Zinc oxide nanoparticles sample is prepared by the precipitation method. This method involves using zinc nitrate and urea in aqueous solution, then (AgNO3) Solution with different concentrations is added. The obtained precipitated compound is structurally characterized by X-ray diffraction (XRD), Scanning electron microscopy (SEM), Atomic force microscopy (AFM) and Fourier transform infrared spectroscopy (FTIR). The average particle size of nanoparticles is around 28nm in pure, the average particle size reaches 26nm with adding AgNO3 (0.05g in100ml =0.002 M) (0.1g in100ml=0.0058M), AgNO3 (0.2g in 100ml=0.01M) was 25nm. The FTIR result shows the existence of -CO, -CO2, -OH, and -NO2- groups in sample and oxides (ZnO, Ag2O).and used an atomic force microscope and microscope scanning electron to model the record.
Blood samples of One hundred and twenty patients from different hospitals in Baghdad infected with hydatidosis in different sites of the body (Liver, Lung, multiorgans and kidney) were collected for this study. On the other hand, 30 healthy individuals were included as a control group. This study was conducted to evaluate the effect of this disease on the serum protein profile of the patients using electrophoresis. The results revealed four different protein banding patterns with difference in number of bands and their molecular weights in comparison to the control group, and these differences depended on the site of infection. However the data showed a presence of the same band in all patients with different site of infection.
The spray quality of two spraying agents with different physical properties was investigated under laboratory conditions to find whether the measurement of deposited drops could be affected by spraying those agents. The first spraying agent Moddus, which is a plant growth regulator, has a surface tension of 28 mN m-1 with almost half the value of the second spraying agent Kelpak (58 mN m-1). A mini boom sprayer containing three flat fan nozzles (XR 11003) was used in the test with three traveling speeds (4.74, 5.42 and 8.13 km. h-1). The test was performed to evaluate the quality of spray drops (spray coverage, spray density and stains diameter) after they were deposited on water sensitive papers (WSP). The results showed a higher ability o
... Show MoreZinc Oxide thin film of 2 μm thickness has been grown on glass substrate by pulsed laser deposition technique at substrate temperature of 500 oC under the vacuum pressure of 8×10-2 mbar. The optical properties concerning the absorption, and transmission spectra were studied for the prepared thin film. From the transmission spectra, the optical gap and linear refractive index of the ZnO thin film was determined. The structure of the ZnO thin film was tested with X-Ray diffraction and it was formed to be a polycrystalline with many peaks.
The present project involves photodegrading the dye solochrom violet under advanced oxidation techniques at (25 oC) temperature and UV light. Zinc Oxide (ZnO) and UV radiation at a wavelength of 580 nm were used to conduct the photocatalytic reaction of the solochrom violet dye. One of the factors looked into was the impact of the starting conditions. pH, the amount of original hydrogen peroxide, and the dye concentration time radiation were used. For hours, the kinetics and percentages of degradation were examined at various intervals. In general, it has been discovered that the photodegradation rates of the dye were greater when H2O2 and ZnO were combined with UV light. The best wavelength to use was determined. Modern oxidation techni
... Show MoreIn this work, the photocatalytic degradation of indigo carmine (IC) using zinc oxide suspension was studied. The effect of influential parameters such as initial indigo carmine concentration and catalyst loading were studied with the effect of Vis irradiation in the presence of reused ZnO was also investigated. The increased in initial dye concentration decreased the photodegradation and the increased catalyst loading increased the degradation percentage and the reused-ZnO exhibits lower photocatalytic activity than the ZnO catalyst. It has been found that the photocatalytic degradation of indigo carmine obeyed the pseudo-first-order kinetic reaction in presence of zinc oxide. This was found from plotting the relationship between ln
... Show MoreAims of this research to determine asbestos fibers levels in surrounding air of some crowded sites of Baghdad city were monitored in summer 2020. Collection of samples was conducted by directing air flow to a mixed cellulose ester membrane filter mounted on an open‑faced filter holder using sniffer a low flow sampling pump, samples of air were collected from five studied areas selected in some heavy traffic areas of Baghdad city, (Al-Bayaa and Al-Shurta tunnel, Al-Jadriya, and Al-Meshin commercial complex, control), then analyzed to determine concentrations of asbestos fibers. Counting of asbestos on the filters was carried out through using both scanning electron microscope SEM and an energy dispersive X‑ray system EDS to count
... Show MoreThis work investigates generating of pure phase Faujasite-type zeolite Y at the ranges chosen for this study via a static aging step in the absence of seeds synthesis. Nano-sized crystals may result when LUDOX AS-40 is used as a silica source for gel composition of range 6 and the crystallization step may be conducted for a period of 4 to 19 hr at 100 ⁰C. Moreover, large-crystals with high crystallinity pure phase Y zeolite can be obtained at hereinabove conditions but when hydrous sodium metasilicate is used as a silica source. The other selected ranges also offer pure phase Y zeolite at the same controlled conditions.
This work investigates generating of pure phase Faujasite-type zeolite Y at the ranges chosen for this study via a static aging step in the absence of seeds synthesis. Nano-sized crystals may result when LUDOX AS-40 is used as a silica source for gel composition of range 6 and the crystallization step may be conducted for a period of 4 to 19 hr at 100 ⁰C. Moreover, large-crystals with high crystallinity pure phase Y zeolite can be obtained at hereinabove conditions but when hydrous sodium metasilicate is used as a silica source. The other selected ranges also offer pure phase Y zeolite at the same controlled conditions.
The dye–semiconductor interface between N749 sensitized and zinc semiconductor (ZnSe) has been investigated and studied according to quantum transition theory with focusing on the electron transfer processes from the N749 sensitized (donor) to the ZnSe semiconductor (acceptor). The electron transfer rate constant and the orientation energy were studied and evaluated depended on the polarity of solvents according to refractive index and dielectric constant coefficient of solvents and ZnSe semiconductor. Attention focusing on the influence of orientation energies on the behavior of electron transfer rate constant. Differentdata of rate constant was discussion with orientation energy and effective driving energy for N749-ZnSe system.
... Show More