Preparation of epoxy/ TiO2 and epoxy/ Al2O3 nanocomposites is studed and investigated in this paper. The nano composites are processed by different nano fillers concentrations (0, 0.01, 0.02 ,0.03, 0.04 ,0.05 ,0.07 and 0.1 wt%). The particles sized of TiO2,Al2O3 are about 20–50 nm.Epoxy resin and nano composites containing different shape nano fillers of (TiO2:Al2O3 composites),are shear mixing with ratio 1 to 1,with different nano hybrid fillers concentrations( 0.025 ,0.0 5 ,0.15 ,0.2, and 0.25 wt%) to Preparation of epoxy/ TiO2- Al2O3 hybrid composites. The mechanical properties of nanocomposites such as bending ,wearing, and fatigue are investigated as mechanical properties.
Concrete structures is affected by a deleterious reaction, which is known as Alkali Aggregate Reaction (AAR). AAR can be defined as a chemical reaction between the alkali content in the pore water solution of the cement paste and reactive forms of silica hold in the aggregate. This internal reaction produces expansion and cracking in concrete, which can lead to loss of strength and stiffness. Carbon fiber-reinforced polymer (CFRP) is one of the methods used to suppress further AAR expansion and rehabilitate and support damaged concrete structures. In this research, thirty-six cylindrical specimens were fabricated from non-reactive and reactive concrete, which contained fused silica as
Premature failure in asphalt concrete pavement has been the main concern for pavement construction companies and engineers in recent years because of the large rise in traffic volume and loads and the temperature extremes in the summer and winter. The use of modifiers in asphalt concrete mixtures has attracted much attention to increase the performance and lifespan of pavements. As nanotechnology developed, several researchers concentrated on how these materials can help increase pavement serviceability by minimizing rutting and moisture damage. This study evaluates the Hydrated Lime (HL) effect by two methods (wet and dry hydrated lime) on the durability of the warm mix asphalt. The first method, HL, has been supplemented to the as
... Show MoreRecently, some of Iraq's newly constructed asphalt concrete pavements showed premature failures with significant negative impacts on roadway safety and the economy. Using Nano hydrated lime (NHL) in pavement construction could be one of the possible steps to improve pavement durability. This article discusses how NHL affects the durability of hot mix asphalt. NHL was added in two methods to the asphalt concrete mixture for the wearing course. The first is the dry method, i.e., on the aggregate, whereas the second is the wet addition method, i.e., to the bitumen. The percentages were tried for each additional method; 1, 2, and 3% by weight of aggregate for the dry method and 0.5, 1, and 1.5% by weight of asphalt concrete for the wet
... Show MorePrevious experimental studies have suggested that hot mixed asphalt (HMA) concrete using hydrated lime (HL) to partially replace the conventional limestone dust filler at 2.5% by the total weight of all aggregates showed an optimum improvement on several key mechanical properties, fatigue life span and moisture susceptibility. However, so far, the knowledge of the thermal response of the modified asphalt concrete and thermal influence on the durability of the pavement constructed are still relatively limited but important to inform pavement design. This paper, at first, reports an experimental study of the tensile fatigue life of HMA concrete mixes designed for wearing layer application. Tests were conducted under three different temperatur
... Show MoreObjective Advantageous properties of silicone elastomer made it one of the favorable materials in maxillofacial prosthesis construction, but these properties may change after months of usage or after pigments addition. This study aimed to define the optimum concentration for a mixture of two types of intrinsic pigments that added to VST-50 maxillofacial silicone material and study their effects on mechanical properties before and after artificial aging. Methods After the pilot study was conducted, 0.1% by weight of rayon flocking and 0. 2% by weight of burnt sienna intrinsic pigment concentration was selected because of improvement in tested mechanical properties of VST-50 maxillofacial silicone. A total of one hundred and eighty samples we
... Show MoreThe research aims to investigate the effects of GMAW or MIG welding process on the mechanical properties of dissimilar aluminum alloys 2024-T351 and AA 6061- T651. A series of experimental techniques have been conducted to evaluate mechanical properties of the alloys, by carrying out hardness, tensile and bending tests for welded and un-welded specimens.
Metal inert gas (MIG) has been carried out on sheet metal using ER- 4043(AlSi5) as a filler metal and argon as shielded gas. The welded joints were tested by X-ray radiography and Faulty pieces were excluded.
Welding joints without defects are subjected to heat treatment including heating the joints in furnace to 170 °C for half an hour then air cooling to rel
... Show MoreThe aim of this research is to develop mechanical properties of a new aluminium-lithium-copper alloy. This alloy prepared under control atmosphere by casting in a permanent metal mould. The microstructure was examined and mechanical properties were tested before and after heat treatment to study the influence of heat treatment on its mechanical properties including; modulus of elasticity, tensile strength, impact, and fatigue. The results showed that the modulus of elasticity of the prepared alloy is higher than standard alloy about 2%. While the alloy that heat treated for 6 h and cooled in water, then showed a higher ultimate tensile stress comparing with as-cast alloy. The homogenous heat treatment gives best fatigue
... Show MoreOverlapped have been prepared from epoxy resin material added to carbon Nanotube and percentages weight (0.1, 0.05, 0.01) % Studied the mechanical properties of the composite (bending, tensile an d hardness) has been found that the Flexural and tensile modulus of the composites were higher than the pure epoxy resin this may be due to the high mechanical strength of carbon nano tube (CNT). The hardness of the epoxy carbon Nanotube composites increased and the reason is due to increased overlap and stacking between the additives and material basis, which reduces the movement of polymer molecules leading to increased resistance to scratching material and cutting, will become more resistance to plastic deformation.