Rutting is one of the most complex and widespread types of distress. The rutting is frequently observed on Iraqi roads, especially at the checkpoints, forming a significant hazard on the asphalt layers. Factors such as heavy loads and high temperatures contribute to this distress. Adding fibers to a hot mix asphalt (HMA) effectively improves performance and extends the lifespan of the flexible pavement. This article used glass, steel, and basalt fibers. The wheel tracking test assessed the fibre-asphalt mixture for rutting resistance and compared it with the mix without adding fibers (control HMA). Meanwhile, the microscopic structure of fibres and asphalt mixture modified with fibers was examined using the Field Emission Scanning Electron Microscopy (FESEM) technique. Steel, glass, and basalt fibers were incorporated into HMA in proportions of 0.25%, 0.10%, and 0.15%, respectively. The incorporation of fibers in asphalt mixtures implies lower rut depths after 5000 cycles. In comparison to the control HMA, a decrease in the rut depth is observed in fiber-asphalt mixtures, about 22.14%, 15.36%, and 9.64% for basalt, glass, and steel fiber, respectively, which consequently enhances flexible pavement resistance against rutting. The microstructure analysis showed the difference in the mixture's diameters, surface properties, and random fiber dispersion. Therefore, this dispersion contributed to creating a three-dimensional network, which improved the behaviour of HMA.
The filler in the asphalt mixture is essential since it plays a significant role in toughening and stiffening the asphalt. Changes in filler type can lead the asphalt mixtures to perform satisfactorily during their design life or degrade rapidly when traffic and environmental effects are considered. This study aims to assess the impact of filler types such as limestone dust (LS) and hydrated lime (HL) on Marshall characteristics and moisture damage in asphalt mixtures. Three different percentages of HL were employed in this study to partially replace the LS mineral filler: 1.5, 2.0, and 2.5% by aggregate weight. Furthermore, a control mixture was created with 7% LS by overall aggregate weight for the wearing course layer. The Marsha
... Show MoreExperts have given much attention on the use of waste in asphalt paving because of its significance from a sustainability perspective. This paper evaluated the performance properties of asphalt concrete mixes modified with Crumb Rubber (CR) as a partial replacement for two grade sizes of fine aggregate (2.36, and 0.3 mm) at six replacement rates: 0%, 2%, 4%, 6%, 8%, and 10% by weight. Asphalt concrete mixes were prepared at their Optimum Asphalt Content (OAC) and then tested for their engineering properties. Marshall properties, fatigue, rutting, ideal CT index test, Scanning Electron Microscopy (SEM), and Energy-Dispersive X-ray (EDX) spectroscopy were deployed to examine the crystalline structure and elemental composition of the C
... Show MorePermanent deformation (Rutting) of asphalt pavements which appears in many roads in Iraq, have caused a major impact on pavement performance by reducing the useful service life of pavement and creating services hazards for highway users. The main objective of this research is investigating the effect of some contributory factors related to permanent deformation of asphalt concrete mixture. To meet the objectives of this research, available local materials are used including asphalt binder, aggregates, mineral filler and modified asphalt binder. The Superpave mix design system was adopted with varying volumetric compositions. The Superpave Gyratory Compactor was used to compact 24 asphalt concrete cylindrical specimens. To collect t
... Show MoreFatigue cracking is the most common distress in road pavement. It is mainly due to the increase in the number of load repetition of vehicles, particularly those with high axle loads, and to the environmental conditions. In this study, four-point bending beam fatigue testing has been used for control and modified mixture under various micro strain levels of (250 μƐ, 400 μƐ, and 750 μƐ) and 5HZ. The main objective of the study is to provide a comparative evaluation of pavement resistance to the phenomenon of fatigue cracking between modified asphalt concrete and conventional asphalt concrete mixes (under the influence of three percentage of Silica fumes 1%, 2%, 3% by the weight of asphalt content), and (chan
... Show MoreMoisture-induced damage is one of the primary causes of premature distress in asphalt pavements, leading to reduced service life and increased maintenance costs. Although nanomaterials have shown potential in enhancing asphalt performance, the underlying composite interaction mechanisms among nanomaterials, asphalt binder, and aggregate phases under moisture exposure are still not fully understood. In addition, comparative evaluations under consistent experimental conditions remain limited. This study investigates the influence of five nanomaterials: nano-silica (NS), nano-alumina (NA), nano-titanium dioxide (NT), nano-zinc oxide (NZ), and carbon nanotubes (CNT) on the physical and mechanical properties of asphalt binders and mixtur
... Show MoreThis research aimed to predict the permanent deformation (rutting) in conventional and rubberized asphalt mixes under repeated load conditions using the Finite Element Method (FEM). A three-dimensional (3D) model was developed to simulate the Wheel Track Testing (WTT) loading. The study was conducted using the Abaqus/Standard finite element software. The pavement slab was simulated using a nonlinear creep (time-hardening) model at 40°C. The responses of the viscoplastic model under the influence of the trapezoidal amplitude of moving wheel loadings were determined for different speeds and numbers of cycles. The results indicated that a wheel speed increase from 0.5Km/h to 1.0Km/h decreased the rut depth by about 22% and 24% in conv
... Show MoreRutting in asphalt mixtures is a very common type of distress. It occurs due to the heavy load applied and slow movement of traffic. Rutting needs to be predicted to avoid major deformation to the pavement. A simple linear viscous method is used in this paper to predict the rutting in asphalt mixtures by using a multi-layer linear computer programme (BISAR). The material properties were derived from the Repeated Load Axial Test (RLAT) and represented by a strain-dependent axial viscosity. The axial viscosity was used in an incremental multi-layer linear viscous analysis to calculate the deformation rate during each increment, and therefore the overall development of rutting. The method has been applied for six mixtures and at different tem
... Show MoreLandfill and incineration are the most common and widely used methods to dispose of solid wastes; both of these techniques are considered the main sources of pollution in the world due to the harmful toxic emissions that are considered an environmental problem. Because of the large areas used by landfills, they are not always considered an economical method. With the increase in the production of solid materials, solid wastes increase the pressure on incinerators and landfills, making the environmental pollution hazard more serious. Instead, these waste materials can be used in some other applications. One of the most important of these applications is asphalt pavements, which are the most used types of pavements in the
... Show MoreRecycled asphalt concrete mixture are prepared, artificially aged and processed in the laboratory to maintain the homogeneity of recycled asphalt concrete mixture gradation, and bitumen content. The loose asphalt concrete mix was subjected to cycle of accelerated aging, (short –term aging) and the compacted mix was subjected to (long -term aging) as per Super-pave procedure. Twenty four Specimens were constructed at optimum asphalt content according to Marshall Method. Recycled mixture was prepared from aged asphalt concrete using recycling agent (soft asphalt cement blended with silica fumes) by (1.5%) weight of mixture as recycling agent content. The effect of recycling agent on aging after recycling process behavior
... Show More