Osteoblast and osteoclast activity is disrupted in post-menopausal osteoporosis. Thus, to fully address this imbalance, therapies should reduce bone resorption and promote bone formation. Dietary factors such as phyto-oestrogens and Zn have beneficial effects on osteoblast and osteoclast activity. However, the effect of combinations of these factors has not been widely studied. We therefore examined the effect of coumestrol, daidzein and genistein in the presence or absence of zinc sulphate (Zn) on osteoclast and osteoblast activity. Osteoclast differentiation and bone resorption were significantly reduced by coumestrol (10- 7 m), daidzein (10- 5 m) and genistein (10- 7 m); and this direct anti-osteoclastic action was unaffected by Zn (10- 5 m). In addition, Zn augmented the inhibitory effect of phyto-oestrogens on the osteoblast-derived stimulus for osteoclast formation, significantly reducing the ratio of receptor activator of NF-κB ligand (RANKL)-to-osteoprotegerin mRNA expression in human osteoblast. We then examined the effect of these compounds on osteoblast activity. Mineralisation was enhanced by coumestrol (10- 5 to 10- 7 m), daidzein (10- 5 to 10- 6 m) and genistein (10- 5 m); and Zn significantly augmented this response. Zn and phyto-oestrogens also significantly enhanced alkaline phosphatase activity and Runt-related transcription factor 2 (Runx2) mRNA expression. On the other hand, Zn blunted phyto-oestrogen-induced type I collagen and osteocalcin expression and suppressed coumestrol and daidzein-stimulated osterix expression. Zn may therefore modify the anabolic action of phyto-oestrogens, promoting characteristics associated with early rather than late stages of osteoblast differentiation. Our data suggest that while Zn enhances the anti-osteoclastic effect of phyto-oestrogens, it may limit aspects of their anabolic action on bone matrix formation.
Objective: To evaluate the effect of mouth rinses (Biofresh and ZAK) on the surface micro hardness
of two light cure restorative material (Tetric ceram ivoclar-vivadent) and (3M Z 250) dental
composite.
Methodology: The microhardness values of (sixty) composite specimens were measured at the top
surfaces after 24 hours of immersion in different solutions (Biofresh, Zak mouth wash and distilled
water as control). Comparison done using descriptive statistics (mean, SD, SEM, minimum and
maximum values) and inferential statistics (ANOVA and LSD) test.
Results: The biofresh mouth rinse which has high alcohol containing has less effect on
microhardness of tetric ceram than the zak &distiled water , while the effect
Due to economic reasons or need for environmental conservatism or also preserve the natural resources; there has been an increasing shift towards the use of reclaimed asphalt pavement (RAP) materials in the pavement construction industry. Therefore, use the Reclaimed Asphalt Pavement (RAP) has been enormously increased in pavement construction and has been become common practice in many countries. Nevertheless, this is a relatively new concept in Iraq, and has to be remarked that is not used RAP in the production of HMA and this valuable material is mostly degraded. For this purpose, the reclaimed materials were collected from deteriorated pavement segments. The components of asphalt mixtures consist of: two asphalt penetration grades (40-5
... Show MorePVA, Starch/PVA, and Starch/PVA/sugar samples of different
concentrations (10, 20, 30 and 40 % wt/wt) were prepared by casting
method. DSC analysis was carried; the results showed only one glass
transition temperature (Tg) for the samples involved, which suggest
that starch/PVA and starch/PVA/sugar blends are miscible. The
miscibility is attributed to the hydrogen bonds between PVA and
starch. This is in a good agreement with (FTIR) results. Tg and Tm
decrease with starch and sugar content compared with that for
(PVA). Systematic decrease in ultimate strength, due to starch and
sugar ratio increase, is attributed to (PVA), which has more hydroxyl
groups that made its ultimate strength higher than that for
The aim of this study is to understand the effect of addition carbon types on aluminum electrical conductivity which used three fillers of carbon reinforced aluminum at different weight fractions. The experimental results showed that electrical conductivity of aluminum was decreased by the addition all carbon types, also at low weight fraction of carbon black; it reached (4.53S/cm), whereas it was appeared highly increasing for each carbon fiber and synthetic graphite. At (45%) weight fraction the electrical conductivity was decreased to (4.36Scm) and (4.27Scm) for each carbon fiber and synthetic graphite, respectively. While it was reached to maximum value with carbon black. Hybrid composites were investigated also; the results exhibit tha
... Show MoreThe current work studies the effect of adding chopped carbon fiber (CCF) on gypsum plaster properties (precisely the compressive strength and the modulus of rupture). The research plan consists of using six mixes of gypsum plaster; these mixes are divided into two groups according to the (Water/Gypsum) ratios (0.5 & 0.6). Each group was divided into three subgroups according to CCF volume fraction (Vf): 0.0%, 0.2% and 0.4%. Three cubic (50×50×50) mm and three prismatic (40×40×160) mm samples were performed for each mix. It was found that, the addition of CCF to the gypsum plaster mixes increases both the compressive strength and the modulus of rupture for both (W/G) ratios, an
In this study, Cobalt Oxide nanostructure was successfully prepared using the chemical spray pyrolysis technique. The cobalt oxide phase was analysed by X-ray Diffraction (XRD) and proved the preparation of two cobalt oxide phases which are Co3O4 and CoO phases. The surface morphology was characterized by Scanning Electron Microscope (SEM) images showing the topography of the sample with grain size smaller than 100 nm. The optical behavior of the prepared material was studied by UV-Vis spectrophotometer. The band gap varied as 1.9 eV and 2.6 eV for Co3O4 prepared from cobalt sulphate precursor, 2.03 eV and 4.04 eV for Co3O4 prepared from cobalt nitrate precursor, 2.04 eV and 4.01 eV for CoO prepared from cobalt chloride precursor where th
... Show MoreReactive Powder Concrete (RPC) could be considered as the furthermost significant modern high compressive strength concrete. In this study, an experimental investigation on the impact of micro steel fiber volume fraction ratio and gamma ray irradiation duration influence upon the compressive strength of RPC is presented. Three volume fraction ratios (0.0, 1.0 and 1.5) % was implemented. For each percentage of the adopted fiber ratios, six different irradiation duration was considered; these are (1, 2, 3, 4, 5 and 6) days. Gamma source (Cs-137) of energy (0.662) MeV and activity (6) mci was used. In a case of zero volume fraction ratio, the experimental results showed that gamma ray had a significant influence on the reducing of the
... Show MoreReactive Powder Concrete (RPC) could be considered as the furthermost significant modern high compressive strength concrete. In this study, an experimental investigation on the impact of micro steel fiber volume fraction ratio and gamma ray irradiation duration influence upon the compressive strength of RPC is presented. Three volume fraction ratios (0.0, 1.0 and 1.5) % was implemented. For each percentage of the adopted fiber ratios, six different irradiation duration was considered; these are (1, 2, 3, 4, 5 and 6) days. Gamma source (Cs-137) of energy (0.662) MeV and activity (6) mci was used. In a case of zero volume fraction ratio, the experimental results showed that gamma ray had a significant influence on the reducing of the
... Show More