Copper zinc tin sulfide selenide, Cu2 ZnSn(S1−x Se x)4 , absorbers are promising earth-abundant and environmentally benign materials for low-cost photovoltaic applications. This study investigates the structural and optical properties of Cu 2 ZnSn(S1−x Se x)4 nanostructured thin films prepared by pulsed laser deposition using melt-quenched targets with selenium compositions x = 0.0–1.0. X-ray diffraction revealed that films with low selenium content remained amorphous, whereas higher selenium incorporation promoted the formation of polycrystalline kesterite–stannite phases with preferred orientations along (112), (200), (220), and (312). The crystallite size increased from 12.3 to 17.9 nm as selenium reached x = 1.0, indicating enhanced crystal growth. Atomic force microscopy showed composition-dependent surface evolution, where average roughness decreased initially, reached a maximum of 88.29 nm at x = 0.6, and then declined, reflecting structural reorganization during phase transition. Optical characterization by UV–Vis–NIR spectroscopy demonstrated high absorption coefficients exceeding 10 4 cm −1 in the visible region, confirming strong light-harvesting capability. The direct optical band gap was tunable between 2.00 and 2.30 eV, with the highest value observed at x = 0.6 due to quantum confinement, nanoscale disorder, and compositional effects. The refractive index, extinction coefficient, and dielectric constants decreased with selenium addition up to x = 0.6, then increased at higher selenium contents, indicating a strong correlation between composition and optical response. The combined results highlight selenium control as an effective route for tailoring phase stability, transparency, and photon management for devices.
This study includes the synthesis of new derivatives of 1, 2, 4- Triazole which are contain Schiff bases derived from 1, 4, 5, 6- tetrahydropyrimidine. The structures of these derivatives were characterized from their melting points, infrared spectroscopy and elemental analysis. These derivatives were tested for inhibition of E-coli and were all found to be active.
Preparation of superposed thin film (CdTe)1-xSex / ZnS) with concentration of (x= 0.1, 0.3, 0.5) at a temperature of substrate (Ts= 80 0C) by using Thermal Vacuum Evaporation System. The measurement of X-ray diffraction shows that the compounds CdTe, ZnS, (CdTe)1-xSex and (CdTe)1-xSex / ZnS have a polycrystalline structure, the C-V characteristic shows that the capacitance degrease by increasing the concentration (x) in reverse bias, while the I-V characteristic shows the current dark (Id) increase in forward and reverse bias by increasing (x) and the photocurrent (Iph) increase in reverse bias by increasing the concentration (x), the values of photocurrent are greater than from the values of the dark current for all concentrations
... Show MoreIn this work, ZnS thin films have been deposited by developed laser deposition technique on glass substrates at room temperature. After deposition process, the films were annealed at different temperatures (200ºC , 300 ºC and 400ºC ) using thermal furnace.The developed technique was used to obtain homogeneous thin films of ZnS depending on vaporization of this semiconductor material by continuous CO2 laser with a simple fan to ensure obtaining homogeneous films. ZnS thin films were annealed at temperature 200ºC, 300 ºC and 400ºC for (20) minute in vacuum environment. Optical properties of ZnS thin film such as absorbance, transmittance, reflectance, optical band gap, refractive index extinction coefficient and absorption coefficien
... Show MoreCopper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show MoreCadmium Oxide thin films were deposited on glass substrate by spray pyrolysis technique at different temperatures (300,350,400, 500)oC. The optical properties of the films were studied in this work. The optical band-gap was determined from absorption spectra, it was found that the optical band-gap was within the range of (2.5-2.56)eV also width of localized states and another optical properties.
Colloidal crystals (opals) made of close-packed polymethylmethacrylate (PMMA) were fabricated and grown by Template-Directed methods to obtain porous materials with well-ordered periodicity and interconnected pore systems to manufacture photonic crystals. Opals were made from aqueous suspensions of monodisperse PMMA spheres with diameters between 280 and 415 nm. SEM confirmed the PMMA spheres crystallized uniformly in a face-centered cubic (FCC) array. Optical properties of synthesized pores PMMA were characterized by UV–Visible spectroscopy. It shows that the colloidal crystals possess pseudo photonic band gaps in the visible region. A combination of Bragg’s law of diffraction and Snell’s law of refraction were used to calculate t
... Show MoreN-Benzylidene m-nitrobenzeneamines (Schiff bases) were prepared by condensation of m-nitroaniline with aromatic aldehydes. These Schiff bases were found to react with maleic anhydride to give 2-Aryl-3-(m-nitrophenyl)-2, 3-dihydro [1, 3] oxazepine–4, 7–diones and with phthalic anhydride to give 2-Aryl-3–(m-nitrophenyl)–2, 3–dihydrobenz|| 1, 2-e|||| 1, 3] oxazepine–4, 7-diones which were reacted with pyrrolidine to give the anilide–pyrrolidides of maleic acid and phthalic acid.
A polycrystalline CdSe thin films doped with (5wt%) of Cu was fabricated using vacuum evaporation technique in the substrate temperature range(Ts=RT-250)oC on glass substrates of the thickness(0.8?m). The structure of these films are determined by X-ray diffraction (XRD). The X-ray diffraction studies shows that the structure is polycrystalline with hexagonal structure, and there are strong peaks at the direction (200) at (Ts=RT-150) oC, while at higher substrate temperature(Ts=150-250) oC the structure is single crystal. The optical properties as a function of Ts were studied. The absorption, transmission, and reflection has been studied, The optical energy gap (Eg)increases with increase of substrate temperature from (1.65
... Show More