigate the effect of magnetized water on the histological structure of heart, lung and spleen. For this purpose, twenty five albino rats were divided into five equal groups, the first group was considered as control group. The other groups were given magnetized water with intensity of 250, 750, 1000, 1500 gause every day for 30 days. Then the animals were sacrificed and the histological change on heart, lung and spleen was studied. Histopathology of heart in rats treated with magnetic water with intensity of 250, 750, 1000, 1500 gause showed no clear pathological lesion. Lung section of rats treated with 250 gause of magnetic water showed no pathological lesion, while lung section belongs to rats group given
... Show More