The rehabilitation of deteriorated pavements using Asphalt Concrete (AC) overlays consistently confronts the reflection cracking challenge, where inherent cracks and joints from an existing pavement layer are mirrored in the new overlay. To address this issue, the current study evaluates the effectiveness of Engineered Cementitious Composite (ECC) and geotextile fabric as mitigation strategies. ECC, characterized by its tensile ductility, fracture resistance, and high deformation capacity, was examined in interlayer thicknesses of 7, 12, and 17 mm. Additionally, the impact of geotextile fabric positioning at the base and at 1/3 depth of the AC specimen was explored. Utilizing the Overlay Testing Machine (OTM) for evaluations, the research demonstrated that ECC17 significantly mitigated reflection cracking, showing a notable 764% increase in the number of load cycles to failure (Nf) compared to the Geotextile Base (GB) specimen. Against the Reference Specimen (RS), ECC17 exhibited a remarkable 1307% enhancement in Nf values, underscoring its effectiveness. Geotextile fabric, particularly at 1/3 depth, demonstrated notable resistance but was overshadowed by the performance of ECC interlayers. The results clearly indicate that ECC, especially ECC17, stands out as an effective solution for mitigating reflection cracking, including joints, in AC overlays.
Portland cement concrete is the most commonly used construction material in the world for decades. However, the searches in concrete technology are remaining growing to meet particular properties related to its strength, durability, and sustainability issue. Thus, several types of concrete have been developed to enhance concrete performance. Most of the modern concrete types have to contain supplementary cementitious materials (SCMs) as a partial replacement of cement. These materials are either by-products of waste such as fly ash, slag, rice husk ash, and silica fume or from a geological resource like natural pozzolans and metakaolin (MK). Ideally, the utilization of SCMs will enhance the concrete performance, minimize
... Show MoreRoller-Compacted Concrete is a no-slump concrete, with no reinforcing steel, no forms, no finishing and wet enough to support compaction by vibratory rollers. Due to the effect of curing on properties and durability of concrete, the main purpose of this research is to study the effect of various curing methods (air curing, 7 days water curing, and permanent water curing) and porcelanite (local material used as an Internal Curing agent) with different replacement percentages of fine aggregate (volumetric replacement) on some properties of Roller-Compacted Concrete and to explore the possibility of introducing practical Roller-Compacted Concrete for road pavement with minimum requirement of curing. Specimens were sawed fro
... Show MoreImproving the permanent deformation resistance of asphalt pavements is a vital challenge. Nanomaterials have emerged as promising additives due to their ability to enhance the binder stiffness and elasticity. This study evaluated the influence of five nanomaterials, namely Nano-Silica (NS), Nano-Alumina (NA), Nano-Zinc (NZ), Nano-Titanium (NT), and Carbon Nanotubes (CNTs) incorporated into a base asphalt binder at varying dosages, with up to 10% for NS, NA, and NT, and up to 5% for NZ and CNT. Fifteen modified binders were assessed using the Multiple Stress Creep Recovery (MSCR) test to obtain non-recoverable creep compliance (Jnr), while the corresponding hot mix asphalt samples underwent repeated load testing and rut depth predict
... Show MoreThis research is carried out to investigate the behavior of self-compacting concrete (SCC) two-way slabs with central square opening under uniformly distributed loads. The experimental part of this research is based on casting and testing six SCC simply supported square slabs having the same dimentions and reinforcement. One of these slabs was cast without opening as a control slab. While, the other five slabs having opening ratios (OR) of 2.78%, 6.25%, 11.11%, 17.36% and 25.00%. From the experimental results it is found that the maximum percentage decrease in cracking and ultimate uniform loads were 31.82% and 12.17% compared to control slab for opening ratios (OR
... Show MoreA new pavement technology has been developed in Highway engineering: asphalt pavement production is less susceptible to oxidation and the consequent damages. The warm mix asphalt (WMA) is produced at a temperature of about (10-40) oC lower than the hot asphalt paving. This is done using one of the methods of producing a WMA. Although WMA's performance is rather good, according to previous studies, as it is less susceptible to oxidation, it is possible to modify some of its properties using different materials, including polymers. Waste tires of vehicles are one of the types of polymers because of their flexible properties. The production of HMA, WMA, and WMA modified with proportions of (1, 1.5, and 2%) of rub
... Show MoreThe subgrade soil is the foundation plate form of the roadway; it should sustain its structural characteristics throughout the design life of the roadway with minimal requirements for maintenance. When Gypseous soil is implemented in the construction of subgrade, problems regarding collapsibility and poor structural capacity usually occur when the subgrade came in touch with excess water. Asphalt stabilization could furnish a proper solution to such problems. In this investigation, an attempt has been made to monitor the variations in compressibility characteristics of asphalt stabilized subgrade soil subjected to 30 cycles of (freezing-thawing) and (heating-cooling). Data have been observed after each 10 cycles, and compared with that of r
... Show MoreRutting is one of the most complex and widespread types of distress. The rutting is frequently observed on Iraqi roads, especially at the checkpoints, forming a significant hazard on the asphalt layers. Factors such as heavy loads and high temperatures contribute to this distress. Adding fibers to a hot mix asphalt (HMA) effectively improves performance and extends the lifespan of the flexible pavement. This article used glass, steel, and basalt fibers. The wheel tracking test assessed the fibre-asphalt mixture for rutting resistance and compared it with the mix without adding fibers (control HMA). Meanwhile, the microscopic structure of fibres and asphalt mixture modified with fibers was examined using the Field Emission Scanning E
... Show MoreFailure in asphalt mixture and distress in pavement are major issues to roads infrastructure. Selecting an appropriate chemical composition of asphalt cement is a key component in avoiding these issues. This work aimed to investigate the effect of the chemical composition of different polar fractions on the rheological and physical properties of asphalt cement. Four types of asphalt cement with penetration grades of 20/30, 40/50, 60/70 and 85/100 were divided into four fractions. Complex shear modules, rutting resistance and rotational viscosity of the asphalt cement were determined by using a Dynamic Shear Rheometer and a Rotation Viscometer, respectively. The results show that an increase in the asphaltene content and Gastel index resulte
... Show MoreConcerns about the environment, the cost of energy, and safety mean that low-energy cold-mix asphalt materials are very interesting as a potential replacement for present-day hot mix asphalt. The main disadvantage of cold bituminous emulsion mixtures is their poor early life strength, meaning they require a long time to achieve mature strength. This research work aims to study the protentional utilization of waste and by-product materials as a filler in cold emulsion mixtures with mechanical properties comparable to those of traditional hot mix asphalt. Accordingly, cold mix asphalt was prepared to utilize paper sludge ash (PSA) and cement kiln dust (CKD) as a substitution for conventional mineral filler with percentages ranging fro
... Show More