Bond strength of acrylic teeth to heat cure acrylic resin and thermoplastic denture base materials
...Show More Authors

Background: tooth debonding was one of the major reasons for denture repair. With the use of recently introduced thermoplastic denture base materials the problem of tooth debonding increased due to the nature of the bond between these materials and the acrylic teeth. This study was aimed to assess the bond of the acrylic teeth to conventional heat cure acrylic resin and to thermoplastic resin denture base material and methods to enhance it. Materials and methods: acrylic resin teeth were bonded to heat cure acrylic resin with and without wetting the ridge laps of the teeth with monomer and acrylic teeth with prefabricated retentive holes, unmodified and modified, in their ridge laps were processed with Valplast thermoplastic resin denture base material. The samples were subjected to tensile forces till failure. Results: In general the chemical bond strength of acrylic teeth and heat cure acrylic resin was greater than the mechanical bond strength of the teeth with the Valplast thermoplastic denture base material. Wetting the acrylic resin teeth with monomer enhanced the bond strength with heat cure acrylic resin by 88%. Modifying the prefabricated retentive means of the acrylic resin teeth enhanced the bond strength with the Valplast thermoplastic resin denture base material by 58% Conclusion: wetting the ridge laps of the teeth can increase the bond strength of acrylic teeth and the conventional heat cure resin. A partial solution for the debonding of teeth from Valplast thermoplastic resin dentures is by modifying the prefabricated retentive means for the acrylic teeth to increase the bond strength.

Preview PDF
Quick Preview PDF
Publication Date
Fri Jan 01 2016
Journal Name
The Pharma Innovation
Preparation, spectroscopic study of Schiff base ligand complexes with some metal ions and Evaluation of antibacterial activity
...Show More Authors

Publication Date
Wed Apr 13 2016
Journal Name
The Pharma Innovation Journal
Preparation, spectroscopic study of Schiff base ligand complexes with some metal ions and Evaluation of antibacterial activity
...Show More Authors

The new bidentate Schiff base ligand namely [(E)-N1-(4-methoxy benzylidene) benzene-1, 2-diamine] was prepared from condensation of 4-Methoxy benzaldehyde with O-Phenylene diamine at 1:1 molar ratio in ethanol as a solvent in presence of drops of 48% HBr. The structure of ligand (L) was characterized by, FT-IR, U.V-Vis., 1H-, 13C- NMR spectrophotometer, melting point and elemental microanalysis C.H.N. Metal complexes of the ligand (L) in general molecular formula [M(L)3], where M= Mn(II), Co(II), Ni(II),Cu(II) and Hg(II); L=(C14H14N2O) in ratio (1:3)(Metal:Ligand) were synthesized and characterized by Atomic absorption, FT- IR, U.V-Vis. spectra, molar conductivity, chloride content, melting point and magnetic susceptibility from the above d

... Show More
View Publication Preview PDF
Publication Date
Wed Dec 15 2021
Journal Name
Natural Volatiles And Essential Oils
Metal complexes of the schiff base of 1H-indole_3_carbaldehyde were produced and their catecholase activities were assessed
...Show More Authors

Publication Date
Wed Mar 15 2023
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of a novel coating material on the microleakage of glass hybrid restoration in primary teeth – An in vitro study
...Show More Authors

Background: Glass ionomer restorations are widely employed in the field of pediatric dentistry. There is a constant demand for a durable restoration that remains functional until exfoliation. This study aimed to measure and compare the effect of a novel coating material (EQUIA Forte Coat) on the microleakage of glass hybrid restoration (EQUIA Forte HT) in primary teeth. Material and method: Thirty cavitated (class-II) primary molars were allocated randomly into two groups based on the coat application; uncoated (control) and coated group (experimental). Cavities were prepared by the use of a ceramic bur (CeraBur) and restored with EQUIA Forte HT with or without applying a protective coat (EQUIA Forte Coat). Samples went through the therm

... Show More
View Publication Preview PDF
Scopus (2)
Crossref (1)
Scopus Crossref
Publication Date
Wed Mar 15 2023
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of a novel coating material on the microleakage of glass hybrid restoration in primary teeth – An in vitro study
...Show More Authors

