This work characterizes the fractographic features of the neat epoxy and ZrO2 epoxy nanocomposites. All samples were subjected to a tensile test to determine the tensile strength and tensile modulus. SEM images were used to study the morphology of the fractured surface. The fractographic of the fracture surfaces were studied by microstructure analysis program (j-images) to specify the effect of ZrO2 nanoparticles on tensile performance and failure mechanism for ZrO2 epoxy nanocomposites. The tensile test results show that the addition of ZrO2 nanoparticles (2, 4, 6, 8, and 10 vol.%) to the epoxy matrix leads to increase the tensile strength about 40% for optimal content of ZrO2 nanoparticles at 4 vol.%, tensile modules of ZrO2 epoxy nanocomposites increased about 200% for optimal content of ZrO2 nanoparticles at 4 vol.%. SEM images show that the patterns of fractured surfaces of ZrO2 epoxy nanocomposites are different from the pattern of the neat epoxy. The fracture roughness of ZrO2 epoxy nanocomposites increased with the increases of the percentages of ZrO2 nanoparticles, where the increment of fracture roughness about 30% for optimal content of ZrO2 nanoparticles at 4 vol.% can be indicator for the improvement of mechanical properties (tensile strength and modules).
Four antimony compounds were used in this inves as additives to retard combustion of unsaturated polyester and epoxy resins, namely: 1. Tetraethyl ammonium tribromoethylantimonates (additive I). 2. Tetraethyl ammonium chlorodibromoethylantimonates (additive II). 3. Tetraethyl ammonium trichloroethylantimonates (additive III). 4. Tetraethyl ammonium bromodichloroethylantimonates (additive IV). The effects of these additives on flammability of unsaturated polyester and epoxy resins have been studied by using sheets of the resins with weight percentages of (0.5,1.0,1.5,2.0,2.5&3.0%) of the additives in dimensions of (150 X150X3)mm .Three standard test methods were used to measure the flame retardation which are: (ASTM:D -2863), (ASTM:D-635
... Show MoreBackground: Nowadays there is an increasing of the emphasis on aesthetic, dentist have been concerned about providing aesthetics and functional removable partial dentures to their patients and this was make the mission more difficult because of the goal now is achieving optimal aesthetic of the denture - while maintaining retentive, stable, and conservative to the health of supporting tooth and supporting tissue. The traditional use of metal clasp like cobalt-chromium, gold, stainless-steel and titanium hampers esthetics because of its obvious display conflicts with patient’s prosthetic confidentiality. Acetal resin (poly oxy methylene) may be used as alternative denture clasp material. This material was promoted primarily on the basis of
... Show MoreBackground: The longevity of any prosthesis depends on the materials from which it was fabricated, that is why, defects in the material properties may reduce the service life of prosthesis and necessitate its replacement. The aim of this study was to evaluate the effect of adding different concentrations of Polyamide-6 (Nylon-6) on the tear and tensile strength of A-2186 RTV silicone elastomer. Materials and Methods: 80 samples were fabricated by the addition of 0%, 1%, 3% and 5% by weight PA-6 micro-particles powder to A-2186 platinum RTV silicone elastomer. The study samples were divided into four (4) groups, each group containing 20 samples. One control group was prepared without PA-6 micro particles and three experimental groups were pr
... Show MoreFiber reinforced polymer composite is an important material for structural application. The diversified application of FRP composite has taken center of attraction for interdisciplinary research. However, improvements on mechanical properties of this class of materials are still under research for different applications. In this paper we have modified the epoxy matrix by Al2O3, SiO2 and TiO2 nano particles in glass fiber/epoxy composite to improve the mechanical and physical properties. The composites are fabricated by hand lay-up method. It is observed that mechanical properties like flexural strength, hardness are more in case of SiO2 modified epoxy composite compare to other nano
... Show MoreThe physical, the thermal and the mechanical properties of Nano-composites, that consisted of Polyprime EP epoxy that reinforced by multi-walled carbon nanotubes (MWCNTs), have been studied. Various loading ratios, 0.1, 0.5, and 1 wt. %of MWCNT shave been infused into epoxy by a magnetic stirrer and then the hardener mixed with the mthat supplied with the epoxy. All sample shave been cutting using CNC machine. Tensile test, three-point bending, hardness tests, lee's disk, differential scanning calorimetry, water absorption and dielectric and electrical conductivity test were utilized on unfilled, MWCNT-filled epoxy to identify the loading effect on the properties of materials. Scanning electron microscopy (SEM) was used to determine the
... Show MoreAbstract\
The value chain analysis is main tools to achieve effective and efficient cost management; it requires a depth and comprehensive understanding for all internal and external activities associated with creating value. Supply chain as apart of value chain, that means managing it in active and efficient can achieve great results when adopting a comprehensive and integrated performance for these two chains activities. The research aims to identify possible ways to integrate the performance of value and supply chains of the sample" Kufa-cement plant" and determine the effect of this integration in enhancing customer value. The research arrival that logical and integrated analysis of value and supply chains helps
... Show MoreIn this work, chemical oxidation was used to polymerize conjugated polymer "Polypyrrole" at room temperature Graphene nanoparticles were added by in situ-polymerization to get (PPY-GN) nano. Optical and Electrical properties were studied for the nanocomposites. optical properties of the nanocomposites were studied by UV-Vis spectroscopy at wavelength range (200 -800 nm). The result showed optical absorption spectra were normally determined and the result showed that the maximum absorbance wave length at 280nm and 590nm. The optical energy gap has been evaluated by direct transition and the value has decreased from (2.1 eV for pure PPy) to (1.3 eV for 5 %wt. of GN). The optical constants such as the band tail width ΔE was evaluated, the
... Show More