The present work elucidates the utilization of activated carbon (AC) and activated carbon loaded with silver nanoparticles (AgNPs-AC) to remove tetracycline (TC) from synthetically polluted water. The activated carbon was prepared from tea residue and loaded with silver nanoparticles. Scanning electron microscopy (SEM), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), and Brunauer-Emmett-Teller (BET) were used to characterize the activated carbon (AC) and silver nanoparticles-loaded activated carbon (AgNPs-AC). The impact of various parameters on the adsorption effectiveness of TC was examined. These variables were the initial adsorbate concentration (Co), solution acidity (pH), adsorption time (t), and dosage of the adsorbent. The maximum TC removal percentage was (88%) at pH = 9, time = 230 min, Co = 60 ppm, and dosage = 0.39 g/25 ml using AC as an adsorbent. Whereas the maximum TC removal percentage was (98%) at pH = 9, time = 46 min, Co = 60 ppm, and dosage = 0.0406 g/25 ml using AgNPs-AC. The isotherm models were also studied. It was found that the Langmuir isotherm model fitted well with the experimental data. The adsorption kinetics study showed that the pseudo-second-order accurately describes the experimental results. The analysis of the adsorption thermodynamics revealed that TC adsorption on TAC and AgNPs-AC was endothermic and spontaneous. The study aims to make activated carbon from tea waste and load silver nanoparticles on that activated carbon (AgNPs-AC). It also studies how two adsorbents (activated carbon and activated carbon loaded with silver nanoparticles) remove tetracycline from artificially polluted water. Then, the outcomes were compared.
Several schottky diodes were fabricated from polyaniline/ Carbon nanotube (single and multiwalled) composites. These composites were synthesized with different concentration and two carbon nanotubes types, Single and Multi-Walled Carbon Nanotubes (SWCNT & MWCNT). Aluminum and silver paste were chosen as schottky and ohmic contact respectively. physical and electrical were used to studied these composite by using Atomic Force Microscopy (AFM) and electrical measurements. The Root Mean Square RMS surface roughness of the composite samples was found to be around 4nm. The currentvoltage characteristic were measurements for all samples in the bias range ±15V at room temperature. The results shows the increasing in carbon nanotubes concentration
... Show MoreAnimal fats are a good, promising and ethical alternative source for biodiesel production, but they need more complex treatments than vegetable oils. Iraqi butchery plants waste fats (sheep fat) which are suggested as feedstock to produce biodiesel. This type of fat contains a large quantity of free fatty acids (FFAs) (acid number 49.13 mg KOH/g of fat). The direct transesterification of such fats produce high amount of soap instead of desired biodiesel, so a pre-treatment step (to reduce FFAs) is necessary before transesterification. This step was done by esterification of the free fatty acids in the fat by adding ethanol and using 1% acid catalyst (H2SO4) for 30 minutes. The results showed that the acid number of sheep fat after pre-tr
... Show MoreTwo Prototypes of Transversely Excited at atmospheric pressure (TEA) Nitrogen laser systems (One Stage Blumlein Circuit and Two Stage Blumlein Circuit) were fabricated and operated. High voltage power supply with variable operating voltage (0-20 kv) and operating current (1-3A) was built and tested successfully. The gas flow rate of 15 L/ min and 10 L/ min for OSBC and TSBC was used. The performance of the fabricated systems was studied extensively reaching to the optimum operating conditions. The obtained laser output energy for the first system has linear relationship with the applied voltage. The maximum output energy was about (1.14 mJ) with (10.40) ns pulse duration and the half-wave divergence angle was about (0.1455 m rad). In the