Background: Glass ionomer restorations are widely employed in the field of pediatric dentistry. There is a constant demand for a durable restoration that remains functional until exfoliation. This study aimed to measure and compare the effect of a novel coating material (EQUIA Forte Coat) on the microleakage of glass hybrid restoration (EQUIA Forte HT) in primary teeth. Material and method: Thirty cavitated (class-II) primary molars were allocated randomly into two groups based on the coat application; uncoated (control) and coated group (experimental). Cavities were prepared by the use of a ceramic bur (CeraBur) and restored with EQUIA Forte HT with or without applying a protective coat (EQUIA Forte Coat). Samples went through the

... Show More
Crossref (1)
Crossref
Publication Date
Fri Feb 08 2019
Journal Name
Iraqi Journal Of Laser
Sealing Depth of Q-Switched Nd:YAG 1064nm Laser in the Treatment of Patients with Hypersensitive Teeth: An In Vitro Study
...Show More Authors

The purpose of this work was to study the effects of the Nd:YAG laser on exposed dentinal
tubules of human extracted teeth using a scanning electron microscope (SEM). Eighty 2.5mm-thick
slices were cut at the cementoenamel junction from 20 extracted human teeth with an electric saw. A
diamond bur was used to remove the cementum layer to expose the dentinal tubules. Each slice was
sectioned into four equal quadrants and the specimens were randomly divided into four groups (A to D ).
Groups B to D were lased for 2 mins using an Nd:YAG laser at 6 pulses per second at energy outputs of
80 , 100 and 120 mJ. Group A served as control. Under SEM observation, nonlased specimens showed
numerous exposed dentinal tubules. SEM o

... Show More
View Publication Preview PDF
Publication Date
Tue Aug 15 2023
Journal Name
Sumer 1
The effect of silver diamine fluoride on the microleakage of glass ionomer restoration in primary teeth at different time intervals
...Show More Authors

Silver diamine fluoride (SDF) has shown effectiveness in hardening tooth structure and killing bacteria. Therefore, it can be used to prevent and arrest dental caries. Riva Star (SDF) treatment alone will stop cavities but will not reverse the cavitation. The Silver Modified Atraumatic Procedure, often known as Smart, is the optimum technique for regaining the tooth's structure and function. Glass ionomer was introduced in (1972) as a new material that has become one of the most widely used materials in restorative dentistry. By releasing fluoride ions, this material has a therapeutic impact on the surrounding tooth structure. Microleakage is the ingress of bacteria, its byproducts, toxins, chemicals, oral fluids, and ions between t

... Show More
View Publication
Scopus (3)
Crossref (2)
Scopus Crossref
Publication Date
Sun Jun 30 2019
Journal Name
Journal Of Engineering
An experimental and numerical investigation of heat transfer effect on cyclic fatigue of gas turbine blade
...Show More Authors

Blades of gas turbine are usually suffered from high thermal cyclic load which leads to crack initiated and then crack growth and finally failure. The high thermal cyclic load is usually coming from high temperature, high pressure, start-up, shut-down and load change. An experimental and numerical analysis was carried out on the real blade and model of blade to simulate the real condition in gas turbine. The pressure, temperature distribution, stress intensity factor and the thermal stress in model of blade have been investigated numerically using ANSYS V.17 software. The experimental works were carried out using a particular designed and manufactured rig to simulate the real condition that blade suffers from. A new cont

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Wed Sep 01 2010
Journal Name
Materials & Design
Influence of glass addition and sintering temperature on the structure, mechanical properties and dielectric strength of high-voltage insulators
...Show More Authors

View Publication
Scopus (13)
Crossref (10)
Scopus Clarivate Crossref
Publication Date
Tue Sep 11 2018
Journal Name
Iraqi Journal Of Physics
Characterization of thermo-physical and hardness properties of unsaturated polyester resin hybrid nano composites Sihama Issa Salih1, Waleed Bdaiwi Salih2, Husam Sakin Hamad2
...Show More Authors

In this work, two groups of nanocomposite material, was prepared from unsaturated polyester resin (UPE), they were prepared by hand lay-up method. The first group was consisting of (UPE) reinforced with individually (ZrO2) nanoparticles with particle size (47.23nm). The second group consists of (UPE) reinforced with hybrid nanoparticles consisting of zirconium oxide and yttrium oxide (70% ZrO2 + 30% Y2O3) with particles size (83.98nm). This study includes the effect of selected volume fraction (0.5%, 1%, 1.5%, 2%, 2.5%, 3%) for both reinforcement nano materials. Experimental investigation was carried out by analyzing the thermo-physical properties like thermal conductivity, thermal diffusivity and specific heat for the polymeric composit