The zirconia ceramic restoration (ZCR) is used as substitutes for the metal-ceramic restoration. Clinical studies demonstrating of ZCRs showed a high fracture incidence of veneering layer than metal-ceramic restorations. This attributed to the low bond strength of zirconia to veneering ceramic as a result of lacking of glass content in its matrix. Surface treatment was proposed to improve the bonding strength between zirconia and veneering ceramic. Several studies revealed that some treatment such as airborne particle abrasion (APA) is responsible for generating chipping of veneering ceramic. The study aimed to develop a new zirconia coatings to increase bonding strength between zirconia substrate and veneering porcelain. Three groups of 150 zirconia specimens (discs, rods and crowns) were divided according to the type of surface treatments; Group M1 designated unsintered zirconia specimens coated with a mixture of glaze porcelain powder and partially-sintered zirconia powder prepared at 1100 °C with two particle sizes; A (26 ± 0.3 μm) and size B (47 ± 0.5 μm), group M2 was coated with mixture of ceramic liner paste and same selected particle sizes of partially-sintered zirconia powders. The coated groups (M1 and M2) subdivided according to powder sizes into M1A, M1B, M2A and M2B. APA group (as control) of sintered zirconia specimens abraded with 50 μm aluminium oxide powder. Surface area roughness (Sa) was measured by surface texture analyser. Surface morphology and elemental composition were analysed by scanning electron microscope (SEM). Crystallographic phases were identified by X-ray diffraction (XRD). The coefficient of thermal expansion (CTE) was assessed by a thermomechanical analyser. For shear bond strength (SBS) test was evaluated by a universal testing machine (UTM). The fracture strength (FS) test prepared and measured by Cercon CAD/CAM system and UTM. Fractographic analysis for SBS and FS were examined by a stereomicroscope and SEM. For each test and measurement, 10 specimens were used per group. Finite element analysis (FEA) was used to simulate and predict the iv stress distributions of the static oblique load in coated and non-coated zirconia crown models. The collected data were analysed by one-way ANOVA and Tukey HSD test at (P<0.05). Surface roughness results showed significant differences among all groups (P<0.000). The M1B group exhibited a higher Sa value (10.33 ± 0.59 μm) among the tested groups. XRD analysis showed tetragonal and monoclinic phases in the control group while only tetragonal was detected in the coated groups. The SBS values for coated groups were higher than the control group. The M1B group showed higher and significant differences in SBS value (37.54 ± 4.38 MPa) among other tested groups (P<0.05). The FS test indicated that coated M1B group (647.92 ± 97.33 N) higher than the other groups (P<0.00). FEA showed the coated crown models have lower stress level than the non-coated model. The new coating (M1B) by airbrush spray technique considered as an alternative way to APA treatment to improve the bond strength of zirconia substrate to veneering ceramic and indicating as an applicable surface treatment for improving the clinical performance of the coated ZCR.
Permanent magnets of different intensities were used to investigate the effect of a magnetic field in the process of preventing deposits of calcium carbonate. The magnets were fixed on the water line from the tap outside. Then heating a sample of this water in flasks and measuring the amount of sediment in a manner weighted differences. These experiments comprise to the change of the velocity of water flow, which amounted to (0.5, 0.75, 1) m/sec through the magnetic fields that are of magnetic strength (2200, 6000, 9250, 11000) Gauss, and conduct measurements, tests and compare them with those obtained from the use of ordinary water.The results showed the effectiveness of magnetic treatment in reducing the rate of deposition of calcium carb
... Show MoreObjective: To enhance bonding strength between thermoplastic denture base and acrylic soft liner through ethyl acetate surface treatment. Materials and Methods: Modifications of thermoplastic acrylic denture base surface were investigated with SEM. FTIR was used to detect whether there was a chemical bond between thermoplastic acrylic and the organic solvent. A total of 80 samples were prepared and divided into 20 samples for the surface roughness test and 60 samples for the shear bond strength test. Failure type was assessed visually. Results: Shear bond strength and surface roughness values of un treated samples were lower in comparison to surface treated groups; the greatest post thermocycling bond strength value was recorded for the sam
... Show MoreBackground: Ageing is a continuous accumulative ordinary physiological phenomena occurs upon all organs and body structures including saliva by its constituents which can influence the caries process, for that this study was conducted to determine the impact of ageing on selected chemical composition of saliva and their effects on dental caries experience characteristics at different age groups among apparently healthy men. Materials and method: A descriptive comparative study was conducted to compare between three study samples (young, middle and old age adults), thirty male in each study insert, aged (20 years, 40 years and 60 years) respectively. They were selected from private health center in Baghdad - Iraq, from the mid of November
... Show MoreBackground: asthma has an influence on craniofacial development. Recently evidences show that there is an association between oral health problems and chronic lung disease. The present study was designed to estimate the changes in arch dimension measurements among asthmatic children aged 12 years old who were collected from AL- Zahra Center Advisory for Allergy and Asthma and compare them with the non-asthmatic children of the same age and gender. Material and Methods: Fifty children (25 asthmatic and 25 non- asthmatic children) were included for the odontometric measurement. For both upper and lower study models, photographs were taken using special photographic apparatus for each child, and the statistical analysis were done by using SPSS
... Show MorePMMA (Poly methyl methacrylate) is considered one of the most commonly used materials in denture base fabrication due to its ideal properties. Although, a major problem with this resin is the frequent fractures due to heavy chewing forces which lead to early crack and fracture in clinical use. The addition of nanoparticles as filler performed in this study to enhance its selected mechanical properties. The Nano-additive effect investigated in normal circumstances and under a different temperature during water exposure. First, tests applied on the prepared samples at room temperature and then after exposure to water bath at (20, 40, 60) C° respectively. SEM, PSD, EDX were utilized for samples evaluation in this study. Flexural
... Show MoreThis study aims to test ceramic waste's capacity to remove nickel from aqueous solutions through adsorption. Ceramic wastes were collected from the Refractories Manufacturing Plant in Ramadi. Through a series of lab tests, the reaction time (5, 10, 15, 20, 25, 30, 35, 40, 45, and 50 minutes, and Ni concentrations (20, 40, 60, and 80) were tested using ceramic wastes with a solid to liquid ratio of 2g/30ml. At a temperature of 30ºC, the pH, total dissolved solids (TDS), and electrical conductivity (EC) were all measured. The equilibrium time was set at 30 min. Thereafter, the sorption (%) somewhat increased positively with the Ni concentration. Freundlich's equation showed that the adsorption intensity is 1.1827 and the Freundlich c
... Show MoreBackground: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreBackground: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreDental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60 test block w
... Show More