The combined system of electrocoagulation (EC) and electro-oxidation (EO) is one of the most promising methods in dye removal. In this work, a solution of 200 mg/l of Congo red was used to examine the removal of anionic dye using an EC-EO system with three stainless steel electrodes as the auxiliary electrodes and an aluminum electrode as anode for the EC process, Cu-Mn-Ni Nanocomposite as anode for the EO process. This composite oxide was simultaneously synthesized by anodic and cathodic deposition of Cu (NO3)2, MnCl2, and Ni (NO3)2 salts with 0.075 M as concentrations of each salt with a fixed molar ratio (1:1:1) at a constant current density of 25 mA/cm2. The characteristics structure and surface morphology of the deposited nano oxides onto the graphite substrates were determined by (XRD), (FE-SEM), (AFM), and (EDX). The results shown that nano Cu-Mn-Ni oxides were successfully deposited onto the anode and cathode. The crystal size and root mean square for the cathode were 30.79 nm and 79.36 nm, respectively, while for the anode, they were 24.19 nm and 41.88 nm, respectively. Furthermore, the combined system was examined for C.D, NaCl concentration, and time. In the EC-EO combined system, the cathode and anode were efficient when used as anodes for the EO process, besides aluminum. The cathode was more effective in the removal process than the anode due to its larger crystal size and the rough, granular shape of its surface. When current density (C.D) increased from 3 to 6 mA/cm², the removal efficiency shifted from 95% to 98%. However, excellent removal of 98% and 96.5% was attained with 1.665 and 2.0859 kWh/kg of dye as energy consumption in the presence and absence of NaCl salt, respectively by applying 6 mA/cm2 within 20 min of electrolysis.
In the present study, advanced oxidation treatment, the TiO2 /UV/H2O2 process was applied to decolorisation of the reactive yellow dyes in aqueous solution. The UV radiation was carried out with a 6 W low-pressure mercury lamp. The rate of color removal was studied by measuring the absorbency at a characteristic wavelength. The effects of H2O2 dosage, dye initial concentration and pH on decolorisation kinetics in the batch photoreactor were investigated. The highest decolorisation rates were observed (98.8) at pH range between 3 and 7. The optimal levels of H2O2 needed for the process were examined. It appears that high levels of H2O2 could reduce decolori
... Show MoreBackground: Prophylaxis methods are used to mechanically remove plaque and stain from tooth surfaces; such methods give rise to loss of superficial structure and roughen the surface of composites as a result of their abrasive action. This study was done to assess the effect of three polishing systems on surface texture of new anterior composites after storage in artificial saliva. Materials and methods: A total of 40 Giomer and Tetric®N-Ceram composite discs of 12 mm internal diameter and 3mm height were prepared using a specially designed cylindrical mold and were stored in artificial saliva for one month and then samples were divided into four groups according to surface treatment: Group A (control group):10 specimens received no surfa
... Show MoreThe electro-optic coefficient r63 and r41 are determined in congruent KDP crystals, using an experimental method based upon the direct measurement of material. Sénarmont system for electro-optic coefficient measurement and characterization of crystals was modified. This modification allowed us to obtain on the frequency dispersion dependence of the electro-optic coefficients within a frequency range up to 20 MHz and on a new version of modulation depth method. To the best of our knowledge, by using this system, the electro-optic coefficients r63 and r41 in different configurations (transverse and longitudinal) have been measured for the first time within a frequency range up to 20 MHz. The measurements have been investigated as a functi
... Show Moreسمير خلف فياض * و محسن طالب د.نوال عزت عبد اللطيف*, مجلة الهندسة والتكنولوجيا, 2010
Background: This study compared in vitro the marginal adaptation of three different, low shrink, direct posterior composites Filtekâ„¢ P60 (packable composite), Filtekâ„¢ P90 (Silorane-based composite) and Sonic fillâ„¢ (nanohybrid composite) at three different composite/enamel interface regions (occlusal, proximal and gingival regions) of a standardized Class II MO cavity after thermal changes and mechanical load cycling by scanning electron microscopy. Materials and methods:Thirty six sound human maxillary first premolars of approximately comparable sizes were divided into three main groups of (12 teeth) in each according to the type of restorative material that was used: group (A) the teeth were restored with Filtekâ„¢ P6
... Show MoreLaser drilling is capable of producing small, precisely positioned holes with high degree of reproductively. In this paper , IR millisecond Nd:YAG single pulsed laser was used to determine the effect of laser parameters on the drilled hole of the glass - fiber reinforced epoxy composite FR-4 sample of 2 mm in thickness . The type of laser source was GSI lumonics JK760TR Series laser 1.064μm system in a CNC cabin. The JK760TR series has a 0.3-50ms pulse length and a maximum repetition rate 500Hz with an average power of 600W. The investigation of single pulse laser drilling in this paper was based on theoretical and experimental solutions. In single pulse technique, the investigation included focal plane position fpp, pulse shap
... Show MoreAn Indirect simple sensitive and applicable spectrofluorometric method has been developed for the determination of Cefotaxime Sodium (CEF), ciprofloxacin Hydrochloride (CIP) and Famotidine (FAM) using reaction system bromate-bromide and acriflavine (AF) as fluorescent dye. The method is based on the oxidation of drugs with known excess bromate-bromide mixture in acidic medium and subsequent determination of unreacted oxidant by quenching fluorescence of AF. Fluorescence intensity of residual AF was measured at 528 nm after excitation at 402 nm. The fluorescence-concentration plots were rectilinear over the ranges 0.1-3.0, 0.05-2.6 and 0.1-3.8 µg ml-1 with lower detection limits of 0.013, 0.018 and 0.021 µg ml-1 an
... Show MoreManganese dioxide rotating cylinder electrode prepared by anodic deposition on a graphite substrate using MnSO4 solution in the presence of 0.918 M of H2SO4. The influence of different operational parameters (MnSO4 concentration, current density, time, and rotation speed) on the structure, and morphology of MnO2 deposit film was examined widely. The structure and crystal size determined by X-ray diffraction (XRD), the morphology examined by scanning electron microscopy (SEM) and atomic force microscopy (AFM) techniques. The γ-MnO2 obtained as the main product of the deposition process. It found that the four parameters have a significant influence on the structure, morphology, and roughness of the prepared MnO2 deposit. The crystal size in
... Show More