The current study executes a fully coupled thermomechanical simulation of friction stir welding (FSW) process of aluminum 6061-T6 alloy T-joint type using finite element method. The analysis simulation accounts for the three steps of the FSW process which includes: plunging, dwelling, and moving stages. The temperature history, associated stresses and strains generated through the FSW phases, tool reaction force, and time-dependence of the energy dissipation were evaluated. To overcome the shortcomings of purely Lagrangian and Eulerian descriptions, Arbitrary Lagrangian Eulerian (ALE) formulation, adaptive meshing, and the mass scaling were used as techniques to improve sequence modeling of the friction stir welding process. Coulomb’s friction law with nonlinear friction coefficient was used to model contact between the tool and T-joint configuration. To verify the numerical results, an experimental setup was constructed to carry out the FSW of a T-joint. Meanwhile, embedded thermocouples were used in the advancing side to measure temperature close to the welding line. The results obtained throughout the simulation study showed that the temperature was symmetrically distributed across the T-joint width, and the temperature contour displayed a high gradient in the weld stirring zone with a V type shape after the plunge stage. Good correlation between numerical and experimental temperature results was obtained with a little shift in the peak value. The results of von-Mises value showed that the maximum stress has been moved from the skin part gradually into the stringer part with the advancement of the tool during plunging. The plastic strain value was higher on the advancing side in comparison with the retreating side. Moreover, the heat generation calculation showed that the frictional dissipation energy was responsible for generating most of the heat needed to obtain a successful FSW.
The corrosion inhibition of aluminum alloy 5083 by an environment friendly compound called (8- Hydroxyquinoline) in
acidic and alkaline solutions of pH (2 and 12) respectively were studied using weight loss and polarization techniques.
Also to examine the main and combined effects of the inhibitor concentration, pH, and contact time using factorial
experimental design. Results show that corrosion rate decreased with increasing both inhibitor concentration and
contact time and increased with increasing pH value. The polarization curves show that 8-hydroxyquinoline is a
cathodic inhibitor
Aluminum alloy 5052 had been anodized by sulfuric acid as an electrolyte under constant voltage and the anodic oxide film produce will be testing by potentiostatic anodic polarization .Two variables, which were considered as important variables, were studied. These variables are anodizing time 15,30 min. and sealing time 10,20 min., and the test by potentiostatic anodic polarization through electro chemical polarization measurements in solutions of 1N na2so4 ( PH= 1 ). The results are discussed in light of the rate of ionic current flow through the coating during anodic polarization measurements.
The aim of this work is to study the factors that affect the welding joint of dissimilar metals. Austenitic stainless steel-type AISI (316L) with a thickness of (2mm) was welded to carbon steel (1mm) using an MIG spot welding. The filler metal is a welding wire of the type E80S-G (according to AWS) is used with (1.2mm) diameter and CO2 is used as shielding gas with flow rate (7L/min) for all times was used in this work.
The results indicate that the increase of the welding current tends to increase the size of spot weld, and also increases the sheer force. Whereas the sheer force increased inversely with the time of welding. Furthermore, the results indicate that i
... Show MoreThis research deals with the effects of welding variables using MIG/MAG spot by using Argon (Ar) gas and CO2 to show their effect on the mechanical characteristics and microstructure of low alloy steel type DIN15Mo3 and determine the optimum condition for the process of welding ; current & time. The results show the possibility of using CO2 and also Ar in low alloy steel welding with a little decrease in the shear force of not more than 13% for 4mm thickness and time 2sec. The shear force increased when using Ar instead of CO2 to be , The shear force reach 36KN when using Ar at 2mm thickness time of 8 sec and current of 220 Amp. , when used CO2 instead of Ar d
... Show MoreTwo different composite materials were prepared by stir casting method of AA 6061 alloy as a matrix reinforced with two addition different ceramic materials Al2O3 and B4C of grain size 20 µm by 2.5, 5, 7.5 and10% in weight. The composite material with aluminum alloy as a matrix possesses a unique mechanical properties such as: high specific strength and hardness, low density, and high resistance to corrosion and friction wear. This composite is widely used in automotive parts space and marine applications.
Pin-on-disc technique was used to calculate the wear rate for each addition of Al2O3 and B4C particles. Rockwell hardness test and
... Show MoreThe present study was conducted to evaluate the effect of different inhibitors on the corrosion rate of aluminum in 50% (v/v) ethylene glycol solution at 80°C and pH 8.0 in which the electrochemical technique of linear sweep voltammetry was employed to characterize each inhibitor function and to calculate the corrosion rate from Tafel plots generated by a computer assisted potentiostat.
It is found that both sodium dichromate and borax reduces the corrosion rate by polarizing the anodic polarization curve while sodium phosphate, potassium phosphate, and sodium benzoate reduces the corrosion rate by polarizing both the anodic and cathodic polarization curve.
When inhibitor concentration increases from I g/l up
... Show MoreThis paper focuses on the optimization of drilling parameters by utilizing “Taguchi method” to obtain the minimum surface roughness. Nine drilling experiments were performed on Al 5050 alloy using high speed steel twist drills. Three drilling parameters (feed rates, cutting speeds, and cutting tools) were used as control factors, and L9 (33) “orthogonal array” was specified for the experimental trials. Signal to Noise (S/N) Ratio and “Analysis of Variance” (ANOVA) were utilized to set the optimum control factors which minimized the surface roughness. The results were tested with the aid of statistical software package MINITAB-17. After the experimental trails, the tool diameter was found as the most important facto
... Show MoreCorrosion behavior of aluminum alloy 7025 was investigated in hydrochloric acid (pH=1) containing 0.6 mol.dm-3 NaCl in the existence and absence of diverse concentrations of sulphamethoxazole as environmentally friendly corrosion inhibitor over the temperature range (298-313)K. Electrochemical polarization method using potentiostatic technique was employed. The inhibition efficiency has been raised with increased sulphamethoxazole concentration but lessened at temperature increases. The highest efficiency value was 96.5 at 298 K and 2 x10-4 mol.dm-3 concentration of sulphamethoxazole. The sulphamethoxazole adsorption was agreed with Langmuir adsorption isotherm. Some thermodynamic parameter (△Gads) and activation energy (Ea) were determin
... Show More