The D.C electrical and thermoelectrically properties of randomly mixed isolator – electrolyte system as (Al/ PVC – LiF/Al) junction consisting of polyvinyl chloride (PVC)resin reinforced with Lithium Fluoride (LiF) powder were studied. A comparison is made the properties of (PVC) material with varying percentage of (LiF) powder (0%, 30%, 50%, 80%)to find out the effect of reinforcement of isolator material. The composites dissolving in 10ml form tettraHaedroflourn (THF) and Solution were the castled in Petri dish and Laved it dry in the air, The out coming Sample were disc - Like shape of a diameter of about 3cm and thickness reneged between (0.01- 0.018) cm . The composites dissolving in 10ml form tettraHaedroflourn (THF) and Solution were the castled in Petri dish and Laved it dry in the air, The out coming Sample were disc - Like shape of a diameter of about 3cm and thickness reneged between (0.01- 0.018) cm . The experimental results show that current and the conductivity of (PVC - LiF) composites increase by three orders of magnitude when the volume fraction (LiF Vol.%) increase and so dose with temperature. The activation energy of the thermal rate - process of the electrical conductivity is determined and found to decrease with increasing the LiF vol. % content. We find that this composite has good conductivity, light weight and easily manufactured. These very good ideal characteristics can make the composite very suitable to be used commercially
Thin films of Zinc Selenide ZnSe have been prepared by using thermal evaporation in vacuum technique (10-5Torr) with thickness (1000, 2700, 4000) A0 and change electrode material and deposited on glass substrates with temperature (373K) and study some electrical properties at this temperature . The graphs shows linear relation between current and voltage and the results have shown increases in the value of current and electrical conductivity with increase thickness and change electrode material from Aluminum to Copper
Nanocrystalline TiO 2 and CuO doped TiO 2 thin films were successfully deposited on suitably cleaned glass substrate at constant room temperature and different concentrations of CuO (0.05,0.1,0.15,0.2) wt% using pulse laser deposition(PLD) technique at a constant deposition parameter such as : (pulse Nd:YAG laser with λ=1064 nm, constant energy 800 mJ, with repetition rate 6 Hz and No. of pulse (500). The films were annealed at different annealing temperatures 423K and 523 K. The effect of annealing on the morphological and electrical properties was studied. Surface morphology of the thin films has been studied by using atomic force microscopes which showed that the films have good crystalline and homogeneous surface. The Root M
... Show MoreABSTRACT: Polypyrrole and polypyrrole / silver nanocomposites were fabricated by in-situ polymerization employing Ammonium Persulphate as an oxidizing agent. Nanocomposites were synthesized by combining polypyrrole and silver nanoparticles in various weight percentages (0.1%, 0.5%, 3%, 5% and 7% wt.). Crystallographic data were collected using X-ray diffraction. PPy particles were found to have an orthorhombic symmetry. In contrast, PPy/Ag nanocomposites were reported to have monoclinic structure. The crystallite size was determined by XRD using Scherrer equation and considered to be within 49 nm range. DC conductivity of pelletized samples was evaluated in the temperature range of 323.15k to 453.15k. The conductiv
... Show MoreAbstract
Binary polymer blend was prepared by mechanical mixing method of unsaturated polyester resin with Nitrile Butadiene Rubber (NBR) with different weight ratios (0, 5, 10 and 15) % of (NBR). Tensile characteristics and wear rates of these blends were studied for all mixing ratios. The microstructure of fracture surfaces of the prepared samples were investigated by optical microscope. The results were showed that strain rates of the resin material increase after blending it with rubber while the ultimate tensile strength and Young’s modulus values of it will decrease. It is also noticed that the wear rate of resin decreases with increasing of (NBR) content.
Keywords:<
... Show MoreIn this work, porous Silicon structures are formed with photochemical etching process of n-type Silicon(111) wafers of resistivity (0.02.cm) in hydrofluoric acid (HF) of concentration (39%wt) under light source of tungeston halogen lamp of (100 Watt) power. Samples were anodized in a solution of 39%HF and ethanol at 1:1 for 15 minutes. The samples were realized on n-type Si substrates Porous Silicon layers of 100m thickness and 30% of porousity. Frequency dependence of conductivity for Al/PSi/Si/Al sandwich form was studied. A frequency range of 102-106Hz was used allowing an accurate determination of the impedance components. Their electronic transport parameters were determined using complex impedance measurements. These measu
... Show MoreIn this work, ZnS thin films have been deposited by developed laser deposition technique on glass substrates at room temperature. After deposition process, the films were annealed at different temperatures (200ºC , 300 ºC and 400ºC ) using thermal furnace.The developed technique was used to obtain homogeneous thin films of ZnS depending on vaporization of this semiconductor material by continuous CO2 laser with a simple fan to ensure obtaining homogeneous films. ZnS thin films were annealed at temperature 200ºC, 300 ºC and 400ºC for (20) minute in vacuum environment. Optical properties of ZnS thin film such as absorbance, transmittance, reflectance, optical band gap, refractive index extinction coefficient and absorption coefficien
... Show MoreOne of the important objectives of the varistor is for a sustainable environment and reduce the pollution resulting from the frequent damage of the electrical devices and power station waste. In present work, the influence of Al2O3 additives on the non –linear electrical features of SnO2 varistors, has been investigated, where SnO2 ceramic powder doped with Al2O3 in three rates (0.005, 0.01, and 0.05), the XRD test improved that SnO2 is the primary phase, while CoCr2O4, and Al2O3 represent the secondary phases. The electrical tests of all prepared samples confirmed that the increasing of Al2O3 rates and sintering temperature improves and increase the electrical features, where the best results obtained at Al2O3 (0.05) and 1000℃, the non
... Show More(Sb2S3)1-xSnx thin films with different concentrations (0, 0.05 and
0.15) and thicknesses (300,500 and 700nm) have been deposited by
single source vacuum thermal evaporation onto glass substrates at
ambient temperature to study the effect of tin content, thickness and
on its structural morphology, and electrical properties. AFM study
revealed that microstructure parameters such as crystallite size, and
roughness found to depend upon deposition conditions. The DC
conductivity of the vacuum evaporated (Sb2S3)1-x Snx thin films was
measured in the temperature range (293-473)K and was found to
increase on order of magnitude with
Thin films of ZnSe arc deposited on glass substrates by thermal evaporation in vacuum with different thickness (1000, 2700, 4000) A° temperature (293-373) °K are studies the electrical properties before and after annealing. The result show decrease D.0 conductivity and increasing the activation energy Eat.