Quantum dots (QDs) can be defined as nanoparticles (NPs) in which the movement of charge carriers is restricted in all directions. CdTe QDs are one of the most important semiconducting crystals among other various types where it has a direct energy gap of about 1.53 eV. The aim of this study is to exaine the optical and structural properties of the 3MPA capped CdTe QDs. The preparation method was based on the work of Ncapayi et al. for preparing 3MPA CdTe QDs, and hen, the same way was treated as by Ahmed et al. via hydrothermal method by using an autoclave at the same temperature but at a different reaction time. The direct optical energy gap of CdTe QDs is between 2.29 eV and 2.50 eV. The FTIR results confirmed the covalent bonding between the 3 MPA ligands and the QDs surface. The XRD results revealed that the synthesized QDs have two crystal structures, wurtzite and cubic zinc blend. FESEM results confirmed that the NPs have a spherical shape with an average diameter of nearly 33.85 nm. TEM analysis confirmed the particle's near sphericity, with an average diameter of around 49.33 nm. The sudden increase in temperature led to increase the particle size. It was found that ligand addition, maintaining the solution's acidity, and autoclaving the material enhanced quantum confinement.
Cupressus sempervirens L., Cupressaceae, that is known as evergreen cypress, Mediterranean cypress and in Arabic called “al -Sarw. It is an evergreen, medium sized, longevity, and wide distributed over all the world. The plant represents an important member of conifer plants which characterized with aromatic leaves and cones. Cupressus sempervirens have been ethnobotanical uses as an antiseptic, relief of cough, astringent, antispasmodic, wound healing and anti-inflammatory. Aims of this work are phytochemical analysis, isolation and structural identification of Quercitroside (quercitrin) and essential oil in Iraqi C. sempervirens. Isolation of quercitrin was
... Show MoreThe development of a reversed phase high performance liquid chromatography fluorescence method for the determination of the mycotoxins fumonisin B1 and fumonisin B2 by using silica-based monolithic column is described. The samples were first extracted using acetonitrile:water (50:50, v/v) and purified by using a C18 solid phase extraction-based clean-up column. Then, pre-column derivatization for the analyte using ortho-phthaldialdehyde in the presence of 2-mercaptoethanol was carried out. The developed method involved optimization of mobile phase composition using methanol and phosphate buffer, injection volume, temperature and flow rate. The liquid chromatographic separation was performed using a reversed phase Chromolith® RP-18e column
... Show MoreThe purpose of my thesis is to prepare four new ligands (L1-L4) that have been used to prepare a series of metal complexes by reacting them with metal ions: M=(Mn(II), Co(II), Ni(II), Cu(II), Zn(II), Cd(II), Hg(II) Where succinyl chloride was used as a raw material for the preparation of bi-dented ligands (L1-L4) by reacting it with potassium thiocyanate as a first step and then reacting with (2-aminobenzothiazole, Benzylamine, 4-aminoantipyrine, Sulfamethoxazole) respectively as a second step with the use of dry acetone as a solvent, the chemical formula of the four ligands prepared in succession: N1,N4-bis(benzo[d]thiazol-2-ylcarbamothioyl)succinamide (L1) N1,N4-bis(benzylcarbamothioyl)succinami
... Show MorePorosity and pore structure are important characteristics of pharmaceutical tablets, since they influence the physical properties, such as mechanical strength, density and disintegration time. This paper is an attempt to investigate the pore structure of four different paracetamol tablets based on mercury porosimetry. The intrusion volumes of mercury were used to calculate the pore diameter, pore volume and pore size distribution. The result obtained indicate that the variation of the pore volume in the tablets followed the sequence:- S.D.I. Iraq? Pharmacare,Dubai-U.A.E.? Bron and Burk(UK) London?Lark Laboratories(India), while the variation of surface area followed the sequence:- S.D.I. Iraq? Lark Laboratories(India)? Pharmacare,Dubai-U.A
