Catalase (EC 1.11.1.6) is a well known enzyme which exists in almost all living creatures exposing to oxygen (such as plants, bacteria, and animals). It is a very necessary enzyme to protect the cell from oxidative detriment by reactive oxygen species (ROS). The aim of this study is the partial purification and characterization of Catalase enzyme from Banana peels. In this study, fresh banana peels are treated with 70 % ethanol ,further separated with chloroform ,water and ethyl acetate respectively .The supernatant of the enzymatic sample which is treated with chloroform is loaded into gel filtration column with Sephadex G-100 (1.0 x 90 cm) equilibrated with pH7 buffer media (phosphate buffer 0.1 M). Kinetic studies of the purified enzyme activity are measured and characterized .The maximal activity (26.04 units/mg) of catalase is observed with chloroform buffer extraction. The kinetics of catalase; Michalis constant Km and maximum velocity Vmax is determined using Linweaver- Burk plot, The Km value for catalase (434.7mM), Vmax (100 m mole min -1). Characterization results demonstrate that the optimal pH for activity is (7.6). And the optimal temperature for activity is 30?C .The present study indicates that Banana peels is a good source of catalase enzyme.
Polyaniline nanofibers (PAni-NFs) have been synthesized under various concentrations (0.12, 0.16, and 0.2 g/l) of aniline and different times (2h and 3 h) by hydrothermal method at 90°C. Was conducted with the use of X-ray diffraction (XRD), Fourier Transform Infrared spectra (FTIR), Ultraviolet-Visible (UV-VIS) absorption spectra, Thermogravimetric Analysis (TGA), and Field Emission-Scanning Electron Microscopy (FE-SEM). The X-ray diffraction patterns revealed the amorphous nature of all the produced samples. FE-SEM demonstrated that Polyaniline has a nanofiber-like structure. The observed typical peaks of PAni were (1580, 1300-1240, and 821 cm-1 ), analyzed by the chemical bonding of the formed PAni through FTIR spectroscopy. Also, tests
... Show MoreThis paper focused on the stone matrix asphalt (SMA) technology that was developed essentially to guard against rutting distress. For this procedure, fibers play a racy role in stabilizing and preventing the drain down problem caused by the necessity of high binder content coupled with their strengthening effect. A set of specimens with cylindrical and slab shapes were fabricated by inclusions jute, polyester, and carbon fibers. For each type, three contents of 0.25%, 0.5%, and 0.75% by weight of mixture were added by lengths of 5, 7.5, and 10 mm. The prepared mixtures were tested to gain the essential pertained parameters discriminated by the values of drain down, Marshall quotient, rut depth, and dynamic stability. It
... Show MoreThe Early – Middle Miocene Ghar and Lower Fars sedimentary succession at the representative oil-well Nu-18 of the Nahr Umr oil field south Iraq; is taken by this study to investigate the sedimentological to reservoir rock facies buildups and related reservoir zonation; as first rock-typing attempt for the both formations. The sedimentological characterization of the Early Miocene Ghar formation is mainly comprised by successive buildups of sands-gravels and sandstones, whereas; the Middle Miocene Lower Fars formation is started by limestone, limestone-marly/marl anhydritic, upgraded into interbedded-series of marl and anhydrite facies, with less-common occurrences of thin-sandstone interlayers, terminated by marl-sandy-secti
... Show MorePolyaniline (PANI) and Ag/PANI nanocomposite thin films have prepared by microwave induced plasma. The Ag powder of average particle size of 50 nm, were used to prepare Ag/PANI nanocomposite thin films. The Ag/PANI nanocomposite thin films prepared by polymerization in plasma and characterized by UV-VIS, FTIR, AFM and SEM to study the effect of silver nanoparticles on the optical properties, morphology and structure of the thin films. The optical properties studies showed that the energy band gap of the Ag/PANI (5%wt silver) decreased from 3.6 to 3.2 eV, where the substrate location varied from 4.4 to 3.4 cm from the axis of the cylindrical plasma chamber. Also the optical energy gap decreased systematically from 3.3 to 3 eV with increas
... Show MoreSpin coating technique used to prepare ZnPc, CdS and ZnPc/CdS blend thin films, these films annealed at 423K for 1h, 2h and 3h. Optical behavior of these films were examined using UV-Vis. and PL. The absorption spectrum of ZnPc shows a decreasing in absorption with the increase of annealing time while CdS spectrum give a clearly absorption peak at~510 nm. Energy gap of ZnPc increases from 1.41 to 1.52 eV by increasing the annealing time. Eg of CdS decrease by increasing annealing time, from 2.3 eV to 2.2 eV. The intensities of the peaks obtained from PL spectra were strongly dependent on annealing time and confirmed the results obtained from UV-Vis. D.C. conductivity measurement showed that all the thin films have two differen
... Show MoreIn this study, Zinc oxide nanostructures were synthesized via a hydrothermal method by using zinc nitrate hexahydrate and sodium hydroxide as a precursor. Three different annealing temperatures were used to study their effect on ZnO NSs properties. The synthesized nanostructure was characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Atomic force microscope (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Their optical properties were studied by using UV -visible spectroscopy. The XRD analysis confirms that all ZnO nanostructures have the hexagonal wurtzite structure with average crystallite size within the range of (30.59 - 34
... Show MoreKHalaf Alhmar and what we get from his poem