Glassy polymers like Poly Mathyel Metha Acrylate are usually classified as non-porous materials; they are almost considered as fully transparent. Thin samples of these materials reflect color changing followed by porous formation and consequently cracking when exposed to certain level of ?-irradiation. The more the dose is the higher the effect have been observed. The optical microscope and UV-VIS spectroscopy have clearly approved these consequences especially for doped polymers.
Addressed the problem of the research is marked (technical openness in the formation of post-modernism - Pop Art an Example) the nature of the technical expansion of the output artifacts postmodern, and the nature of the raw materials taken as components of its sensual. The search came in four sections: general framework for research and identified the research problem and the need for him. With an indication of the importance of his presence. From then select the search goal (revealed openness to hire technical material in the art of Pop Art), followed by the establishment of the three search limits (objectivity, the temporal and spatial) were then determine the terms related to the title. Then provide the theoretical framework and indi
... Show MoreMRSA is one of the major pathogens in hospitals and the community, which have the ability to produce biofilm as a virulence factor, the impact of chalcone on biofilm formation, the synergism effect of chalcone and antibiotic in both in vitro and in vivo experiments, the gene expression of virulence genes (srtA, fnbA, fnbB) before and after treatment of it on MRSA biofilm cells in vitro, all these were the prime aims of this study. Chalcone at MBIC (20 μg/ml), significantly reduced the biofilm formation to 21.45% and at sub MBIC (15 μg/ml) to 36.58 %. While, Chalcone at MIC(5 μg/ml) reduced MRSA planktonic cells to 49.61%. Susceptibility of MRSA isolates against eight antibiotics showed that all isolates were sensitive to vancomycin and n
... Show MoreIn this work, the effect of anodizing duration on the morphology and photoelectrochemical properties of TiO2 nanotubes arrays (NTAs) has been investigated The samples were characterized by X-ray diffraction (XRD) and energy dispersive X-ray (EDX) to characterize their crystalline structure and compositional. Surface morphological and their dimensional variation was examined by field emission scanning electron microscopy (FESEM). The anodizing duration played a significant role in the formation of TiO2 nanotubes arrays. Moreover, the photoelectrochemical properties (PEC) were studied through photocurrent measurements. Optimum anodizing duration of 60 min at 40 V exhibited maximum photocurrent of 0.03 mA cm-2 under illumination of hal
... Show MoreIn this study lattice parameters, band structure, and optical characteristics of pure and V-doped ZnO are examined by employing (USP) and (GGA) with the assistance of First-principles calculation (FPC) derived from (DFT). The measurements are performed in the supercell geometry that were optimized. GGA+U, the geometrical structures of all models, are utilized to compute the amount of energy after optimizing all parameters in the models. The volume of the doped system grows as the content of the dopant V is increased. Pure and V-doped ZnO are investigated for band structure and energy bandgaps using the Monkhorst–Pack scheme's k-point sampling techniques in the Brillouin zone (G-A-H-K-G-M-L-H). In the presence of high V content, the ban
... Show MorePure and doped TiO 2 with Bi films are obtained by pulse laser deposition technique at RT under vacume 10-3 mbar, and the influence of Bi content on the photocvoltaic properties of TiO 2 hetrojunctions is studied. All the films display photovoltaic in the near visible region. A broad double peaks are observed around λ= 300nm for pure TiO 2 at RT in the spectral response of the photocurrent, which corresponds approximately to the absorption edge and this peak shift to higher wavelength (600 nm) when Bi content increase by 7% then decrease by 9%. The result is confirmed with the decreasing of the energy gap in optical properties. Also, the increasing is due to an increase in the amount of Bi content, and shifted to 400nm when annealed at 523
... Show More