In this work, the possibility of a multiwavelength mode-locked fiber laser generation based on Four-Wave Mixing (FWM) induced by Fe2O3-SiO2 nanocomposite material is investigated for the first time. A multiwavelength mode-locked pulses fiber laser are generated from Ytterbium–doped fiber laser (YDFL) due to the combined action of high nonlinear absorption and high refractive coefficients of Fe2O3-SiO2 nanocomposite incorporated inside YDFL ring cavity. Up to more than 20 lasing lines in the 1040–1070 nm band with an equally lines separation of ~0.6 nm have been observed by just simple variation of passive modulation of the state of the polarization and the pump power altogether. Moreover, a passively mode-locked operation of YDFL laser has been realized with repetition rate of 18.75 MHz and pulse width of 10 ps. The proposed laser offers excellent long-standing stability with the average amount of optical signal/noise ratio of more than 41 dBm. Our study may pave a novel technique to generate multiwavelength lasing from fiber laser with the assistance by nanocomposite disordered media at low threshold pumping.
The protective effect of benfotiamine against doxorubicin-induced cardiotoxicity was evaluated in rabbits. Pretreatment of rabbits with 70mg/kg benfotiamine orally 7 days before induction of cardiotoxicity with I.V 15mg/kg doxorubicin. injection resulted in significant reduction of the activities of lactate dehydrogenase and creatine phosphokinase enzyme in the serum compared to doxorubicin treated animals; benfotiamine also improves the histological changes produced by doxorubicin in the cardiac muscle compared to control. In conclusion, benfotiamine when used concomitantly with doxorubicin protects the myocardium against the cardiotoxicity induced by this cytotoxic drug.
The present study aimed to investigate the possible protective effect of cafestol against doxorubicin-induced chromosomal and DNA damage in rat bone marrow cells. Wistar
Albino rats of both sexes were administered cafestol (5mg/kg body weight once
Chemical spray pyrolysis technique was used at substrate temperature 250 ˚C with annealing temperature at 400 ˚C (for 1hour) to deposition tungsten oxide thin film with different doping concentration of Au nanoparticle (0, 10, 20, 30 and 40)% wt. on glass substrate with thickness about 100 nm. The structural, optical properties were investigated. The X-ray diffraction shows that the films at substrate temperature (250 ˚C) was amorphous while at annealing temperature have a polycrystalline structure with the preferred orientation of (200), all the samples have a hexagonal structure for WO3 and Au gold nanoparticles have a cubic structure. Atomic force microscopy (AFM) was used to characterize the morphology of the films. The optical pr
... Show MoreAgInSe2 (AIS) thin films solar cell involving of n-type AgInSe2 and Si of p-type substrate by using thermal evaporation method. The influence of annealing of the preparation AgInSe2 were considered to find the best properties of solar device. Thin film AIS have been deposited under the vacuum of 1.5*10-6 Torr with (400) nm thickness at R.T and annealing temperatures (473,573) K. Polycrystalline tetragonal structure for AIS thin films from XRD and increasing of surface roughness from AFM, energy gap values decreasing with increasing annealing temperatures, all films were negative type, I-V characteristics show increasing of efficiency with increasing of annealing temperatures.
Abstract: In this paper, a U-shaped probe with a curvature diameter of half a centimeter was implemented using plastic optical fibers. A layer of the outer shell of the fibers was removed by polishing to a D-section. The sensor was tested by immersing it in a sodium chloride solution with variable refractive index depending on solution concentrations ranging from 1.333 to 1.363. In this design, the sensor experienced a decrease in its intensity as the concentration of the solution increased. The next step The sensor was coated with a thin layer of gold with a thickness of 20 nm, and the sensor was tested with the same solutions which resulted in a shift in wavelengths where the shift in wavelength was 5.37 nm and sensiti
... Show MoreIn this work, seven soil samples were brought brought to study and analyses the element concentrations from different southern regions of Iraq using laser-induced breakdown spectroscopy (LIBS) technique. It has been documented as an atomic emission spectroscopy (AES) technique. Laser-induced plasma utilized to analyze elements in materials (gases, liquids, and solids). In order to analyze elements in materials (gases, liquids, and solid). The Nd: YAG laser excitation source at 1064 nm with pulse width 9 ns is used to generate power density of 5.5 x 1012 MW/mm2, with optical spectrum in the range 320-740 nm. From this investigation, the soil sample analysis of the southern cities of Iraqi, it is concluded that the rich soil element of P, Si,
... Show MoreIn this paper Zener diode was manufactured using ZnO-CuO-ZnO/Si heterojunction structure that used laser induced plasma technique to prepare the nanofilms. Six samples were prepared with a different number of laser pulses, started with 200 to 600 pulses on ZnO tablet with fixed the number of laser pulses on CuO tablet at 300 pulses. The pulse energy of laser deposited was 900mJ using ZnO tablet and 600mJ using CuO tablet. All prepared films shown good behavior as Zener diode when using porous silicon as substrate.
Fe2O3/ MgO composites with various ratios (90/10,80/20,70/30,60/40 and 50/50 %wt.) were synthesized. Their structure was determined using the X-ray diffractometer. The observed X-Ray patterns showed that the prepared composites were polycrystalline with rhombohedral Hematite (α-Fe2O3) whereas the preferred planes for crystal growth are (104) and (110).The dielectric properties of the Fe2O3/ MgO, with various ratios, were studied as function of frequency over the range (50Hz – 1MHz). The conductivity as function to frequency σa.c(ω) obey the power law relation σa.c(ω) =Aωs where the factor s was found to be in the range 0.329-0.491. The dielectric constant is increasing; but not in a regular way, with the increasing MgO content. The
... Show MoreThe work concerned with studying the effect of (SiO2) addition as a
filler on the adhesive properties of (PVA). Samples were prepared as
sheets by using casting method. The mechanical properties showed
that increase in tensile strength from (34MPa) to (68MPa) when
(SiO2) added to (PVA). The adhesive strength showed that joint
properties depend upon specific adhesive characteristic of material
(PVA) and (SiO2\PVA)composites at different concentrations (1.5%,
2.5%, 3.5%, 4.5wt%), the cohesive strength of the adhesive material,
the joint design, and adherent type (Sponge Rubber(SR), Natural
leather (NL), Vulcanized Rubber(VR), and Cartoon). The results
proved the tensile strength increased with (SiO2) ratio, so
In this paper, SiO2 nanoparticles thin films were synthesised at different PH values of solution by sol gel method at fixed temperature (25oC) and molar ratio (R =H2O/precursor) of (Tetra Ethyl Ortho Silicate) TEOS as precursor at (R=1). The structure and optical properties of the thin films have been investigated. All thin films were tested by using X-RAY diffraction. All X-RAY spectrum can be indexed as monoclinic structure with strong crystalline (110) plane. The morphological properties of the prepared films were studied by SEM. The results indicate that all films are in nano scale and the particle size around (19-62) nm .The size of silica particles increases with increasing PH value of solution where both the rate of hydrolysis and
... Show More