Background: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in the canal for 1 min, roots were randomly divided into two groups according to the obturation technique (thirty teeth for each group): Group I: Single Reciproc Gutta percha cone obturation technique, Group II: Gutta fusion obturation technique, then each group divided into three subgroup according to the type of sealer, AH subgroup: AH Plus sealer, BC subgroup: bioceramic sealer and GF subgroup: Gutta flow 2 sealer. The roots then stored in moist environment at 37°C for one week, the roots were embedded in clear acrylic resin and each root sectioned into three levels apical, middle and cervical. The bond strength was measured using computerized universal testing machine each section fixed in the machine so that the load applied from apical to cervical direction at 0.5mm/min. speed and the computer show the higher bond force before dislodgment of the filling material. These forces were divided by the surface area to obtain the bond strength in MPa. Results: Statistical analysis was performed and the result showed a highly significant differences between the three types of sealers when the same obturation technique were used, also there is highly significant differences between two groups with two different obturation technique. Conclusion: This study showed that the push out bond strength of AH plus sealer was higher than bioceramic sealer and Gutta flow 2 sealer respectively when the same obturation technique was used. The push out bond strength was affected by the obturation technique and Gutta fusion obturation technique showed higher bond strength than single cone obturation technique when the same type of sealer was used.
Through an experimental program of eighteen specimens presented in this paper, the bond strength between reinforcing bar and rubberized concrete was produced by adding waste tire rubber instead of natural aggregate. The fine and coarse aggregate was replaced in 0%, 25%, and 50% with the small pieces of a waste tire. Natural aggregate replacement ratio, rebar size, embedded rebar length, the rebar yield stress of rebar, cover, and concrete compressive strength were studied in this investigation. Ultimate bond stress, bond stress-slip response, and failure modes were presented. The experimental results reported that a reduction of 19% in bond strength was noticed in 50% replaced rubberized concrete compared with convention
... Show MoreBackground: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets
... Show MoreBackground: The treatment of dental tissues proceeding to adhesive procedures is a crucial step in the bonding protocol and decides the clinical success ofrestorations. This study was conducted in vitro, with the aim of evaluating thenanoleakage on the interface between the adhesive system and the dentine treated by five surface modalities using scanning electron microscopy and energydispersiveX-ray spectrometry. Materials and methods: Twenty five extracted premolars teeth were selected in the study. Standardized class V cavities were prepared on the buccal and lingual surfaces then the teeth divided into five main groups of (5 teeth in each group n=10) according to the type of dentine surface treatment that was used: Group (A): dentine was
... Show MoreBackground: The treatment of dental tissues proceeding to adhesive procedures is a crucial step in the bonding protocol and decides the clinical success ofrestorations. This study was conducted in vitro, with the aim of evaluating thenanoleakage on the interface between the adhesive system and the dentine treated by five surface modalities using scanning electron microscopy and energydispersiveX-ray spectrometry. Materials and methods: Twenty five extracted premolars teeth were selected in the study. Standardized class V cavities were prepared on the buccal and lingual surfaces then the teeth divided into five main groups of (5 teeth in each group n=10) according to the type of dentine surface treatment that was used: Group (A): dentine was
... Show MoreObjective: To evaluate and compare the effect of mechanical surface treatment (groove, aluminum oxide particles)
with 45 degree bevel type of joint on tensile bond strength of acrylic specimens repaired by two curing methods
(microwave and water both).
Methodology: Eighty specimens (80) were prepared from pink heat cure acrylic resin. They were divided into two
main groups (40 specimen repaired by microwave energy and 40 specimens repaired by water bath method).Each
group can be divided into four subgroups of ten according to the surface treatment. The control group A was left
intact, group B received no surface treatment, group C and D received surface treatment by (groove, 50 m aluminum
oxide particles). Specimens
Background: The aim of this in vitro study was to evaluate and compare the effect of preheating microleakage among three different filler size composites which include Filtektm Z250 micro hybrid, Z250xt Nano hybrid and nanocomposite Z350xt. in Class II cavity preparation .
Materials and methods: sixty maxillary first premolars were prepared with class II cavities. Samples were divided into three groups according to material used group A (FiltekZ250 micro hybrid). Group B(Z250xt Nano hybrid). Group C (nanocomposite Z350xt)and each group divided into two subgroups of ten teeth according to temperature of composite:
... Show MoreABSRTACT Background: Soft liner material is become important in dental prosthetic treatment. They are applied to the surface of the dentures to achieve more equal force distribution , reduce localized pressure and improve denture retention by engaging undercut . So the aim of the study is to evaluate the effect of different surface treatment by air-abrasion AL2O3 and laser treatment with CO2 laser on improving the shear bond strength of the denture liner to acrylic denture base material . Materials and methods: the 30 specimens of heat cured acrylic denture base material (high Impact acrylic )and heat cured soft liner (Vertex ,Nether Lands )were prepared for this study .They were designed and divided according to type of the s
... Show MoreABSTRACT Background: This study aimed to study the effect of some acidic drinks (Vinegars and fresh Orange juice) and energy drinks (Red bull) on surface roughness of three types of bulkfill composite materials: Filtek posterior bulkfill (3M), Sonicfill (Kerr) and Filtek p60 (3M). Materials and Methods: Total number of 120 samples are prepared by using a mold of (12mm diameter and 3mm height), which were divided into three groups forty samples for each group: Group A: Filtek bulkfill posterior composite (3M), Group B: Sonicfill composite (Kerr), Group C: Filtek P60 (3 M) which then divided into four sub- groups (n=10) (1) samples were kept in distilled water as a control group (2) samples were immersed in Redbull (3) samples were immersed