This study presents the debonding propagation in single NiTi wire shape memory alloy into linear low-density polyethylene matrix composite the study of using the pull-out test. The aim of this study is to investigate the pull-out tests to check the interfacial strength of the polymer composite in two cases, with activation NiTinol wire and without activation. In this study, shape memory alloy NiTinol wire 2 mm diameter and linear fully annealed straight shape were used. The study involved experimental and finite element analysis and eventually comparison between them. This pull-out test is considered a substantial test because its results have a relation with behavior of smart composite materials. The pull-out test was carried out by a u
... Show MoreHerein, we report designing a new Δ (delta‐shaped) proton sponge base of 4,12‐dihydrogen‐4,8,12‐triazatriangulene (compound
Fifty-Four paddy samples, 45 soil samples, and nine irrigation water samples of some paddy fields at Alfurat Alawsat Area, Iraq were collected to investigate the microbial quality including total count bacteria (TCB), molds and yeast, total coliform (TC), and E. coli bacteria. Paddy samples were processed at the laboratory level to produce rice at 32 and 36 whiteness, and the microbial quality of the produced rice was conducted too. The results showed that all irrigation water samples were overpassed the FDA limit for E. coli. All paddy samples were exceeded the good limit of TCB, but no sample exceeded the acceptable limit. Most paddy samples were exceeded the FDA limit for molds and yeast, and few paddy samples exc
... Show MoreIn this study, polymeric coating was developed by incorporating nano graphene in the polymer blend with applications to oil storage tanks. The oil storage tanks samples were brought from the oil Pipeline Company / Doura refinery in Baghdad. The coating polymer was formed with a blend (epoxy resin and repcoat ZR). The proportion of mixing the mixture was 3:1:1 epoxy resin 21.06 gm: repcoat ZR 10.53 gm: hardener 10.53 gm. The blend/graphene was prepared using in stui-polymerization method with different weight percentage 1, 3, 5, and 7 wt % added to blend. The resulting solution was put in a glass tube on a magnetic stirrer for one hour at a temperature of 40 °C. The result of contact angle and wate
... Show More