This paper studied the behaviour of reinforced reactive powder concrete (RPC) two-way slabs under static load. The experimental program included testing three simply supported slabs of 1000 mm length, 1000 mm width, and 70 mm thickness. Tested specimens were of identical properties except their steel fibers volume ratio (0.5 %, 1 %, and 1.5 %). Static test results revealed that, increasing steel fibers volume ratio from 0.5% to 1% and from 1% to 1.5%, led to an increase in: first crack load by (32.2 % and 52.3 %), ultimate load by (36.1 % and 17.0 %), ultimate deflection by (33.6 % and 3.4 %), absorbed energy by (128 % and 20.2 %), and the ultimate strain by (1.1 % and 6.73 %). The stiffness and ductility of the specimens also increased. A numerical analysis was performed using ANSYS 14.5 software. The FE analysis overestimated the ultimate load capacity of all specimens by (6–28) %, and underestimated the ultimate deflection by (22-44) %. The deflected shape and crack patterns of the FE models were similar to that of the corresponding experimental specimens. It was found out that the optimum values of steel fibers volume fraction are 1.5 % and 1.6%.
A new concrete rheometer is introduced including its innovation, actual design, working rules,
calibration, and reliability. A modified design of Tattersall two-point device is created. Some of
components are purchased from local and foreign markets, while other components and the
manufacturing process are locally fabricated. The matching viscosity method of determining the mixer
viscometer constants is demonstrated and followed to relate torque and rotational speed to yield stress
and viscosity (Bingham parameters). The calibration procedures and its calculation are explained.
Water is used as a Newtonian fluid, while; cement paste (cement + water) with w/c ratio equal to
(0.442) is used as a non-Newtonian fluid. Th
The results of research to reach the conditions that prevents the emergence of primary or secondary voids and achieve worker benefit from molded by almost 100%, which was the situation that cast poured in a mold heated and insulated from all sides to achieve freezing directional full starting from the region remote from the casting and ending then. Has also been compared to the microscopic structure of the resulting castings of various molding conditions, as these conditions have achieved the best sound microscopic structures.
In this research, the effect of reinforcing epoxy resin composites with a filler derived from chopped agriculture waste from oil palm (OP). Epoxy/OP composites were formed by dispersing (1, 3, 5, and 10 wt%) OP filler using a high-speed mechanical stirrer utilizing a hand lay-up method. The effect of adding zinc oxide (ZnO) nanoparticles, with an average size of 10-30 nm, with different wt% (1,2,3, and 5wt%) to the epoxy/oil palm composite, on the behavior of an epoxy/oil palm composite was studied with different ratios (1,2,3, and 5wt%) and an average size of 10-30 nm. Fourier Transform Infrared (FTIR) spectrometry and mechanical properties (tensile, impact, hardness, and wear rate) were used to examine the composites. The FTIR
... Show MoreDirect agglutination test was used to evaluate the immunogenicity of three different antigens inoculated in hamsters as one , two and three doses which were: Group (1) inoculated with autoclaved killed Leishmania tropica , Group (2) inoculated with BCG vaccine alone while Group (3) inoculated with mixed antigens (autoclaved killed Leishmania "AKL"+ BCG).(4) Control animals inoculated with phosphate buffer saline. The maximum level of antibody titers were evaluated in animal inoculated with one , two or three dose of mixed antigens (320 , 640 and 1280) respectively when it compared with animals inoculated with corresponding doses of AKL antigen (80 , 160 and 320) respectively. While the minimum level of antibody titers were observed in ani
... Show MoreThis paper presents the thermophysical properties of zinc oxide nanofluid that have been measured for experimental investigation. The main contribution of this study is to define the heat transfer characteristics of nanofluids. The measuring of these properties was carried out within a range of temperatures from 25 °C to 45 °C, volume fraction from 1 to 2 %, and the average nanoparticle diameter size is 25 nm, and the base fluid is water. The thermophysical properties, including viscosity and thermal conductivity, were measured by using Brookfield rotational Viscometer and Thermal Properties Analyzer, respectively. The result indicates that the thermophysical properties of zinc oxide nanofluid increasing with nanoparticle volume f
... Show MoreThe occurrence of two species of the genus Myxobolus Bütschli, 1882 (Myxozoa: Myxosporea) for the first time in Iraq from freshwater fishes.
In the current study, new derivatives were synthesized by reaction of N-hydroxyphthalimide with chloro acetyl chloride in the presence of Et3N as a base to form 1,3-dioxoisoindolin-2-yl 2-chloroacetate (B1), which in turn enters several reactions with different amines where it interacts with primary amines to give 1,3-dioxoisoindolin-2-yl acetate derivatives (B2-B4) in basic medium, in the same way it interacts with these amines but with adding KNCS to form thiourea derivatives (B5-B7). It also reacts with diamines to give bis(azanediyl) derivatives (compounds B8-B10). The prepared derivatives were diagnosed using infrared FTIR and 1HNMR,13CNMR for some derivatives. Compounds B4, B5 and B9 were measured as corrosion inhibitors the inhibitio
... Show MoreIn the present work the performance of semifluidized bed adsorber was evaluated for removal of phenolic compound from wastewater using commercial activated carbon as adsorbent. P-chlorophenol (4-Chlorophenol) and o-cresol (2-methylphenol) was selected as a phenolic compound for that purpose. The phenols percent removal, in term of breakthrough curves were studied as affected by hydrodynamics limitations which include minimum and maximum semifluidization velocities and packed bed formation in the column by varying various parameters such as inlet liquid superficial velocity (from Uminsf to 8Uminsf m/s), and retaining grid (sometimes referred to as adsorbent loading) to initial static bed height ratio (from 3-4.5). In
... Show MoreConcrete is the main construction material of many structures. Exposing to loads creates cracks in concrete, which reduce the performance and durability. The decrease of concrete cracks becomes a necessity demand to ensure more durability and structural integrity of the concrete structure. Autogenous healing concrete is a kind of new smart concretes, which has the ability to reclose its cracks by means of itself. Concrete self-healing is a type of free repairs processes, which is reduce direct and indirect cost of maintenance and repairing. This work targets to inspect the mechanical properties of concrete after using two combinations of two materials (20 kg/m3 calcium hydroxide Ca(OH