This study investigates the influence of silver oxide (Ag2O) concentration on the optical characteristics of phosphate bioactive glasses (PBGs). PBGs have emerged as promising alternatives to conventional silicate glasses in the medical field due to their excellent bioactivity and chemical resistance. Samples with varying Ag2O concentrations (0, 0.25, 0.5, and 0.75g) were sintered at 780°C for 2 hrs in an electric furnace. The samples were subjected to Fourier transfer infrared spectroscopy (FTIR), ultraviolet-visible (UV-Vis) spectroscopy, and photoluminescence (PL) tests to assess their functional groups and optical properties. By analyzing the FTIR spectrum of phosphate bioactive glass containing different amounts of Ag2O, it is possible to identify changes in the vibrational modes associated with Ag-O bonds and to gain insights into the structure and composition of the material. Because Ag-O bonds exhibit infrared vibrational modes, introducing Ag2O changed the FTIR spectrum. As Ag2O concentration increased, Ag-O vibrational modes strengthened, indicating more Ag-O bonds. UV-Vis spectroscopy, with increasing Ag2O concentration, the peak location shifted towards shorter wavelengths. Optical spectra show distinct UV absorption in the prepared glass spectrum, extending to near visible with increasing Ag2O content. The PL spectra peaks and band gap energies revealed that Ag2O altered the glass's electrical structure and optical activity. These discoveries help optimize metal-phosphate bi-active glass for biomedical implants and UV-blocking coatings. The melting-annealing technique prepared glasses based on the base host Na2O-CaF2-P2O5 system with increasing Ag2O as additives or loading (0.2 to 1 wt%).
In this work, ZnO nanostructures for powder ZnO were synthesized by Hydrothermal Method. Size and shape of ZnO nanostructureas can be controlled by change ammonia concentration. In the preparation of ZnO nanostructure, zinc nitrate hexahydrate [Zn(NO3)2·6H2O] was used as a precursor. The structure and morphology of ZnO nanostructure have been characterized by scanning electron microscopy (SEM), atomic force microscopy (AFM), X-ray diffraction (XRD). The synthesized ZnO nanostructures have a hexagonal wurtzite structure. Also using Zeta potential and Particle Size Analyzers and size distribution of the ZnO powder
Many people believe that diabetes appears after a psychological crisis, which is a misconception but it could be in them before having a crisis ore the crisis. But emotion increases the appearance of symptoms, and athletes are at risk of developing diabetes. Hypoglycemia is not unusual for athletes, and during physical activity the sugar level changes in the blood. Therefore, it is important to conduct tests for the measurement of sugar before and immediately after the activity, for the purpose of detecting the sharp drop in the sugar level and treating it, and the early detection is necessary to avoid the possibility of diabetes, the concept of psychological immunity in psychology is considered a positive concepts that maintain the balance
... Show MorePure and Fe-doped zinc oxide nanocrystalline films were prepared
via a sol–gel method using -
C for 2 h.
The thin films were prepared and characterized by X-ray diffraction
(XRD), atomic force microscopy (AFM), field emission scanning
electron microscopy (FE-SEM) and UV- visible spectroscopy. The
XRD results showed that ZnO has hexagonal wurtzite structure and
the Fe ions were well incorporated into the ZnO structure. As the Fe
level increased from 2 wt% to 8 wt%, the crystallite size reduced in
comparison with the pure ZnO. The transmittance spectra were then
recorded at wavelengths ranging from 300 nm to 1000 nm. The
optical band gap energy of spin-coated films also decreased as Fe
doping concentra