In this research the a-As flims have been prepared by thermal evaporation with thickness 250 nm and rata of deposition (1.04nm/sec) as function to annealing temperature (373 and 373K), from XRD analysis we can see that the degree of crystalline increase with , and I-V characteristic for dark and illumination shows that forward bias current varieties approximately exponentially with voltage bias. Also we found that the quality factor and saturation current dependence on annealing temperatures.
Objective: The purpose of this study was to assess the effectiveness of Vibriophage Universiti Sains Malaysia 8 (VPUSM 8), a bacteriophage that destroys bacteria, in managing the proliferation of Vibrio cholerae, specifically the El Tor serotype, as an alternate therapeutic strategy. Methods: The study entailed subjecting water samples from Kelantan, Malaysia, to reproduce the natural circumstances that promote the growth of V. cholerae. Subsequently, the samples were contaminated with the V. cholerae O1 El Tor Inaba strain and treated using VPUSM 8. The study employed a controlled experimental design, wherein the samples were divided into three groups, each experiencing different treatment methods. Quantifying the number of colony-
... Show MoreLaue back reflection patterns for quartz crystal are indexed by using Orient Express- program to simulate orientation of single crystals from assignment of principle zones. An oriented quartz single crystal was used as a substrate to deposit Zn metal by controlled thermal evaporation to achieve single crystal films of Zn that are subsequently evaluated by x-ray powder diffraction.
Back ground: Diabetic nephropathy is rapidly becoming the leading cause of end-stage renal disease (ESRD). The onset and course of DN can be ameliorated to a very significant degree if intervention institutes at a point very early in the course of the development of this complication.
Objective: The aim of this study was to characterize risk factors associated with nephropathy in type I diabetes and construct a module for early prediction of diabetic nephropathy (DN) by analyzing their risk factors.
Methods: Case control design of 400 patients with type I diabetes mellitus (IDDM), aged 19-45 years. The cases were 200 diabetic patients with overt protein urea while the controls were 200 diabetic patients with no protein urea or micr
... Show MoreThe investigation of the effect of tempering on thermal analysis of
Al-Ti-Si alloy and its composites with MgO and SiC particles was
performed. Thermal analysis was performed before and after
tempering by DSC scan. Optical microscopy was used to identify the
phases and precipitations that may be formed in base alloy and
composites. X-ray diffraction test indicated that the Al3Ti is the main
phase in Al-Ti-Si alloy in addition to form Al5Ti7Si12 phase. Some
chemical reactions can be occurred between reinforcements and
matrix such as MgO.Al2O3 in Al-Ti/MgO, and Al4C3 and Al(OH)3 in
Al-Ti/SiC composite. X-ray florescence technique is used to
investigate the chemical composition of the fabricated specimens.
H
In current research Copper was employed for preparing a ternary system of Al–Si alloy in different (0.2–2.5 wt. %) the best was taken is (1.5%wt) of copper that circumstances of solidification for improving the mechanical performance of the available in aluminium alloy. Cast iron molds were prepared to obtain tensile strength testing specimens. Alloys were prepared by employing gas furnaces. The molten metal was poured into a preheated cast-iron mold. The obtained alloy structures were studied using an X-ray diffractometer and optical microscopy. The mechanical performance of the prepared alloys was examined under the influence of different hardening conditions in both heat and non-heat-treated conditions. The outcomes showed at the
... Show MoreIn this research the effect of cooling rate and mold type on mechanical properties of the eutectic
and hypoeutectic (Al-Si) alloys has been studied. The alloys used in this research work were (Al- 12.6%Si
alloy) and (Al- 7%Si alloy).The two alloys have been melted and poured in two types of molds with
different cooling rates. One of them was a sand mold and the other was metal mold. Mechanical tests
(hardness, tensile test and impact test) were carried out on the specimens. Also the metallographic
examination was performed.
It has been found that the values of hardness for the alloys(Al-12.6%Si and Al-7%Si) which poured in
metal mold is greater than the values of hardness for the same alloy when it poured in a heated