... Show MoreIn this research , phthallic anhydride ring is opened with 4-methyl aniline and acetone as a solvent to results the compound [I] that reacted with dimethyl sulphate and anhydrous sodium carbonate formation to phathalate ester [II], while the acid hydrazide compound [III], was obtained from mixed the compound [II]with hydrazine hydrate, Synthesis four type of shiff bases[IV]a-d was synthesized from the reaction of acid hydrazide [III] with aromatic aldehyde or ketone , when reacted Shiff bases with phthalic anhydride or naphthalicanhydride,I get eight derivatives of oxazepine [V]a-d , [VI]a-d. The bacterial activity of the new compounds studied by four species of bacteria: Esherichia Coli, Enterobactecloacae (Gram negative) and staphylococcu
... Show MoreBackground: Plasma-activated water (PAW) is considered one of the emerging strategies that has been highlighted recently in the food industry for microbial decontamination and mycotoxin detoxification, due to its unique provisional characteristics. Aim: The effectiveness of PAW for aflatoxin B1 (AFB1), ochratoxin A (OTA), and fumonisin B1 (FB1) detoxification in naturally contaminated poultry feeds with its impacts on the feed quality were inspected. Methods: PAW-30 and PAW-60 were utilized for feed treatment for six time durations (5, 10, 15, 20, 40 and 60 min) each. The alterations in the physicochemical properties of PAW after different time durations of plasma inducement and treatment with and without feed samples were monit
... Show MoreThe effect of applied current on protection of carbon steel in 0.1N NaCl solution (pH=7) was investigated under flow conditions (0-0.262 m/s) for a range of temperatures (35-55°C) using rotating cylinder electrode. Various values of currents were applied to protect steel from corrosion, these were Iapp.=Icorr., Iapp.=2Icorr. and Iapp.=2.4Icorr. under stationary and flow conditions. Corrosion current was measured by weight loss method. The variation of protection potential with time and rotation velocity at various applied currents was assessed. It is found that the corrosion rate of carbon steel increases with rotation velocity and
has unstable trend with temperature. The protection current required varies with temperature and it inc
The 4-(?-bromo acetyl)-4?-toluene sulfonanilide (2) was used as key intermediate to synthesize new heterocyclic compounds. This bromo compound was synthesized via sulfonation of amino group of p-amino acetophenone using Hinsburg method with 4-toluene sulfonyl chloride to form 4-acetyl-4?-toluene sulfonanilide (1) which is used as a starting material in this work. This compound was brominated to yield compound (2) which is used as a precursor to synthesize new five and seven membered heterocyclic compounds such as substituted 1,3-oxazoles (3,4), 1,3-thiazole derivatives (5-7), thiourea compounds (8a,b), 1,3-Thiazoline-2-thione compounds (9a-f) and 1,2,5-triazepine compounds (11a-d). The synthesized compounds were identified depending u
... Show MoreThis study was aimed to evaluate the effect of spraying nano chitosan loaded with NPK fertilizer and nettle leaf and green tea extracts on the growth and productivity of potato for the spring and fall seasons of 2021.It was conducted at private farm in Wasit Governorate, Iraq, as a factorial experiment (5 × 5) within randomized complete block design using three replicates. The first factor included spraying with four concentrations of chitosan nanoparticles loaded with NPK fertilizer 0, 10. 15 and 20% in addition to chemical fertilization treatment, the second factor was spraying nettle leaf extract 25 and 35 gL-1 and green tea extract with 2 and 4 g.L-1, in addition to the control treatment, spraying with distilled water only. The
... Show MoreThe removal of heavy metal ions from wastewater by ion exchange resins ( zeolite and purolite C105), was investigated. The adsorption process, which is pH dependent, shows maximum removal of metal ions at pH 6 and 7 for zeolite and purolite C105 for initial metal ion
concentrations of 50-250 mg/l, with resin dose of 0.25-3 g. The maximum ion exchange capacity was found to be 9.74, 9.23 and 9.71 mg/g for Cu2+, Pb2+, and Ni2+ on zeolite respectively, while on purolite C105 the maximum ion exchange capacity was found to be 9.64 ,8.73 and 9.39 for Cu2+, Pb2+, and Ni2+ respectively. The maximum removal was 97-98% for Cu2+ and Ni2+ and 92- 93% for Pb2+ on zeolite, while it was 93-94% for Cu2+, 96-97% for Ni2+, and 87-88% for Pb2+ on puroli