... Show MoreThe hydroisomerization of n-decane was studied on SAPO-11 catalyst. Catalyst of 0.25wt.%Pt/SAPO-11 was prepared locally and used in the present work. The hydroconversion performed in a continuous fixed-bed laboratory reaction unit. Experiments of n-decane isomerization were performed in a temperature range of 200 to 275°C,LHSV range of 0.5-2 h-1, and hydrogen to decane mole ratio of 2.1-8.2. The results show that the n-decane conversion increases with increasing temperature and decreasing LHSV , the maximum conversion 56.77 % was achieved at temperature 275°C and LHSV of 0.5 h-1. The kinetic of n-decane isomerization was also studied and the reaction was first order. The kinetic analysis also showed that the activation energy eq
... Show MoreThe hydroisomerization of n-decane was studied on SAPO-11 catalyst. Catalyst of 0.25wt.%Pt/SAPO-11 was prepared locally and used in the present work. The hydroconversion performed in a continuous fixed-bed laboratory reaction unit. Experiments of n-decane isomerization were performed in a temperature range of 200 to 275°C,LHSV range of 0.5-2 h-1, and hydrogen to decane mole ratio of 2.1-8.2. The results show that the n-decane conversion increases with increasing temperature and decreasing LHSV , the maximum conversion 56.77 % was achieved at temperature 275°C and LHSV of 0.5 h-1. The kinetic of n-decane isomerization was also studied and the reaction was first order. The kinetic analysis also showed that the
... Show MoreIn this research, a sensor for chemical solutions was designed and formed using optical fiber-based on a surface Plasmon resonance technology. A single-mode optical fiber with three different diameters (25, 45 and 65) µm was used, respectively. The second layer of the low refractive fiber was replaced by gold, which was electrically deposited at 40 µm thickness. For each of the three types of optical fiber, different saline concentrations (different index of refraction) were used to evaluate the performance of the refractive index sensor (chemical sensor) by measuring its sensitivity and resolutions. The highest values we could get for these two parameters were 240mm/RIU, and 6*10-5 RIU respectively, when the diameter of a
... Show MoreNiO0.99Cu0.01 films have been deposited using thermal evaporation
technique on glass substrates under vacuum 10-5mbar. The thickness
of the films was 220nm. The as -deposited films were annealed to
different annealing temperatures (373, 423, and 473) K under
vacuum 10-3mbar for 1 h. The structural properties of the films were
examined using X-ray diffraction (XRD). The results show that no
clear diffraction peaks in the range 2θ= (20-50)o for the as deposited
films. On the other hand, by annealing the films to 423K in vacuum
for 1 h, a weak reflection peak attributable to cubic NiO was
detected. On heating the films at 473K for 1 h, this peak was
observed to be stronger. The most intense peak is at 2θ = 37
Chlorine doped SnS have been prepared utilizing chemical spray pyrolysis. The effects of chlorine concentration on the optical constants were studied. It was seen that the transmittance decreased with doping, while reflectance, refractive index, extinction coefficient, real and imaginary parts of dielectric constant were increased as the doping percentage increased. The results show also that the skin depth decrease as the chlorine percentage increased which could be assure that it is transmittance related.
The effect of the concentration of the colloidal nanomaterial on their optical limiting behavior is reported in this paper. The colloids of sliver nanoparticles in deionized water were chemically prepared for the two concentrations (31 ppm and 11ppm). Two cw lasers (473 nm Blue DPSS laser and 532 nm Nd:YAG laser) are used to compare the optical limiting performance for the samples. UV–visible spectrophotometer, transmission electron microscope (TEM) and Fourier Transformation Infrared Spectrometer (FTIR) were used to obtain the characteristics of the sample. The nonlinear refractive index was calculated to be in the order of 10-9 cm2/W. The results demonstrate that the observed limiting response is significant for 532nm. In addition, t