Background: The ideal maxillofacial prosthesis should have fine and thin boundaries that bindwith the surrounding facial structures and possess high tear strength.This study aims to determinethe best percentages of nanofiller (TiO2) and intrinsic pigment (silicone functional intrinsic) thatcould be mixed in as additives to improve the tear strength of Cosmesil M511 andVST50F siliconeelastomers with the least effect on their hardness.Materials and Methods: In this in vitro experimental study, a total of 80 samples, 40 for eachelastomer, were fabricated. Each elastomer sample was split into two equal groups to test for tearstrength and Shore A hardness. Each group consisted of 20 samples, including 10 control sampleswithout additives and 10 experimental samples with additives (mixtures of 0.2 wt% nano‑TiO2 + 0.25wt% intrinsic pigment and 0.25 wt% nano‑TiO2 + 0.25 wt% intrinsic pigment for the CosmesilM511 and VST50F silicone elastomers, respectively).Two‑way ANOVA and Tukey test were usedfor comparison; P < 0.05 was considered statistically significant.Results: Significant differences in tear strength were found among all tested groups (P < 0.05).The tear strength of the experimental subgroups significantly increased compared with the controlsubgroups (P < 0.05). Significant differences in Shore A hardness were also observed among alltested groups (P < 0.05) except between the experimental subgroups of both materials, where anonsignificant difference was obtained (P > 0.05).Conclusion: Incorporation of select percentages of TiO2 nanofiller and intrinsic pigment intoCosmesil M511 andVST50F silicone elastomers yields improvements in tear strength with a slightincrease in hardness (PDF) Impact of a mixture of nanofiller and intrinsic pigment on tear strength and hardness of two types of maxillofacial silicone elastomers. Available from: https://www.researchgate.net/publication/343647971_Impact_of_a_mixture_of_nanofiller_and_intrinsic_pigment_on_tear_strength_and_hardness_of_two_types_of_maxillofacial_silicone_elastomers [accessed Apr 05 2023].
This study has three parts, the first one is the synthesis of a novel Schiff bases by the condensation of guanine or 9-[{2-hydroxyethoxy}methyl]-9H-guanine with variety aldehydes to yield four different bases as follows: (E)-2-((4-nitrobenzylidene)amino)-1,9-dihydro-6H-purin-6-one (S1), (E)-2-((4-methoxybenzylidene)amino)-1,9-dihydro-6H-purin-6-one (S2), (E)-2-((2-hydroxybenzylidene) amino)-9-((2-hydroxy ethoxy)methyl)-1,9-dihydro-6H-purin-6-one (S3), and (E)-2-(((9-((2-hydroxy ethoxy)methyl)-6-oxo-6,9-dihydro-1H-purin-2-yl)imino)methyl)benzoic acid (S4). Then, spectroscopic analyses such as Elemental Analysis, UV/VIS, Mass spectra, FTIR, 1H,13C-NMR were made to recognize these bases. In the second part, the ability of synthesized bases to
... Show MoreThis in vitro study evaluated the influence of chemomechanical caries removal solution on the surface topography of metal-ceramic feldspar porcelain (MAJOR ceramic) and All-ceramic feldspar porcelain (Vita Alpha) using light polarizing microscope. Forty specimens of MAJOR ceramic and forty specimens of Vita Alpha ceramic of (12mm diameter & 3mm height) were prepared .All specimens were polished with silicon polishing burs, cleaned, autoglazed and stored in 37°C before exposure to Carisolv. Thirty specimens of each material randomly exposed to Carisolv gel for 5, 10 and 20 minutes respectively, other ten specimens were not, to act as control group. All specimens were subjected to surface roughness test by profilometer and evalua
... Show MorePremature degradation is the problem of maxillofacial silicones, significantly affected by ultraviolet exposure, contributing to silicones photodegradation. Degradation necessitates frequent replacement of prostheses that increase the total cost of rehabilitation.
This study evaluated the effect of bisoctrizole on the ultraviolet absorption properties of silicone material and the stability of this absorption over time. Also, the bisoctrizole effect on the surface roughness of silicone was evaluated.
There are no single materials which can withstand all the extreme operating conditions in modern technology. Protection of the metals from hostile environments has therefore become a technical and economic necessity.
In this work, for enhancing their wear-resistance, boride layers were deposited on the surface of low carbon steel by a pack cementation method at 850 °C for (2, 4, and 6) h using vacuum furnace. The boronizing process was achieved using different concentration of boron source (20, 25, and 30) % wt. into coating mixture to optimize the best conditions which ensure the higher properties with lower time. The coating was characteristic by X ray diffraction (XRD), and it is confirmed t
... Show MoreBackground: Acute myocardial infarction (AMI) is one of the most common diagnoses in hospitalized patients. Increased plasma hemostatic markers were noted in acute myocardial infarction, indicating that the blood coagulation system is highly activated in those patients. Aims of the study: To study the level of intrinsic coagulation factors including (FVIII:C, FIX:C ,FXI:C ,FXII:C ) in patients with acute myocardial infarction. Type of the study: Cross –sectional study. Methods: Thirty patients (their age range is 48-68 years) were included in this study (9 female, 21 male) who were just admitted to the coronary care unit in AL-Yarmouk Teaching Hospital and diagnosed as having acute myocardial infarction patients, blood samples were tak
... Show MoreExcess alcohol consumption is associated with numerous metabolic changes and homeostasis disturbances of many macro- and micro-elements in the body. It has been associated with multiple pathologies at all levels. In the digestive apparatus, alcohol has generally been related to its toxic effects upon the liver. Alpha-1 antitrypsin (α-1 AT or AAT) plays an important role in controlling inflammation, coagulation and repair mechanisms in the body and most α-1 AT in the body is produced by the liver; from the other hand, Intrinsic factor (IF), which is a glycoprotein produced by the parietal cells of the stomach is necessary for the absorption of vitamin B12 in the small intestine. This study was designed to assess serum levels of α-1 AT and
... Show MoreThe vacancy of natural resources is undoubtedly limited by time. The sustainable development principle recommends modern technology for its protection and renewal. This project conducted analyses on two underground water sources in the north of Algeria (Mechroha Province). Besides, the use of the hardness factor and the adoption of the titration method, which is the determining the concentration of an unknown solution using a known solution concentration, have permitted the characterization of the examples taken and to verify their conformity to the standard required, the results found showed HT=6.66 French degrees (oF) ) for Ain Guilloume water spring in comparison to Ain Messai water spring H
Background: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in
... Show MoreFacial trauma in children and adolescents is reported to range from 1% to 30%. Because of many anatomical, physiological, and psychological characteristics of the pediatric population, maxillofacial injuries in children should be treated with special consideration that is attributable to certain features inherent in facial growth patterns of children. This study evaluated maxillofacial injuries in 726 children in terms of incidence, patterns of injury, causes, and treatment modalities and compared these parameters among 3 pediatric age groups. Intergroup differences were analyzed using Z test for 2 populations' proportion. The results showed that the incidence of pediatric maxillofacial injuries and fractures is higher than that reported el
... Show More