In this publication, several six coordinate Co(III)-complexes are reported. The reaction of 2,3-butanedione monoxime with ethylenediamine or o-phenylenediamine in mole ratios of 2:1 gave the tetradentate imine-oxime ligands diaminoethane-N,N`-bis(2-butylidine-3-onedioxime) H2L1 and o-phenylenediamine-N,N`-bis(2-butylidine-3-onedioxime), respectively. The reaction of H2L1 and H2L2 with Co(NO3)2, and the amino acid co-ligands (glycine or serine) resulted in the formation of the required complexes. Upon complex formation, the ligands behave as a neutral tetradantate species, while the amino acid co-ligand acts as a monobasic species. The mode of bonding and overall geometry of the complexes were determined through physico-chemical and spectroscopic methods. These studies revealed octahedral geometry about Co(III) complexes in which the co-ligands bound through the amine and the carboxylate groups. Molecular structure for the complexes have been optimised by CS Chem 3D Ultra Molecular Modelling and Analysis Program and supported six coordinate geometry.
The corrosion inhibition effect of a new furan derivative (furan-2-ylmethyl sulfanyl acetic acid furan-2-ylmethylenehydrazide) on mild steel in 1.0 M HCl was investigated using corrosion potential (ECORR) and potentiodynamic polarization. The obtained results indicated that the new furan derivative (furan-2-ylmethyl sulfanyl acetic acid furan-2-ylmethylenehydrazide) (FSFD) has a promising inhibitive effects on the corrosion of mild steel in 1.0 M HCl across all of the conditions examined. The density functional theory (DFT) study was performed on the new furan derivative (FSFD) at the B3LYP/6-311G (d, p) basis set level to explore the relation between their inhibition efficiency and molecular electro
In this study a polymeric composite material was prepared by hand
lay-up technique from epoxy resin as a matrix and magnesium oxide
(MgO) as a reinforcement with different weight fraction (5,10,15,
and 20)% to resin. Then the prepared samples were immersed under
normal condition in H2So4(1 M) solution, for periods ranging up to
10 weeks. The result revealed that the diffusion coefficient
decreasing as the concentration of MgO increase. Also we studied
Hardness for the prepared samples before and after immersion. The
result revealed that the hardness values increase as the concentration
of MgO increase, while the hardness for the samples after immersion
in H2SO4 dec
A new light-weight nanocarbon prepared by spray-drying method to obtain particle size is 21.7 nm based of polylactic acid biodegradable film in antistatic packaging .Bio carbon (biochar) is obtained from plants and soils to naturally absorb and store carbon dioxide from the atmosphere . Therefor it has been used to support biodegradable polylactic acid (PLA) with to obtain 100% recyclable material.
Using plasticizer thymol of polylactic acid and biochar (bio carbon) as composites were prepared by a solution casting method with (0.5-10)wt% biochar. The composites characterized by FTIR, electrical conductivity, mechanical properties , contact angle and Colar and Brightness . Results show th
... Show MoreHR Al-Hamamy, AA Noaimi, IA Al-Turfy, AI Rajab, Journal of Cosmetics, Dermatological Sciences and Applications, 2015
The present work involved synthesis of several new N-Sulfamethoxazol derivatives imide on Polymeric chain by two steps. The first stip involved preparation of N- (sub.orunsub benzoyl and sub unsub acetyl) amidyl sub sulfamethoxazole (1-5) by condensation of sulfamethoxazole drug with many substituted acid chloride, then the second step include, preparation new five N-(acrly-N–sub or unsub benzoyl) imidyl substituted sulfamethoxazol(6-10) by reaction of poly acryloyl chloride with the prepared compound (1-5) in first stepin asuitable solvent in the presenceamount triethylamine (Et3N) with heating. The structure confirmations of all polymers wereconfirmed using FT-IR,1H-NMR,13C-NMR and UV spectroscopy. Other physical properties including so
... Show MoreThe sol-gel route using an agar gel with calcium nitrate and phosphate solution as starting materials for producing hydroxyapatite (HAP). The product formed were needle like, zigzag and straight fibres. The fibrous products on sintering transformed into stoichiometric HAP with a biological Ca/P ratio of 1.67. The influences of pH, temperature, nature of base and phosphate solution on the growth of fibrous HAP were studied. The pH of the solution was found to greatly influence the growth rate and morphology of the resultant product. The optimum gel temperature was found to be 60oC and sintering temperature of 900oC for 1 hour. The crystalline, thermal, functional and morphological characteristics of the fibrous HAP were investigated.
Phenol condensed with β-keto esters via Pechmann condensation to form derivatives of Coumarin in various reaction conditions by two ways. Present paper is comparative study of synthesis Coumarin with the yield of product , reaction time and reaction conditions.