This work compares the changes in optical and structural properties of cerium oxide (CeO2) when doped with different concentrations (3%,5%,7%, and 9%) of two oxides, In2O3 and Eu2O3. X-ray diffraction and spectrophotometry were employed in the visible, ultraviolet, and near-infrared regions. The findings demonstrated that CeO2 doped with In2O3 and Eu2O3 thin films were polycrystalline and had a cubic structure. The crystal size increased from 20.5 to 32.15 when Eu2O3 doping ratio increased from 0% to 7% and then decreased to 28.46 nm at 9%. While the crystal size showed an increase from 20.5 to 21.42 nm with the increase of the In2O3 doping ratio, while the lattice constant measured for cubic CeO2 changed opposite to that
... Show MoreThis study investigates the influence of phosphoric acid (H3PO4) molarity (2 M, 4 M, and 6 M) on the structural, thermal, optical, and electrical properties of polyvinyl alcohol (PVA)/20% graphene oxide (GO) composite films. X-ray diffraction analysis revealed a semi-crystalline nature for PVA, with characteristic peaks at 19.7 degrees and 42 degrees, and crystalline peaks for GO at 10.1 degrees and 39.8 degrees. The addition of H3PO4 to the PVA/GO composite resulted in the disappearance of GO crystalline peaks, suggesting reduced crystallinity. Differential scanning calorimetry revealed a reduction in both glass transition and melting temperatures as H3PO4 concentration increased. Pure PVA exhibited Tg and Tm values of 68.9 degrees C and 1
... Show MoreCompounds from ZnO doped with AgO in different ratio (0,3,5,7, and 9)wt.% were prepared.Thin films from the prepared compounds were deposited on a glass substrate using the pulsed laser deposition method. The XRD pattern confirmed the presence of a single-phase hexagonal wurtzite ZnO structure, without the presence of a secondary phase. AFM measurements showed an increase in both average grain size and average surface roughness with increasing concentration content of (AgO).The crystallite size of ZnO of the main peak corresponding to the preferred plane of crystal growth named (100) increases from 17.8 to 22.5nm by increasing of AgO doping ratio from 0 to 9%. The absorbance and transmittance in the wavelength range (350-1100 nm)
... Show MoreIn this work, two graphene oxide (GO) samples were prepared using the Hummers method with graphite (g) and KMnO4 (g) ratios of 1:3 (GO3) and 1:6 (GO6). The effect of oxidation degree on the structural, electrical, and dielectric properties of the GO samples was investigated. The structures of the GO samples were studied using various techniques, including X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, scanning electron microscopy (SEM), and energy-dispersive X-ray spectroscopy (EDXS). XRD analysis revealed an increase in the interlayer spacing and a decrease in the number of layers of the samples with increasing oxidant content. The two GO samples have giant permittivity values of ~105 in the low-frequency
... Show MoreIn the present work we prepared heterojunction not homogenous CdS/:In/Cu2S) by spray and displacement methods on glass substrate , CdS:In films prepared by different impurities constration. Cu2S prepared by chemical displacement method to improve the junction properties , structural and optical properties of the deposited films was achieved . The study shows that the film polycrystalline by XRD result for all film and the energy gap was direct to 2.38 eV with no effect on this value by impurities at this constration .
In the present work, the focusing was on the study of the x-ray diffraction, dielectric constant, loses dielectric coefficient, tangent angle, alter- natively conductivity and morphology of PET/BaTio3. The PET/BaTio3 composite was prepared for polyethylene terephthalate PET polymer composite containing 0, 10, 20, 30, 40, 50, and 60 wt. % from Barium titanate BaTi03 powder. The composite of two materials leads to form mixing solution and hot-pressing method. The effect of BaTio3 on the structure and dielectric properties with morphology was studied on PET matrix polymer using XRD, LCR meter and SEM.
The structural, optical and electrical properties of ZnS films prepared by vacuum evaporation technique on glass substrate at room temperature and treated at different annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction studies show that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (111). The optical properties investigated which include the absorbance and transmittance spectra, energy band gab, absorption coefficient, and other optical constants. The results showed that films have direct optical transition. The optical band gab was found to be in the range t
... Show MoreA high Tc superconductor with a nominal composition
(Bi1-xPbx)2(Sr1-yBay)2Ca2Cu3O10+δ for (0 £ x £ 0.5) and (0 £ y £ 0.5) was prepared by
a solid state reaction method. The effect of the substitution of Pb for Bi and Ba for Sr and
quenching temperature on the superconductivity has been investigated to obtain the
optimum conditions for the formation and stabilization of the high Tc phase (2223).
The results showed that the optimum sintering temperature for the pure composition is
equal to 875°C and the sintering time is equal to 240h with heating and cooling rate of
60°C/h . Our results indicated that a small amount of (Ba = 0.1) could raise the transition
temperature (Tc), but enhancing Ba to 0.4 has raised
This study includes the manufacture of four ternary alloys represented S60Se40-XPbX with weight ratios x = 0, 10, 20, and 30 by the melting point method. The components of each alloy were mixed separately, then placed in quartz ampoules and vacuumed out with a vacuum of roger that 10−4 Torr. The ampule was heated in two stages to avoid sudden dissipation and precipitation of selenium on the inner mass of the quartz tube. The ampoule was gradually heated and kept at 450°C for approximately 4 hours followed by 950°C for 10 hours.at a rate of 10 degrees Celsius, the temperature of the electric furnace