The adhesion strength between Polyethylene (PE) film and Aluminum surface by using the adhesive material (Cyanoacrylate) has been studied. Aluminum (Al) was used as a substrate, and polyethylene (PE) was used as a film adhered to the Al surface. Standard specimens were prepared to use in the peeling test in dry condition, other specimens were immersed in water for 12 days at room temperature. the results for the specimens in the dry condition had shown that high value in the peel force and the peel energy, the peel force was 0.38*103 N/m and the peel energy was 0.605*103 N/m, peeling the film from Al surface leaves a residual of the adhesive material on both adherend, the failure for this specimen were combination of adhesive and cohesive failure. For the specimens that were immersed in water for 12 days, the results had shown that the effect of water on the specimen (Al /PE), where the water diffusion coefficient on the adhesive joint was 1.09*10-14 m2/s and the peel force was 0.062*103 N/m and the peel energy was 0.124*103 N/m, PE film was peeled from Al surface without any resistance.

This paper presents the thermophysical properties of zinc oxide nanofluid that have been measured for experimental investigation. The main contribution of this study is to define the heat transfer characteristics of nanofluids. The measuring of these properties was carried out within a range of temperatures from 25 °C to 45 °C, volume fraction from 1 to 2 %, and the average nanoparticle diameter size is 25 nm, and the base fluid is water. The thermophysical properties, including viscosity and thermal conductivity, were measured by using Brookfield rotational Viscometer and Thermal Properties Analyzer, respectively. The result indicates that the thermophysical properties of zinc oxide nanofluid increasing with nanoparticle volume f
... Show MoreThis study aims to evaluate drinking water quality at the Al Wahda plant (WTP) in Baghdad city. A conventional water treatment plant with an average flow rate of 72.82 MLD. Water samples were taken from the influent and effluent of the treatment plant and analyzed for some physicochemical and biological parameters during the period from June to November 2020. The results of the evaluation indicate that treated water has almost the same characteristics as raw water; in other terms, the plant units do not remove pollutants as efficiently as intended. Based on this, the station appears to be nothing more than a series of water passage units. However, apart from Total dissolved solids, the mean values of all parameters in th
... Show MoreIn the current study, two sites were selected from the city of Adhamiya, central Baghdad. The first site is the Adhamiya Corniche, which includes a sample of river water and the second includes domestic sewage in the same area. The total density of benthic invertebrates was 775 ind/m2, which is divided into 15 taxa. Biological indices were found, such as the stability index, the abundance index, the biodiversity index (Shannon’s index), the homogeneity index, and the invader’s guide. The result showed an increase in the density of benthic invertebrates, as well as an increase in the diversity of these organisms.
In any natural area or water body, evapotranspiration is one of the main outcomes in the water balance equation. It is also a crucial component of the hydrologic cycle and considers as the main requirement in the planning and designing of any irrigation project. The climatic parameters for the Ishaqi area are calculated from the available date of Samarra and Al-Khlais meteorological stations according to a method for the period (1982–2017) according to Fetter method. The results of the mean of rainfall, relative humidity temperature, evaporation, sunshine, and wind speed of the Ishaqi area are 171.96 mm, 49.67%, 24.86 C°, 1733.61 mm, 8.34 h/day, and 2.3 m/sec, respectively. Values of Potential Evapotranspiration are determined by
... Show MoreThis search aim to measure Hardness for Epoxy resin and for unsaturated Polyester resin as base materials for composite Hybrid and the materials used is Hybrid fiber Carbon-Kevlar. The Hand Lay-up method was used to manufacture plates of Epoxy resin (EP) and unsaturated Polyester EP,UPE backed by Hybrid fiber (Carbon-Kevlar) and with small volume fraction 5,10 and 15 for every there are Layer of fibers (1,2 and 3). The hardness test was count for material EP, UPE resin and there composites and that we notice that the Hardness (HB) decreased with increase of temperatures.
High temperature superconductor with nominal composition Bi1.6Pb0.4Sr1.8Ba0.2Ca2 Cu3O10+? was prepared by solid state reaction method. Two sets of samples have been prepared .The first one was quenched in air; the second set was quenched in liquid nitrogen. X-ray diffraction analyses showed an orthorhombic structure with two phases, high –Tc phase (2223) and low-Tc phase (2212) in addition to that impure phase was found. It has been observed that quenched in air samples display a sharp superconducting transition and a higher-Tc phase than that of the quenched in liquid nitrogen samples.
Surfaces quality is one of the most specified customer requirements for machine parts. The major indication of surfaces quality on machined parts is surface roughness. The research aim is to study the cutting conditions and their effects on the surface roughness. This paper utilizes regression models to predict surface roughness over the machining time for variety of cutting conditions in turning. In the experimental part for turning, different types of materials (Aluminum alloy, Copper alloy, and Gray cast iron) were considered with different cutting speed ( ) and feed rate ( ). A mathematical Model depending on statistical-mathematical method between surface roughness (Rz ) and cutting condition ( , ) were derived, for the three materials
... Show Moreto evaluate the effect of various Nd:YAG frequency doubled laser parameters on the acid
dissolution and the progression of in vitro caries like lesions in human enamel.
Materials and Methods: Human extracted caries free upper first premolar teeth were collected for
this study. The irradiated teeth were divided into two groups. The first group was irradiated with
continuous Nd:YAG laser radiation, and the second group was irradiated with chopped Nd:YAG laser
radiation. For the first group, power and exposure time were changed while for the second group
power and number of pulses were changed. The spot diameter was kept constant for all the samples.
Results: using 1.5 W and 3 seconds (exposure time), best results among