This study investigates the influence of five nanomaterials nano-alumina (NA), nano-silica (NS), nano-titanium (NT), nano-zinc oxide (NZ), and carbon nanotubes (CNT)on enhancing the fatigue resistance of asphalt binders. NA, NS, and NT were incorporated at dosages of 2%, 4%, 6%, 8%, and 10%, while NZ and CNT were added at 1%, 2%, 3%, 4%, and 5%. A series of physical, rheological, and performance-based tests were conducted, including penetration, softening point, ductility, and rotational viscosity. Based on the outcomes of the overall desirability evaluation, the first three dosages of each nanomaterial were selected for further testing due to their superior workability and binder flexibility. Subsequent investigations included the high-temperature performance grade, fatigue parameter (G*.sin δ), Linear Amplitude Sweep (LAS), and IDEAL-CT test integrated with Digital Image Correlation (DIC). The results confirmed that nanomaterial modification significantly enhanced asphalt binder performance, though the effectiveness varied with type and dosage. Physical tests demonstrated improved stiffness, softening point, and reduced temperature susceptibility, with slight ductility losses at higher dosages. Rotational viscosity analysis indicated that low-to-moderate contents ensured workability excluding high CNT dosages which exceeded Superpave limits. High-temperature PG improved notably with NS, NZ, and CNT, while NA and NT showed limited gains. Fatigue parameter results (G*.sin δ) identified NA and NT as the most consistent in reducing cracking susceptibility. LAS testing confirmed superior fatigue lives at optimal dosages of 6% NA, 6% NT, 2% NS, 2% CNT, and 1% NZ, while higher concentrations often caused agglomeration and performance decline. IDEAL-CT and DIC analyses validated these findings by demonstrating increased fracture energy, CT index, and more uniform strain distributions in nano-modified mixtures compared to neat asphalt. FTIR spectra confirmed reduced oxidative aging most prominently with NT and NA while SEM revealed enhanced microstructural cohesion and reduced surface defects. The integration of the Overall Desirability (OD) framework confirmed NT-6 as the most effective dosage, followed by NZ-1 and NS-2, while higher dosages often led to poor compatibility and performance decline. Complementary cost–effectiveness analysis further demonstrated that lower dosages of NZ, NT, and NS achieved the best balance between technical performance and economic viability, whereas excessive CNT and NT contents were not recommended due to unfavorable cost-to-performance ratios. These findings highlight that dosage optimization is critical for translating nanomaterial benefits into practical pavement engineering applications, ensuring enhanced durability with rational investment of resources.
With the increasing intensity of the ecological and environmental problems and the scarcity of fresh water, this paper was introduced to investigate the ability to use treated wastewater as a cooling media via studying its behavior throughout a cooling tower. The simultaneous transfer of heat and mass from the treated wastewater to air over splash-fill packing arranged in a zigzag manner was studied. The characteristic of the cooling tower, the outlet water temperature, and the rejected heat were investigated as the water-to-air ratio and inlet water temperature were varied. The core results show that the cooling tower of the tower decreases with increasing water-to-air ratio, and increases with the raise of inlet water temperature.
... Show MoreBackground: The aim of this study was to measure the radiopacity (RO) of modified microhybrid composite resins by adding 2 types of nanofillers (Zinc Oxide and Calcium Carbonate) in two concentrations 3% and 5% and comparing them to unmodified microhybrid composite resins and to nanofilled composite resin. Materials and Methods: Two types of composite resin were used (Microhybrid composite MH Quadrent anterior shine and Nanofilled composite resin Filtek Z350 XT), for each tested group five disk-shaped specimens (1-mm-thick and 15 mm diameter) were fabricated. The material samples were radiographed together with the aluminum step wedge. The density of the specimens was determined with a transmission densitometer and was expressed in term of
... Show MoreNanofluids, liquid suspensions of nanoparticles (Np), are an effective agent to alter the wettability of oil-wet reservoirs to water-wet thus promoting hydrocarbon recovery. It can also have an application to more efficient carbon storage. We present a series of contact angle (θ) investigations on initially oil-wet calcite surfaces to quantify the performance of hydrophilic silica nanoparticles for wettability alteration. These tests are conducted at typical in-situ high pressure (CO2), temperature and salinity conditions. A high pressure–temperature (P/T) optical cell with a regulated tilted surface was used to measure the advancing and receding contact angles at the desired conditions. The results showed that silica nanofluids can alte
... Show MoreThis research studies the effect of adding five different percentages of polymer (2, 4, 6, 8, and 10% of cement weight) on cement mortar's fresh and hardened properties, which was cured at laboratory temperature for 7, 14, and 28 days. Workability increases with increasing polymer. The workability value was lowest (25.6 and 29.4) % in mixtures containing 2% and 4% of (SBR). Increasing polymer ratios significantly decreased mechanical properties (compressive and flexural strength). Therefore, the best results were at 2% SBR and 4% SBR at 28 days of age. An inverse relationship was recorded between the increase in SBR ratios and polymer-modified cement mortar's compressive and flexural strength values. In general, the high
... Show MorePoly(L-lactic acid) (PLLA)/poly(caprolactone) (PCL) and two types of organoclay (OMMT) including a fatty amide and ocatdecylamine montmorillonite (FA-MMT and ODA-MMT) were employed to produce polymer nanocomposites by melt blending. Materials were characterized using X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, thermogravimetric analysis (TGA), elemental analysis, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Mechanical properties were also investigated for these nanocomposites. The nanocomposites showed increasing mechanical properties and thermal stability. XRD results indicated that the materials formed nanocomposites. SEM morphology showed that increasing content of OMMT reduc
... Show MoreRapid population growth and the development of industries result in an increase in solid waste. Glass, which represents a large proportion of solid waste, can be used in construction applications. The utilization of recycled glass waste in the asphalt mixture is considered an environmentally-friendly application. In this laboratory study, glass bottles were recycled by crushing, grinding, and sieving them into particles that pass through sieve No. 200 to be used as a partial replacement for the filler in the hot mixture asphalt of wearing course Type-A. The ratios (4, 4.3, 4.6, 4.9, 5.2,5.5) were used to determine the optimum asphalt content (OAC), and three ratios (30, 60, and 90) were used for the replacement of limestone powder filler to
... Show MoreThe incorporation of safety characteristics into the traditional pavement structural design or in the functional evaluation of pavement condition has not been established yet. The design has focused on the structural capacity of the roadway so that the pavement can withstand specific level of repetitive loading over the design life. On the other hand, the surface texture condition was neither included in the AASHTO design procedure nor in the present serviceability index measurements.
The pavement surface course should provide adequate levels of friction and ride quality and maintain low levels of noise and roughness. Many transportation departments perform routine skid resistant testing, the type of equipment us
... Show MoreThe distress of moisture induced damage in flexible pavement received tremendous attention over the past decades. The harmful effects of this distress expand the deterioration of other known distresses such as rutting and fatigue cracking. This paper focused on the efficiency of using the waste material of demolished concrete to prepare asphalt mixtures that can withstand the effect of moisture in the pavement. For this purpose, different percentages of waste demolished concrete (0, 10, 20, 30, 50, 70 and 100) were embedded as a replacement for coarse aggregate to construct the base course. The optimum asphalt contents were determined depending on the Marshall method. Then after, two parameters were founded to evaluate the moisture
... Show More