Different polymers were prepared by condensation polymerization of sebacic anhydride and adipic anhydride with ethylene glycol and poly(ethylene glycol). Their number average molecular weights were determined by end group analysis. Then, they were grafted on the prepared phthalocyaninatocopper(II) compounds with the general formula (NH2)4PcCu(II) having amino groups of 3,3',3'',3'''- or 4,4',4'',4'''- positions. All prepared polymers, compounds, and phthalocyaninatocopper(II)-grafted polymers were characterized by FTIR. The sizing measurements were carried out in 3,3',3'',3'''- (NH2)4PcCu(II) and 4,4',4'',4'''- (NH2)4PcCu(II) compounds with and without grafting polymers. The results showed that the grafting process led to decreasing in particle size and increasing in surface area. The grafting process was reflected positively on the thermal degradation of 3,3',3'',3'''- (NH2)4PcCu(II) and 4,4',4'',4'''- (NH2)4PcCu(II) grafted polymers. They had higher thermal stability accompanied with higher char residue and T50% weight loss with 3,3',3'',3'''-(NH2)4PcCu(II) and their grafted polymers being the best.
PVC/Kaolinite composites were prepared by the melt intercalation method. Mechanical properties, thermal properties, flammability and water absorption percentage of prepared samples were tested. Mechanical characteristic such as tensile strength, elongation at break; hardness and impact strength (charpy type) were measured for all samples. It was found that the tensile strength and elongation at break of PVC composites decreased with increasing kaolinite loading. Also, the hardness of the composites increases with increase in filler content .The impact strength of the composites at the beginning increases at lower kaolinite loadings is due to the lack of kaolin adhesion to the matrix. However, at higher kaolin loadings. This severe agglom
... Show MorePurpose: This study aimed to compare the stability and marginal bone loss of implants inserted with flapped and flapless approaches 8 weeks after surgery and 3 months after loading. Material and Methods: Thirty SLActive implants were inserted in 11 patients and early loaded with final restoration 8 weeks after healing period. The stability values determined by Osstell and the marginal bone loss measured by CBCT at the initial time (1st) and 8 weeks of the healing period (2nd) and 3 months after loading (3rd). Results: The overall survival rate was 100%. A significant increase in the 3rd implant stability value in the age of ˂ 40. A significant decrease in the 2nd implant stability value in both gender and traumatic zone with a flapless app
... Show MoreFaujasite type NaY zeolite catalyst was prepared from locally available kaolin, then the prepared NaY zeolite have been modified by exchanging of sodium ion with ammonium to produce NH4Y zeolite. NH4Y zeolite was converted to HY zeolite by ion exchanging with oxalic acid. Zinc and nickel promoters have been added to the prepared HY zeolite catalyst, and the effect of these promoters on the catalytic activity of the prepared HY catalyst was studied in fluid catalytic cracking process using light gas oil as a feedstock. The experimental results show that the promoted catalyst gives higher gas oil conversion and gasoline yield than HY zeolite catalyst at the same reaction temperature and WHSV. It was also found that the promoted catalyst gi
... Show MoreThin films of Mn2O3 doped with Cu have been fabricated using the simplest and cheapest chemical spray pyrolysis technique onto a glass substrate heated up to 250 oC. Transmittance and absorptance spectra were studied in the wavelength range (300 -1100) nm. The average transmittance at low energy was about 60% and decrease with Cu doping, Optical constants like refractive index, extinction coefficient and dielectric constants (εr), (εi) are calculated and correlated with doping process.
Steel fiber aluminum matrix composites were prepared by atomization technique. Different air atomization conditions were considered; which were atomization pressure and distance between sample and nozzle. Tensile stress properties were studied. XRF and XRD techniques were used to study the primary compositions and the structure of the raw materials and the atomized products. The tensile results showed that the best reported tensile strength observed for an atomization pressure equal to 4 mbar and sample to nozzle distance equal to 12 cm. Young modulus results showed that the best result occurred with an air atomization pressure equal to 8 mbar and sample to nozzle distance equal to 16cm
Sol-gel method was use to prepare Ag-SiO2 nanoparticles. Crystal structure of the nanocomposite was investigated by means of X-ray diffraction patterns while the color intensity was evaluated by spectrophotometry. The morphology analysis using atomic force microscopy showed that the average grain sizes were in range (68.96-75.81 nm) for all samples. The characterization of Ag-SiO2 nanoparticles were investigated by using Scanning Electron Microscopy (SEM). Ag-SiO2 NPs are highly stable and have significant effect on both Gram positive and negative bacteria. Antibacterial properties of the nanocomposite were tested with the use of Staphylococcus aureus (S. aureus) and Escherichia coli (E. coli) bacteria. The results have shown antibacteri
... Show MoreThe placenta is an organ between the mother and fetus necessary for fetal growth and development. Gestational diabetes mellitus (DM) is the most frequent metabolic condition detected during pregnancy. It is characterized as hyperglycemia of various severity with onset or first detection during pregnancy that does not clearly describe any form of preexisting diabetes. Urotensin II (UII), a pluripotent vasoactive peptide, is important in developing insulin resistance. This study aimed to determine the level of Urotensin II(UII) in placenta and in the serum of diabetic and nondiabetic women. Methods The blood and placenta tissue collected from 50 ladies had been enrolled in this research ( 25 females with uncomplicated), (25 women with gestati
... Show MorePure and Fe-doped zinc oxide nanocrystalline films were prepared
via a sol–gel method using -
C for 2 h.
The thin films were prepared and characterized by X-ray diffraction
(XRD), atomic force microscopy (AFM), field emission scanning
electron microscopy (FE-SEM) and UV- visible spectroscopy. The
XRD results showed that ZnO has hexagonal wurtzite structure and
the Fe ions were well incorporated into the ZnO structure. As the Fe
level increased from 2 wt% to 8 wt%, the crystallite size reduced in
comparison with the pure ZnO. The transmittance spectra were then
recorded at wavelengths ranging from 300 nm to 1000 nm. The
optical band gap energy of spin-coated films also decreased as Fe
doping concentra