Bentonite is widely used in industrial applications. The present study reports the effect of adding different weights of ZnO to the Iraqi bentonite, on surface area, pore volume and real density. These surface properties were evaluated for pure and modified bentonite. The modification was made by adding different ZnO weights such as; ( 0.5%, 1%, 5%, 10% ). The effect of heat exposing for all modified clay samples at 500 ?C have been also evaluated. The results show that the addition of 0.5% ZnO leads to increase the surface area percentage about 36%, increase pore volume percentage about 5.48% and increase the real density percentage about 27.116%. When the samples exposed to 500 ?C, their surface area and pore volumes have been decreased and the real density increased in compared with non-heat exposed samples.
Background: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreDental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60 test block w
... Show MoreBackground: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreThree plants extracts of Eucalyptus, Pomegranate and Oolong tea leaves have been used to synthesize iron oxide nanoparticles. The structure and particle size of the nanoparticles have been investigated by XRD spectrum. The results exhibit the polycrystalline nature of the material with a size around (17-19 nm). FESEM analysis showed that using different extracts as a reduction and capping agent might affect the shape of nanoparticles such as forming of round, polygon and irregular shapes under the same conditions. The photo catalyst activity of the prepared NPs in the degradation of MB dye has been investigated. the results showed a good efficiency reached to 91%, 88% and 80%.
MWCNTs and hybrid nanocomposite ZnO/Se/MWCNTs have been prepared via Solvothermal technique using Parr reactor at the temperature 180°C and SeCl2 as a catalyst. The obtained MWCNTs and ZnO/Se/MWCNTs are investigated using the FE-SEM, XRD, UV-VIS Spectroscopy and Z-Scan. The novelty of this research is studying the nonlinear optical properties for these prepared materials and the results exhibit that the thickness of the deposited film for hybrid nanocomposite ZnO/Se/MWCNTs is increased, which in turn, increase the nonlinear phase shift of the laser beam compared with the MWCNTs.
The semiconductor ZnO is one of II – VI compound group, it is prepare as thin films by using chemical spray pyrolysis technique; the films are deposited onto glass substrate at 450 °C by using aqueous zinc chloride as a spray solution of molar concentration 0.1 M/L. Sample of the prepared film is irradiating by Gamma ray using CS 137, other sample is annealed at 550°C. The structure of the irradiated and annealed films are analyzed with X-ray diffraction, the results show that the films are polycrystalline in nature with preferred (002) orientation. The general morphology of ZnO films are imaged by using the Atomic Force Microscope (AFM), it constructed from nanostructure with dimensions in order of 77 nm.
The optical properties o
In this study, the results of the uranium concentrations and specific activity in 10 rice samples are described using a solid-state track detector (CR-39). Samples were collected from various local Iraqi markets with different origins (Iraq, India, America, and Thailand). Our findings found that the results of uranium concentration in all studied samples are ranging from (0.55 ± 0.28 to 1.74 ± 0.31) ppm with a weighted average of (1.24 ± 0.99) ppm. Also, results demonstrate that the specific activity values of the studied samples swing between values of (6.88 ± 3.52 and 21.49 ± 3.85) Bq/Kg. The obtained results of the studied rice samples are indicated that it is less than the acceptable limit of those studies established by ma
... Show MoreIn this paper Zener diode was manufactured using ZnO-CuO-ZnO/Si heterojunction structure that used laser induced plasma technique to prepare the nanofilms. Six samples were prepared with a different number of laser pulses, started with 200 to 600 pulses on ZnO tablet with fixed the number of laser pulses on CuO tablet at 300 pulses. The pulse energy of laser deposited was 900mJ using ZnO tablet and 600mJ using CuO tablet. All prepared films shown good behavior as Zener diode when using porous silicon as substrate.